JPH08188619A5 - - Google Patents

Info

Publication number
JPH08188619A5
JPH08188619A5 JP7-1177A JP117795A JPH08188619A5 JP H08188619 A5 JPH08188619 A5 JP H08188619A5 JP 117795 A JP117795 A JP 117795A JP H08188619 A5 JPH08188619 A5 JP H08188619A5
Authority
JP
Japan
Prior art keywords
document
aqueous slurry
procedural amendment
acid
fine particles
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP7-1177A
Other languages
English (en)
Japanese (ja)
Other versions
JP3602590B2 (ja
JPH08188619A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP00117795A priority Critical patent/JP3602590B2/ja
Priority claimed from JP00117795A external-priority patent/JP3602590B2/ja
Publication of JPH08188619A publication Critical patent/JPH08188619A/ja
Publication of JPH08188619A5 publication Critical patent/JPH08188619A5/ja
Application granted granted Critical
Publication of JP3602590B2 publication Critical patent/JP3602590B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP00117795A 1995-01-09 1995-01-09 ポリビニルアルコール系重合体微粒子の製造方法 Expired - Fee Related JP3602590B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP00117795A JP3602590B2 (ja) 1995-01-09 1995-01-09 ポリビニルアルコール系重合体微粒子の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP00117795A JP3602590B2 (ja) 1995-01-09 1995-01-09 ポリビニルアルコール系重合体微粒子の製造方法

Publications (3)

Publication Number Publication Date
JPH08188619A JPH08188619A (ja) 1996-07-23
JPH08188619A5 true JPH08188619A5 (enExample) 2002-01-15
JP3602590B2 JP3602590B2 (ja) 2004-12-15

Family

ID=11494167

Family Applications (1)

Application Number Title Priority Date Filing Date
JP00117795A Expired - Fee Related JP3602590B2 (ja) 1995-01-09 1995-01-09 ポリビニルアルコール系重合体微粒子の製造方法

Country Status (1)

Country Link
JP (1) JP3602590B2 (enExample)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4087321B2 (ja) 2003-09-17 2008-05-21 株式会社クラレ ポリビニルアルコール系重合体およびその製造方法
JP5121172B2 (ja) * 2005-07-01 2013-01-16 日本合成化学工業株式会社 血管一時塞栓材料、その製造方法、および血管一時塞栓剤
US8361454B2 (en) 2005-07-01 2013-01-29 The Nippon Synthetic Chemical Industry Co., Ltd. PVA particle for temporary embolic material and production process thereof, and temporary embolic material

Similar Documents

Publication Publication Date Title
JP2005145059A (ja) 水圧転写方法
DE69603731D1 (de) Flammgeschützte produkte
US3817887A (en) Adhesive stick comprising an alkylated n-vinylpyrrolidone polymer
JPH0995538A5 (enExample)
JPH09255541A5 (enExample)
JPH06227124A5 (enExample)
JPH06298841A5 (enExample)
JP2003201454A (ja) 水性接着剤とその製造方法、及び段ボールとその製造方法
JPH08188695A5 (enExample)
JP2000034347A5 (enExample)
JPS6024823B2 (ja) 再湿接着剤
KR950003322A (ko) 마이클(Michael) 첨가 반응에 의한 폴리비닐 알코올 변성용 고상 프로세스
JP3712546B2 (ja) 澱粉糊
JP2849401B2 (ja) 無機質繊維板の製造方法
JPH09268492A5 (enExample)
JPH09228291A (ja) 水解紙用バインダー及び水解紙
JPH0970260A5 (enExample)
JPH08283682A (ja) 接着剤
JP3600044B2 (ja) 澱粉糊
JPH07216784A (ja) 紙のサイジング方法
JP3310703B2 (ja) 金属性モノリス担体の製造方法
JPH02221492A (ja) 紙の抄紙方法
JPH0788357A5 (enExample)
CN1063497A (zh) 即用即调、水再湿粘性胶粉
GB2357524A (en) Paper sizing composition