JPH0710832Y2 - 溶湯流路管 - Google Patents
溶湯流路管Info
- Publication number
- JPH0710832Y2 JPH0710832Y2 JP1988073718U JP7371888U JPH0710832Y2 JP H0710832 Y2 JPH0710832 Y2 JP H0710832Y2 JP 1988073718 U JP1988073718 U JP 1988073718U JP 7371888 U JP7371888 U JP 7371888U JP H0710832 Y2 JPH0710832 Y2 JP H0710832Y2
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- molten metal
- ceramic
- metal flow
- powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Continuous Casting (AREA)
- Casting Support Devices, Ladles, And Melt Control Thereby (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1988073718U JPH0710832Y2 (ja) | 1988-06-01 | 1988-06-01 | 溶湯流路管 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1988073718U JPH0710832Y2 (ja) | 1988-06-01 | 1988-06-01 | 溶湯流路管 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH01177057U JPH01177057U (enExample) | 1989-12-18 |
| JPH0710832Y2 true JPH0710832Y2 (ja) | 1995-03-15 |
Family
ID=31298850
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1988073718U Expired - Lifetime JPH0710832Y2 (ja) | 1988-06-01 | 1988-06-01 | 溶湯流路管 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0710832Y2 (enExample) |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57205377A (en) * | 1981-06-09 | 1982-12-16 | Toshiba Ceramics Co | Nitride refractories |
| JPS6178541A (ja) * | 1984-09-27 | 1986-04-22 | Mitsubishi Steel Mfg Co Ltd | ノズル |
-
1988
- 1988-06-01 JP JP1988073718U patent/JPH0710832Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH01177057U (enExample) | 1989-12-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP1479659A3 (en) | Bond coating for silicon based substrates such as silicon nitride | |
| JP2000203953A (ja) | 高炉樋用キャスタブル耐火物 | |
| JP3537642B2 (ja) | 連続鋳造用ノズル | |
| JPH10305357A (ja) | 連続鋳造用内挿式浸漬ノズル | |
| EP0846514B1 (en) | A continuous casting nozzle for casting molten steel | |
| EP0856369B1 (en) | Nozzle for continuous casting of steel | |
| US6479175B1 (en) | Ceramic composite | |
| JPH0753607B2 (ja) | 窒化硼素含有耐火物の製造方法 | |
| JP2002323486A (ja) | ダスト,スラグに対する難付着性評価試験方法 | |
| JP3232259B2 (ja) | 高炉主樋用不定形耐火物 | |
| JPH0643923B2 (ja) | 溶融金属の連続測温計 | |
| JPS6082256A (ja) | 溶融金属用ストツパ− | |
| JPH0240625B2 (enExample) | ||
| JPH08132191A (ja) | アルミナー炭素系鋳造用ノズル耐火物 | |
| JPH0635565B2 (ja) | 耐熱性接着剤又はコ−テイング剤 | |
| JP2004026564A (ja) | 高炉樋用不定形耐火物 | |
| JP2003238261A (ja) | 塩基性耐火モルタル | |
| JPH0735644Y2 (ja) | 鋳造用ストーク | |
| Kirianov et al. | Sintering and physicochemical properties of compositions in the SiC-Al sub 2 O sub 3-La sub 2 O sub 3-Cr sub 2 O sub 3 system. II. Oxidation resistance of pressureless sintered compact in the SiC-Al sub 2 O sub 3-LaO O sub 3-Cr sub 2 O sub 3 system | |
| TW494025B (en) | Stopper rod | |
| TW418140B (en) | Soft-bore monoblock pouring tube | |
| Yorita | QUALITIES OF FIRECLAY BRICK FOR AIR FURNACE AT AJIMU IN 1855-1868 | |
| JPS59175844U (ja) | 工業炉用ガスバ−ナ | |
| JP3476312B2 (ja) | ジルコニア−黒鉛質の連続鋳造用ノズル | |
| JP2002308677A (ja) | 黒鉛含有不定形耐火物用結合剤およびこれを用いた黒鉛含有不定形耐火物 |