JPH044975B2 - - Google Patents

Info

Publication number
JPH044975B2
JPH044975B2 JP12573784A JP12573784A JPH044975B2 JP H044975 B2 JPH044975 B2 JP H044975B2 JP 12573784 A JP12573784 A JP 12573784A JP 12573784 A JP12573784 A JP 12573784A JP H044975 B2 JPH044975 B2 JP H044975B2
Authority
JP
Japan
Prior art keywords
alkali metal
boron
titanate
atmosphere
metal titanate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP12573784A
Other languages
English (en)
Japanese (ja)
Other versions
JPS616125A (ja
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP12573784A priority Critical patent/JPS616125A/ja
Publication of JPS616125A publication Critical patent/JPS616125A/ja
Publication of JPH044975B2 publication Critical patent/JPH044975B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Inorganic Compounds Of Heavy Metals (AREA)
  • Crystals, And After-Treatments Of Crystals (AREA)
JP12573784A 1984-06-19 1984-06-19 還元チタン酸アルカリ金属塩の製法 Granted JPS616125A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP12573784A JPS616125A (ja) 1984-06-19 1984-06-19 還元チタン酸アルカリ金属塩の製法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP12573784A JPS616125A (ja) 1984-06-19 1984-06-19 還元チタン酸アルカリ金属塩の製法

Publications (2)

Publication Number Publication Date
JPS616125A JPS616125A (ja) 1986-01-11
JPH044975B2 true JPH044975B2 (de) 1992-01-30

Family

ID=14917537

Family Applications (1)

Application Number Title Priority Date Filing Date
JP12573784A Granted JPS616125A (ja) 1984-06-19 1984-06-19 還元チタン酸アルカリ金属塩の製法

Country Status (1)

Country Link
JP (1) JPS616125A (de)

Also Published As

Publication number Publication date
JPS616125A (ja) 1986-01-11

Similar Documents

Publication Publication Date Title
Wu et al. All-solid-state lithium batteries with sulfide electrolytes and oxide cathodes
Liu et al. Salt melt synthesis of ceramics, semiconductors and carbon nanostructures
CN109755641A (zh) 一种复合材料及其制备方法及锂离子电池
CN114267874A (zh) 含卤化锂包覆层的硫银锗矿型硫化物固体电解质及其制备
Zheng et al. Synthesis and characterization of Li7La3Zr2O12 via a novel solid-liquid route
JPH0512320B2 (de)
CN101891193B (zh) 一种溶胶凝胶法制备纳米碳化钒
Nadimi et al. Formation reaction kinetics of nanocrystalline TiC via molten LiCl–KCl applying shrinking core model
JPH08337500A (ja) 酸化スズウィスカおよびその製造方法
CN114956085A (zh) 一种低温熔融盐体系制备抗氧化MXene的方法
CN114956084A (zh) 一种Al掺杂的MXene的制备方法
JPH044975B2 (de)
JPH0575698B2 (de)
US4609694A (en) Process for preparing metamorphosed alkaline titanates
JPH0522649B2 (de)
JPH0352411B2 (de)
JP4252054B2 (ja) 超伝導セラミックス薄膜の形成方法
JP3256570B2 (ja) 導電性物質の製造法
JPH0433732B2 (de)
Perthuis et al. Li+ eucryptite superionic conductors thick films
Jiao et al. A route for producing nano-CaRuO3 perovskite by combusting precursors prepared using reverse micelle synthesis
JPS6131316A (ja) 還元チタン酸アルカリ金属塩の製造法
Feng et al. Fabrication plate-like BaBi4Ti4 O 1 5 single-crystalline particles by the molten salt synthesis method
JPS63256564A (ja) 鱗片状酸化物超伝導性セラミツクス及びその製造方法
WO2022158127A1 (ja) 窒化ホウ素の製造方法