JPH0470385B2 - - Google Patents
Info
- Publication number
- JPH0470385B2 JPH0470385B2 JP61045819A JP4581986A JPH0470385B2 JP H0470385 B2 JPH0470385 B2 JP H0470385B2 JP 61045819 A JP61045819 A JP 61045819A JP 4581986 A JP4581986 A JP 4581986A JP H0470385 B2 JPH0470385 B2 JP H0470385B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- less
- toughness
- hot forging
- effect
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4581986A JPS62202054A (ja) | 1986-03-03 | 1986-03-03 | 熱間鍛造用非調質鋼 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4581986A JPS62202054A (ja) | 1986-03-03 | 1986-03-03 | 熱間鍛造用非調質鋼 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62202054A JPS62202054A (ja) | 1987-09-05 |
JPH0470385B2 true JPH0470385B2 (enrdf_load_stackoverflow) | 1992-11-10 |
Family
ID=12729855
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4581986A Granted JPS62202054A (ja) | 1986-03-03 | 1986-03-03 | 熱間鍛造用非調質鋼 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62202054A (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO1998013529A1 (fr) * | 1996-09-27 | 1998-04-02 | Kawasaki Steel Corporation | Acier non traite a chaud, de haute resistance et haute tenacite, presentant une excellente usinabilite |
WO2010010649A1 (ja) | 2008-07-23 | 2010-01-28 | Takahashi Yoshiaki | 摩擦抵抗低減船およびその運転方法 |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2515173B2 (ja) * | 1990-09-28 | 1996-07-10 | 愛知製鋼株式会社 | 高強度、高靭性鍛造用非調質鋼 |
JP3139876B2 (ja) * | 1993-04-05 | 2001-03-05 | 新日本製鐵株式会社 | 熱間鍛造用非調質鋼および非調質熱間鍛造品の製造方法ならびに非調質熱間鍛造品 |
US5922145A (en) * | 1996-11-25 | 1999-07-13 | Sumitomo Metal Industries, Ltd. | Steel products excellent in machinability and machined steel parts |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS543126B2 (enrdf_load_stackoverflow) * | 1972-12-26 | 1979-02-19 | ||
JPS5524932A (en) * | 1978-08-08 | 1980-02-22 | Nippon Steel Corp | Manufacture of bainite tough hardening steel |
JPS5719324A (en) * | 1980-05-30 | 1982-02-01 | Nippon Steel Corp | Production of steel for machine structural use for forging having fine structure at high temperature |
JPS57200541A (en) * | 1981-06-04 | 1982-12-08 | Nippon Steel Corp | Forged direct tempering steel excellent in tenacity |
-
1986
- 1986-03-03 JP JP4581986A patent/JPS62202054A/ja active Granted
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO1998013529A1 (fr) * | 1996-09-27 | 1998-04-02 | Kawasaki Steel Corporation | Acier non traite a chaud, de haute resistance et haute tenacite, presentant une excellente usinabilite |
WO2010010649A1 (ja) | 2008-07-23 | 2010-01-28 | Takahashi Yoshiaki | 摩擦抵抗低減船およびその運転方法 |
US7677191B2 (en) | 2008-07-23 | 2010-03-16 | Yoshiaki Takahashi | Frictional resistance reduction ship and operation method |
Also Published As
Publication number | Publication date |
---|---|
JPS62202054A (ja) | 1987-09-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN111511936B (zh) | 用于冷镦的线材、使用其的加工产品、及其制造方法 | |
EP3926065A1 (en) | Hot work die steel, heat treatment method thereof and hot work die | |
CN112877591B (zh) | 一种高强韧五金工具及链条用钢及其制造方法 | |
JPH0892690A (ja) | 耐疲労特性に優れた浸炭部品およびその製造方法 | |
EP0648853A1 (en) | Non-heat-treated steel for hot forging, process for producing non-heat-treated hot forging, and non-heat-treated hot forging | |
JP3036416B2 (ja) | 高疲労強度を有する熱間鍛造非調質鋼および鍛造品の製造方法 | |
JP3327635B2 (ja) | 疲労強度に優れた熱間鍛造用非調質鋼材及びその鋼材を用いた非調質熱間鍛造品の製造方法 | |
JPH09170017A (ja) | 高強度高靭性鋼板の製造方法 | |
JPH0925539A (ja) | 強度と靭性に優れた快削非調質鋼 | |
CN114134387A (zh) | 一种抗拉强度1300MPa级厚规格超高强钢板及其制造方法 | |
JPS62207821A (ja) | 熱間鍛造用非調質鋼の製造方法 | |
JP3422865B2 (ja) | 高強度マルテンサイト系ステンレス鋼部材の製造方法 | |
JPH0470385B2 (enrdf_load_stackoverflow) | ||
JPH0472886B2 (enrdf_load_stackoverflow) | ||
JPH11124623A (ja) | 含ボロン冷間鍛造用鋼材の製造方法 | |
JPH0425343B2 (enrdf_load_stackoverflow) | ||
JPH11131187A (ja) | 迅速黒鉛化鋼および迅速黒鉛化鋼の製造方法 | |
JP2518873B2 (ja) | 熱処理用鋼板 | |
KR101140911B1 (ko) | 조질합금강급 V-Free비조질강의 제조방법 | |
JPS63161117A (ja) | 高強度高靭性熱間圧延鋼材の製造方法 | |
JP3042574B2 (ja) | 高疲労強度を有する熱間鍛造品及びその製造方法 | |
JPH0813028A (ja) | 析出硬化型高張力高靱性鋼材の製造方法 | |
JP2000160285A (ja) | 高強度高靱性非調質鋼材 | |
JP2767254B2 (ja) | Cr−Mo肌焼鋼の製造方法 | |
JP3468875B2 (ja) | 高強度高靭性鋼の製造方法 |