JPH06111816A5 - - Google Patents
Info
- Publication number
- JPH06111816A5 JPH06111816A5 JP4-262487A JP26248792A JPH06111816A5 JP H06111816 A5 JPH06111816 A5 JP H06111816A5 JP 26248792 A JP26248792 A JP 26248792A JP H06111816 A5 JPH06111816 A5 JP H06111816A5
- Authority
- JP
- Japan
- Prior art keywords
- active material
- nickel
- positive electrode
- battery
- electrode plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP26248792A JP3182228B2 (ja) | 1992-09-30 | 1992-09-30 | アルカリ蓄電池用非焼結式正極板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP26248792A JP3182228B2 (ja) | 1992-09-30 | 1992-09-30 | アルカリ蓄電池用非焼結式正極板の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH06111816A JPH06111816A (ja) | 1994-04-22 |
| JPH06111816A5 true JPH06111816A5 (enExample) | 1999-09-24 |
| JP3182228B2 JP3182228B2 (ja) | 2001-07-03 |
Family
ID=17376479
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP26248792A Expired - Fee Related JP3182228B2 (ja) | 1992-09-30 | 1992-09-30 | アルカリ蓄電池用非焼結式正極板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3182228B2 (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2021184392A1 (en) * | 2020-03-20 | 2021-09-23 | Guangdong Haozhi Technology Co. Limited | Method of preparing cathode for secondary battery |
| KR102628735B1 (ko) * | 2020-03-20 | 2024-01-23 | 쥐알에스티 인터내셔널 리미티드 | 2차 전지용 캐소드의 제조 방법 |
-
1992
- 1992-09-30 JP JP26248792A patent/JP3182228B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| WO2001073872A1 (en) | Rechargeable battery | |
| JPH11238509A (ja) | アルカリ蓄電池用ニッケル電極活物質とそれを用いたニッケル正極 | |
| JP2004538609A (ja) | 亜鉛正極を有するアルカリ二次電気化学発電装置 | |
| JPH0521064A5 (enExample) | ||
| JP3182228B2 (ja) | アルカリ蓄電池用非焼結式正極板の製造方法 | |
| JPH0447676A (ja) | 密閉型蓄電池の製造法 | |
| JP3204275B2 (ja) | アルカリ蓄電池用ニッケル電極 | |
| JP3338226B2 (ja) | アルカリ蓄電池用非焼結式ニッケル極 | |
| KR100205136B1 (ko) | 니켈 계열 전지의 양극용 활물질 및 이의 제조 방법 | |
| JP3788484B2 (ja) | アルカリ蓄電池用ニッケル電極 | |
| US6329100B1 (en) | Hydrogen absorbing alloy electrode and process for producing same | |
| JP3214569B2 (ja) | 水素化物二次電池の製造方法 | |
| EP1093673A1 (en) | Active electrode compositions comprising raney based catalysts and materials | |
| JPS62140359A (ja) | 電池用電極 | |
| JP2968360B2 (ja) | 水素化物二次電池の製造方法 | |
| JPH10172559A (ja) | アルカリ蓄電池用ニッケル活物質およびその製造方法 | |
| JPH1021904A (ja) | アルカリ蓄電池 | |
| JP2981537B2 (ja) | アルカリ電池用負極 | |
| JP3292204B2 (ja) | アルカリ蓄電池用ニッケル焼結式電極 | |
| JP2001266860A (ja) | ニッケル−水素蓄電池 | |
| JP2589750B2 (ja) | ニッケルカドミウム蓄電池 | |
| JPH0845506A5 (enExample) | ||
| JP2638055B2 (ja) | アルカリ蓄電池用ペースト式カドミウム負極の製造法 | |
| JP2999277B2 (ja) | 水素化物二次電池およびその製造方法 | |
| JP2810460B2 (ja) | アルカリ蓄電池用正極板 |