JPH06248455A - ZrO2 膜の製造方法 - Google Patents
ZrO2 膜の製造方法Info
- Publication number
- JPH06248455A JPH06248455A JP3633393A JP3633393A JPH06248455A JP H06248455 A JPH06248455 A JP H06248455A JP 3633393 A JP3633393 A JP 3633393A JP 3633393 A JP3633393 A JP 3633393A JP H06248455 A JPH06248455 A JP H06248455A
- Authority
- JP
- Japan
- Prior art keywords
- substrate
- film
- zro2
- wavelength
- diketone complex
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Inorganic Compounds Of Heavy Metals (AREA)
- Chemical Vapour Deposition (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3633393A JPH06248455A (ja) | 1993-02-25 | 1993-02-25 | ZrO2 膜の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3633393A JPH06248455A (ja) | 1993-02-25 | 1993-02-25 | ZrO2 膜の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH06248455A true JPH06248455A (ja) | 1994-09-06 |
| JPH06248455A5 JPH06248455A5 (enExample) | 1997-05-13 |
Family
ID=12466907
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3633393A Pending JPH06248455A (ja) | 1993-02-25 | 1993-02-25 | ZrO2 膜の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH06248455A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2023157775A1 (ja) * | 2022-02-17 | 2023-08-24 | 日本軽金属株式会社 | 耐食性部材の製造方法及びレーザーcvd装置 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5625961A (en) * | 1979-07-07 | 1981-03-12 | British Petroleum Co | Protective metal oxide coating on surface of metal or alloy substrate sensitive to coking * corrosion or catalyst activity |
| JPH01503151A (ja) * | 1987-03-26 | 1989-10-26 | ジーイーシー ― マルコニ リミテッド | 薄層フィルム蒸着法 |
| JPH03111574A (ja) * | 1989-06-08 | 1991-05-13 | Schering Ag | 金属有機化合物のプラズマ反応により薄い酸化物層を製造する方法、薄い酸化物層、並びに保護層、導体層、半導体層、誘電性層及び帯電防止被膜の製法 |
-
1993
- 1993-02-25 JP JP3633393A patent/JPH06248455A/ja active Pending
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5625961A (en) * | 1979-07-07 | 1981-03-12 | British Petroleum Co | Protective metal oxide coating on surface of metal or alloy substrate sensitive to coking * corrosion or catalyst activity |
| JPH01503151A (ja) * | 1987-03-26 | 1989-10-26 | ジーイーシー ― マルコニ リミテッド | 薄層フィルム蒸着法 |
| JPH03111574A (ja) * | 1989-06-08 | 1991-05-13 | Schering Ag | 金属有機化合物のプラズマ反応により薄い酸化物層を製造する方法、薄い酸化物層、並びに保護層、導体層、半導体層、誘電性層及び帯電防止被膜の製法 |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2023157775A1 (ja) * | 2022-02-17 | 2023-08-24 | 日本軽金属株式会社 | 耐食性部材の製造方法及びレーザーcvd装置 |
| JP2023119686A (ja) * | 2022-02-17 | 2023-08-29 | 日本軽金属株式会社 | 耐食性部材の製造方法及びレーザーcvd装置 |
| US20250101591A1 (en) * | 2022-02-17 | 2025-03-27 | Nippon Light Metal Company, Ltd. | Corrosion-resistant member production method and laser cvd device |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4675089A (en) | Low temperature deposition method for high quality aluminum oxide films | |
| JPS6289873A (ja) | 透明導電膜形成方法 | |
| GB2295401A (en) | Monocrystalline diamond films | |
| JP2002532900A (ja) | 酸窒化ケイ素膜 | |
| EP0275267B1 (en) | Process for photochemical vapor deposition of oxide layers at enhanced deposition rates | |
| US4645687A (en) | Deposition of III-V semiconductor materials | |
| JP2663471B2 (ja) | 絶縁薄膜の製造方法 | |
| EP0967008A2 (en) | Film of titanium dioxide containing silicon dioxide and a method of forming the same | |
| CN2550376Y (zh) | 一种多功能的等离子体和激光束联合处理材料的装置 | |
| JP2758247B2 (ja) | 有機金属ガス利用薄膜形成装置 | |
| JPH06248455A5 (enExample) | ||
| JPH08115912A (ja) | 窒化ケイ素薄膜の作製方法 | |
| JPH04362017A (ja) | 配向性Ta2O5薄膜の作製方法 | |
| JPH01294506A (ja) | エキシマレーザーによる金属酸化物および金属酸化物薄膜の製造方法 | |
| JP3550658B2 (ja) | 結晶構造の制御された二酸化チタン系薄膜の製造方法 | |
| JPH0420982B2 (enExample) | ||
| JP3534676B2 (ja) | Cu又はCu含有膜の形成方法、及び装置 | |
| JPS59129774A (ja) | 選択的窒化膜の作製方法 | |
| JPH04182317A (ja) | 酸化物超電導薄膜の作製方法 | |
| JPH08134654A (ja) | 金属化合物薄膜の成膜方法及びそのパタ−ニング方法 | |
| JPH07309695A (ja) | チタン酸鉛及びチタン酸ジルコン酸鉛薄膜の製造方法 | |
| RU2040072C1 (ru) | Способ получения тонких пленок диоксида кремния | |
| JPH07258851A (ja) | 金属化合物薄膜のパタ−ニング方法 | |
| JP2606063B2 (ja) | 有機金錯体による金膜の形成方法 | |
| JPS62271437A (ja) | 絶縁膜の形成方法 |