JPH11256303A5 - - Google Patents
Info
- Publication number
- JPH11256303A5 JPH11256303A5 JP10-75001A JP7500198A JPH11256303A5 JP H11256303 A5 JPH11256303 A5 JP H11256303A5 JP 7500198 A JP7500198 A JP 7500198A JP H11256303 A5 JPH11256303 A5 JP H11256303A5
- Authority
- JP
- Japan
- Prior art keywords
- sec
- particles
- penetrate
- melt
- impact
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP07500198A JP3172488B2 (ja) | 1998-03-10 | 1998-03-10 | 耐摩耗性に優れる軟質非鉄金属部材および軟質非鉄金属部材の表面改質方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP07500198A JP3172488B2 (ja) | 1998-03-10 | 1998-03-10 | 耐摩耗性に優れる軟質非鉄金属部材および軟質非鉄金属部材の表面改質方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH11256303A JPH11256303A (ja) | 1999-09-21 |
| JPH11256303A5 true JPH11256303A5 (enExample) | 2001-03-13 |
| JP3172488B2 JP3172488B2 (ja) | 2001-06-04 |
Family
ID=13563546
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP07500198A Expired - Lifetime JP3172488B2 (ja) | 1998-03-10 | 1998-03-10 | 耐摩耗性に優れる軟質非鉄金属部材および軟質非鉄金属部材の表面改質方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3172488B2 (enExample) |
Families Citing this family (15)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2001181859A (ja) * | 1999-10-12 | 2001-07-03 | Natl Inst Of Advanced Industrial Science & Technology Meti | 複合構造物の作製方法および作製装置 |
| JP2002336744A (ja) * | 1999-11-25 | 2002-11-26 | Asahi:Kk | 物質を形成する高速熱スプレー装置及びこのスプレー装置によりコーティングまたは塊状物質を形成する方法 |
| JP3874682B2 (ja) * | 2001-03-22 | 2007-01-31 | 独立行政法人産業技術総合研究所 | 摺動部材とその作製方法 |
| JP4626945B2 (ja) * | 2004-07-06 | 2011-02-09 | 第一高周波工業株式会社 | サーメット溶射皮膜形成部材およびその製造方法 |
| US20060093736A1 (en) * | 2004-10-29 | 2006-05-04 | Derek Raybould | Aluminum articles with wear-resistant coatings and methods for applying the coatings onto the articles |
| JP4885445B2 (ja) * | 2004-12-21 | 2012-02-29 | 株式会社フジミインコーポレーテッド | 溶射用粉末 |
| KR100802328B1 (ko) * | 2005-04-07 | 2008-02-13 | 주식회사 솔믹스 | 내마모성 금속기지 복합체 코팅층 형성방법 및 이를이용하여 제조된 코팅층 |
| JP5175449B2 (ja) * | 2006-03-30 | 2013-04-03 | 大同メタル工業株式会社 | 皮膜付き摺動部材 |
| JP5493334B2 (ja) * | 2008-11-05 | 2014-05-14 | 国立大学法人東北大学 | 高炭素鋼部材の補修における高効率付着方法及び材料 |
| JP2010111905A (ja) * | 2008-11-05 | 2010-05-20 | Tohoku Univ | 高炭素鋼の補修技術 |
| JP2010242160A (ja) * | 2009-04-06 | 2010-10-28 | Kanagawa Prefecture | 耐摩耗性導電部材及びその製造方法 |
| JP5889564B2 (ja) * | 2011-07-26 | 2016-03-22 | オーエスジー株式会社 | 工具の表面改質方法 |
| US20170204920A1 (en) * | 2014-06-06 | 2017-07-20 | National Research Council Of Canada | Bi-layer iron coating of lightweight metallic substrate |
| CA2994633C (en) * | 2015-08-06 | 2019-01-08 | Nissan Motor Co., Ltd. | Sliding member and manufacturing method therefor |
| CN113878238A (zh) * | 2021-10-18 | 2022-01-04 | 天津大学 | 一种利用激光辅助改性提升软质金属表面加工质量的方法 |
-
1998
- 1998-03-10 JP JP07500198A patent/JP3172488B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ATE184328T1 (de) | Verfahren zum thermischen sprühen von pulvern mit temperaturen unterhalb des schmelzpunkts dieser pulver | |
| FR2827311B1 (fr) | Procede de reparation locale de pieces revetues d'une barriere thermique | |
| US20100080982A1 (en) | Thermal spray coating application | |
| SG123725A1 (en) | Laser enhancements of cold sprayed deposits | |
| ATE299776T1 (de) | Verfahren zur herstellung eines oberflächenlegierten zylindrischen, teilzylindrischen oder hohlzylindrischen bauteils | |
| DE69321295D1 (de) | Laserverfahren zum Anbringen von vorbehandelten überzogenen Schleifpartikeln und einer Metallmatrix auf der Spitze einer Turbinenschaufel | |
| JPH07323384A5 (enExample) | ||
| CN103717344A (zh) | 用于包覆基板的工艺 | |
| CN113249717A (zh) | 一种镍基合金激光熔覆粉末的激光熔覆方法 | |
| CN110586944A (zh) | 金属3d打印零件的激光表面改性方法 | |
| US20110229665A1 (en) | Thermal spray coating for track roller frame | |
| KR20040063999A (ko) | 코팅 도포 방법 | |
| RU2016131959A (ru) | Композиционный материал на основе титанового сплава и способ его получения | |
| JPH091296A5 (enExample) | ||
| JPS62274062A (ja) | セラミツク被覆部材の製造方法 | |
| Blue et al. | High-density-infrared transient liquid coatings | |
| CN106939400B (zh) | 一种用于提高输电线路悬垂金具耐磨性的热喷涂方法 | |
| US5096662A (en) | Method for forming high abrasion resisting layers on parent materials | |
| JPH093528A5 (enExample) | ||
| JPS62112769A (ja) | 耐摩耗性、耐食性、耐久性に優れる容射被膜の形成方法 | |
| RU2001104809A (ru) | Способ создания упрочненного поверхностного слоя на деталях из металлических сплавов и композиционных материалов | |
| RU99111117A (ru) | Способ обработки поверхности металлических изделий | |
| JPS61113757A (ja) | 金属基体面に形成した異種金属被膜のレ−ザ−処理方法 | |
| Girzhon et al. | Influence of pulsed laser processing on structure of alloy cast iron | |
| RU2499077C1 (ru) | Способ нанесения износостойких покрытий на стальные изделия |