JPH073429A5 - - Google Patents

Info

Publication number
JPH073429A5
JPH073429A5 JP5-149557A JP14955793A JPH073429A5 JP H073429 A5 JPH073429 A5 JP H073429A5 JP 14955793 A JP14955793 A JP 14955793A JP H073429 A5 JPH073429 A5 JP H073429A5
Authority
JP
Japan
Prior art keywords
less
dent resistance
manufacturing
procedural amendment
nitriding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP5-149557A
Other languages
English (en)
Japanese (ja)
Other versions
JP3105380B2 (ja
JPH073429A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP05149557A priority Critical patent/JP3105380B2/ja
Priority claimed from JP05149557A external-priority patent/JP3105380B2/ja
Publication of JPH073429A publication Critical patent/JPH073429A/ja
Publication of JPH073429A5 publication Critical patent/JPH073429A5/ja
Application granted granted Critical
Publication of JP3105380B2 publication Critical patent/JP3105380B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP05149557A 1993-06-21 1993-06-21 耐デント性ならびに耐面ひずみ性に優れた深絞り用冷延鋼板の製造方法 Expired - Fee Related JP3105380B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP05149557A JP3105380B2 (ja) 1993-06-21 1993-06-21 耐デント性ならびに耐面ひずみ性に優れた深絞り用冷延鋼板の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP05149557A JP3105380B2 (ja) 1993-06-21 1993-06-21 耐デント性ならびに耐面ひずみ性に優れた深絞り用冷延鋼板の製造方法

Publications (3)

Publication Number Publication Date
JPH073429A JPH073429A (ja) 1995-01-06
JPH073429A5 true JPH073429A5 (enExample) 1999-12-21
JP3105380B2 JP3105380B2 (ja) 2000-10-30

Family

ID=15477778

Family Applications (1)

Application Number Title Priority Date Filing Date
JP05149557A Expired - Fee Related JP3105380B2 (ja) 1993-06-21 1993-06-21 耐デント性ならびに耐面ひずみ性に優れた深絞り用冷延鋼板の製造方法

Country Status (1)

Country Link
JP (1) JP3105380B2 (enExample)

Families Citing this family (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100895347B1 (ko) * 2003-12-09 2009-04-29 신닛뽄세이테쯔 카부시키카이샤 용기용 강판 및 그 제조 방법
CN1910296B (zh) * 2004-01-19 2011-08-31 新日本制铁株式会社 用于容器中的钢板及其制造方法
WO2006027854A1 (ja) * 2004-09-09 2006-03-16 Nippon Steel Corporation 極薄容器用の鋼板およびその製造方法
JP5541243B2 (ja) * 2011-07-15 2014-07-09 Jfeスチール株式会社 形状凍結性に優れた冷延鋼板およびその製造方法
JP5846113B2 (ja) * 2011-12-28 2016-01-20 Jfeスチール株式会社 耐デント性に優れた高強度薄鋼板およびその製造方法
IN2015KN00599A (enExample) * 2012-10-11 2015-07-17 Jfe Steel Corp

Similar Documents

Publication Publication Date Title
JP2016537502A (ja) 熱間成形鋼材
KR910004836A (ko) 강시이트의 제조방법
US4046601A (en) Method of nitride-strengthening low carbon steel articles
JPH05279802A (ja) ばね特性および加工部の疲労特性に優れたばね用ステンレス鋼およびその製造方法
US4011111A (en) High strength, deep drawing quality, low carbon steel, article formed therefrom, and method for production thereof
GB2060696A (en) Method for making shadow masks
JPH06100979A (ja) 高い張り剛性を有すると共にプレス成形性にも優れるプレス加工用薄鋼板
KR920009999A (ko) 자기특성과 피막특성이 개선된 일방향성 전자강판의 제조방법
JP2018512503A (ja) 熱間成形鋼材
JP2542535B2 (ja) 耐デント性の優れた深絞り用冷延鋼板の製造方法
JP3105380B2 (ja) 耐デント性ならびに耐面ひずみ性に優れた深絞り用冷延鋼板の製造方法
JPS62112720A (ja) Fe−Mn−Si系形状記憶合金の特性向上方法
JP2003268489A (ja) 熱処理用鋼板およびその製造方法
JP2623124B2 (ja) 窒化用鋼素材
JP3777049B2 (ja) 耐デント性ならびに耐面ひずみ性に優れた深絞り用bh冷延鋼板の製造方法
JP3115746B2 (ja) 耐デント性ならびに耐面ひずみ性に優れた非時効深絞り用冷延鋼板の製造方法
JP2001335908A5 (enExample)
JP3620384B2 (ja) 表面性状に優れた冷延鋼板およびその製造方法
JPH0598356A (ja) 焼き戻し省略型Ti−B系高炭素薄鋼板の製造方法
JPH0774412B2 (ja) 加工性および耐置き割れ性に優れた高強度薄鋼板およびその製造方法
JPH0598357A (ja) 焼き戻し省略型高炭素薄鋼板の製造方法
JPH08279408A5 (enExample)
JPH08311545A (ja) 缶用鋼板の製造方法
JPH0681044A5 (enExample)
JPH0681043A5 (enExample)