JPH11354470A5 - - Google Patents
Info
- Publication number
- JPH11354470A5 JPH11354470A5 JP1998176723A JP17672398A JPH11354470A5 JP H11354470 A5 JPH11354470 A5 JP H11354470A5 JP 1998176723 A JP1998176723 A JP 1998176723A JP 17672398 A JP17672398 A JP 17672398A JP H11354470 A5 JPH11354470 A5 JP H11354470A5
- Authority
- JP
- Japan
- Prior art keywords
- gas
- forming method
- film forming
- film
- containing gas
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP17672398A JP3988256B2 (ja) | 1998-06-09 | 1998-06-09 | 成膜方法 |
| TW088121590A TW554382B (en) | 1998-06-09 | 1999-12-09 | Method of forming TiSiN film, diffusion preventing film and semiconductor device constituted by TiSiN film and method of producing the same, and TiSiN film forming device |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP17672398A JP3988256B2 (ja) | 1998-06-09 | 1998-06-09 | 成膜方法 |
Related Child Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2006195788A Division JP4640281B2 (ja) | 2006-07-18 | 2006-07-18 | バリヤメタル層及びその形成方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH11354470A JPH11354470A (ja) | 1999-12-24 |
| JPH11354470A5 true JPH11354470A5 (cg-RX-API-DMAC7.html) | 2005-06-30 |
| JP3988256B2 JP3988256B2 (ja) | 2007-10-10 |
Family
ID=16018662
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP17672398A Expired - Fee Related JP3988256B2 (ja) | 1998-06-09 | 1998-06-09 | 成膜方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3988256B2 (cg-RX-API-DMAC7.html) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100762863B1 (ko) * | 2000-06-30 | 2007-10-08 | 주식회사 하이닉스반도체 | 확산방지 티타늄-실리콘-질소 막을 이용한 구리금속배선방법 |
| JP2002363759A (ja) * | 2001-06-12 | 2002-12-18 | Tokyo Electron Ltd | プラズマ処理装置、プラズマ処理方法及び微量ガスの導入時期検出方法 |
| TWI252512B (en) * | 2004-10-20 | 2006-04-01 | Hynix Semiconductor Inc | Semiconductor device and method of manufacturing the same |
-
1998
- 1998-06-09 JP JP17672398A patent/JP3988256B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6573182B2 (en) | Chemical vapor deposition using organometallic precursors | |
| JP5829196B2 (ja) | シリコン酸化物膜の成膜方法 | |
| US5595784A (en) | Titanium nitride and multilayers formed by chemical vapor deposition of titanium halides | |
| US8821986B2 (en) | Activated silicon precursors for low temperature deposition | |
| CN105390381B (zh) | 使用具有金属类前驱物的cvd与ald工艺的nmos金属栅极材料、制造方法以及设备 | |
| US6214714B1 (en) | Method of titanium/titanium nitride integration | |
| US4966869A (en) | Tungsten disilicide CVD | |
| US6252295B1 (en) | Adhesion of silicon carbide films | |
| KR910015011A (ko) | 금속 또는 금속 실리사이드막의 형성방법 | |
| JP2001358139A (ja) | 窒化ケイ素材のcvd合成 | |
| JPH05195228A (ja) | 低温化学蒸着法 | |
| JP4001509B2 (ja) | 半導体素子の拡散防止膜形成方法 | |
| KR20220083730A (ko) | 평활한 티타늄 나이트라이드 층 및 이를 형성시키는 방법 | |
| US20060024959A1 (en) | Thin tungsten silicide layer deposition and gate metal integration | |
| JP7542046B2 (ja) | バリア層なしのタングステン堆積物 | |
| KR100447031B1 (ko) | 텅스텐 실리사이드막의 형성방법 | |
| JP7295749B2 (ja) | 半導体装置の製造方法 | |
| KR950012607A (ko) | 반도체 기판상에 규화 텅스텐 피복을 증착시키기 전에 증착챔버의 알루미늄 함유면들을 예비처리하기 위한 방법 | |
| JPH09260306A (ja) | 薄膜形成方法 | |
| JP2751606B2 (ja) | 配線の形成方法 | |
| JPH0410219B2 (cg-RX-API-DMAC7.html) | ||
| JPH05129230A (ja) | タングステン膜の形成方法 | |
| JP3953244B2 (ja) | 薄膜形成方法 | |
| KR100342825B1 (ko) | 반도체소자의텅스텐실리사이드층형성방법 | |
| JP2024541052A5 (cg-RX-API-DMAC7.html) |