JPH0566713B2 - - Google Patents
Info
- Publication number
- JPH0566713B2 JPH0566713B2 JP60244757A JP24475785A JPH0566713B2 JP H0566713 B2 JPH0566713 B2 JP H0566713B2 JP 60244757 A JP60244757 A JP 60244757A JP 24475785 A JP24475785 A JP 24475785A JP H0566713 B2 JPH0566713 B2 JP H0566713B2
- Authority
- JP
- Japan
- Prior art keywords
- positive electrode
- filled
- lead powder
- paste
- electrode plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/14—Electrodes for lead-acid accumulators
- H01M4/16—Processes of manufacture
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60244757A JPS62103974A (ja) | 1985-10-30 | 1985-10-30 | クラツド式鉛電池正極板 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60244757A JPS62103974A (ja) | 1985-10-30 | 1985-10-30 | クラツド式鉛電池正極板 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62103974A JPS62103974A (ja) | 1987-05-14 |
JPH0566713B2 true JPH0566713B2 (enrdf_load_stackoverflow) | 1993-09-22 |
Family
ID=17123443
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP60244757A Granted JPS62103974A (ja) | 1985-10-30 | 1985-10-30 | クラツド式鉛電池正極板 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62103974A (enrdf_load_stackoverflow) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP5407271B2 (ja) * | 2008-10-23 | 2014-02-05 | パナソニック株式会社 | 鉛蓄電池用正極板の製造方法、鉛蓄電池の製造方法および鉛蓄電池 |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS591969A (ja) * | 1982-06-28 | 1984-01-07 | 株式会社東芝 | 空気調和機 |
JPS5951466A (ja) * | 1982-09-18 | 1984-03-24 | Japan Storage Battery Co Ltd | 鉛蓄電池用正極板 |
JPS59121560A (ja) * | 1982-12-28 | 1984-07-13 | Fujitsu Ltd | フロツピ−デイスクの読出制御方式 |
-
1985
- 1985-10-30 JP JP60244757A patent/JPS62103974A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS62103974A (ja) | 1987-05-14 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPH0566713B2 (enrdf_load_stackoverflow) | ||
JPH01128367A (ja) | 密閉形鉛蓄電池 | |
JPH05242887A (ja) | 鉛蓄電池用極板の製造方法 | |
JPS61269853A (ja) | クラツド式鉛電池正極板 | |
JP3414941B2 (ja) | 鉛蓄電池用極板およびその製造方法 | |
JPH01124958A (ja) | 密閉形鉛蓄電池 | |
JPH11329420A (ja) | 鉛蓄電池の製造方法 | |
JPS61269855A (ja) | クラツド式鉛電池正極板 | |
JPS61264675A (ja) | クラツド式鉛電池正極板 | |
JP2000149932A (ja) | 鉛蓄電池およびその製造方法 | |
JP2815439B2 (ja) | 密閉形鉛蓄電池 | |
JPH0414760A (ja) | 鉛蓄電池 | |
JPH088104B2 (ja) | 密閉形鉛蓄電池 | |
JPS6028171A (ja) | 鉛蓄電池用ペ−スト式極板の製造法 | |
JPS6030054A (ja) | ペ−スト式鉛蓄電池極板の製造法 | |
JPS6322414B2 (enrdf_load_stackoverflow) | ||
JPS62150653A (ja) | クラツド式鉛電池正極板 | |
JPH04229556A (ja) | 鉛蓄電池用極板及び凝集粒の製造方法 | |
JPS61114473A (ja) | クラツド式鉛電池正極板 | |
JP2815440B2 (ja) | 密閉形鉛蓄電池 | |
JPS607062A (ja) | 鉛蓄電池用陰極板の製造法 | |
JPS6161228B2 (enrdf_load_stackoverflow) | ||
JPS6155749B2 (enrdf_load_stackoverflow) | ||
JPH08180857A (ja) | 鉛蓄電池用極板 | |
JPH0193055A (ja) | 鉛蓄電池の製造法 |