JPH0588841B2 - - Google Patents
Info
- Publication number
- JPH0588841B2 JPH0588841B2 JP689187A JP689187A JPH0588841B2 JP H0588841 B2 JPH0588841 B2 JP H0588841B2 JP 689187 A JP689187 A JP 689187A JP 689187 A JP689187 A JP 689187A JP H0588841 B2 JPH0588841 B2 JP H0588841B2
- Authority
- JP
- Japan
- Prior art keywords
- polymerization
- scale
- polymerization vessel
- acid
- vinyl
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Polymerisation Methods In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP689187A JPS63175002A (ja) | 1987-01-14 | 1987-01-14 | ビニル系重合体の製法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP689187A JPS63175002A (ja) | 1987-01-14 | 1987-01-14 | ビニル系重合体の製法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63175002A JPS63175002A (ja) | 1988-07-19 |
| JPH0588841B2 true JPH0588841B2 (enExample) | 1993-12-24 |
Family
ID=11650851
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP689187A Granted JPS63175002A (ja) | 1987-01-14 | 1987-01-14 | ビニル系重合体の製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63175002A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0460458B1 (en) * | 1990-05-25 | 1995-10-18 | Shin-Etsu Chemical Co., Ltd. | Method of preventing polymer scale deposition and polymer scale preventive agent used therefor |
| DE10131764A1 (de) * | 2001-06-30 | 2003-01-09 | Cognis Deutschland Gmbh | Verwendung von Fluoralkansulfonsäuren zur Stabilisierung von halogenhaltigen organischen Kunststoffen |
-
1987
- 1987-01-14 JP JP689187A patent/JPS63175002A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS63175002A (ja) | 1988-07-19 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH0138121B2 (enExample) | ||
| JPH02228303A (ja) | 重合体スケールの付着防止方法 | |
| JPH0431402A (ja) | 重合体スケールの付着防止方法およびこの方法で用いる重合体スケール付着防止用塗布液 | |
| US5292834A (en) | Method of preventing polymer scale deposition | |
| JP3375844B2 (ja) | 重合体スケール付着防止剤およびそれを用いた塩化ビニル系重合体の製造方法 | |
| JPS63175002A (ja) | ビニル系重合体の製法 | |
| US5397849A (en) | Process for preventing polymer scale using an alkaline solution of a condensation product of an aromatic compound having at least two amino groups and an aromatic bisester anhydride | |
| JPH03115305A (ja) | 重合体スケールの付着防止方法および重合体スケール付着防止剤 | |
| JP2764654B2 (ja) | 重合体スケール付着防止剤および重合体スケールの付着防止方法 | |
| JPS6356884B2 (enExample) | ||
| JP2727393B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| US5393857A (en) | Polymer scale preventive agent | |
| JP2719842B2 (ja) | 重合体スケールの付着防止方法および重合体スケール付着防止剤 | |
| JP2639775B2 (ja) | 重合体スケール付着防止剤、重合体スケールの付着防止に有効な重合器及びそれを利用する重合体の製造方法 | |
| JPS629123B2 (enExample) | ||
| JP2962617B2 (ja) | 重合体スケール付着防止剤、重合体スケールの付着を防止する重合器及びそれを使用する重合体製造方法 | |
| JP3272907B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体の製造方法 | |
| JP3276498B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| JP2764653B2 (ja) | 重合体スケール付着防止剤および重合体スケールの付着防止方法 | |
| JP3251412B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| JP3260953B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| JP3197434B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| JP3251411B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| JP2727401B2 (ja) | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 | |
| JPS6152162B2 (enExample) |