JPH04319256A5 - - Google Patents
Info
- Publication number
- JPH04319256A5 JPH04319256A5 JP3-85112A JP8511291A JPH04319256A5 JP H04319256 A5 JPH04319256 A5 JP H04319256A5 JP 8511291 A JP8511291 A JP 8511291A JP H04319256 A5 JPH04319256 A5 JP H04319256A5
- Authority
- JP
- Japan
- Prior art keywords
- neodymium
- rare earth
- praseodymium
- amendment
- hydrogen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP08511291A JP3238930B2 (ja) | 1991-04-17 | 1991-04-17 | 金属−水素アルカリ蓄電池の製造方法 |
| US07/756,496 US5108851A (en) | 1991-04-17 | 1991-09-09 | Metal-hydrogen alkaline storage cell |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP08511291A JP3238930B2 (ja) | 1991-04-17 | 1991-04-17 | 金属−水素アルカリ蓄電池の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH04319256A JPH04319256A (ja) | 1992-11-10 |
| JPH04319256A5 true JPH04319256A5 (enExample) | 1999-05-28 |
| JP3238930B2 JP3238930B2 (ja) | 2001-12-17 |
Family
ID=13849545
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP08511291A Expired - Lifetime JP3238930B2 (ja) | 1991-04-17 | 1991-04-17 | 金属−水素アルカリ蓄電池の製造方法 |
Country Status (2)
| Country | Link |
|---|---|
| US (1) | US5108851A (enExample) |
| JP (1) | JP3238930B2 (enExample) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR2698881B1 (fr) * | 1992-12-04 | 1995-01-13 | Accumulateurs Fixes | Matériau hydrurable pour électrode négative d'accumulateur nickel-hydrure. |
| JPH06338344A (ja) * | 1993-05-31 | 1994-12-06 | Sanyo Electric Co Ltd | 密閉形ニッケル・金属水素化物アルカリ蓄電池 |
| US5368614A (en) * | 1994-03-21 | 1994-11-29 | Hughes Aircraft Company | Preparation of polymer-impregnated battery separator material and cell made therewith |
| US5645953A (en) * | 1994-05-04 | 1997-07-08 | Hyundai Motor Company, Ltd. | Secondary battery and method for controlling the self-discharge of a nickel/metal hydride secondary battery |
| US7725980B2 (en) * | 2004-12-15 | 2010-06-01 | Colgate-Palmolive Company | Oral care implement |
| US7763160B2 (en) * | 2003-12-19 | 2010-07-27 | Shell Oil Company | Systems and methods of producing a crude product |
Family Cites Families (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3959018A (en) * | 1972-11-27 | 1976-05-25 | Communications Satellite Corporation | Low pressure nickel hydrogen cell |
| US4623597A (en) * | 1982-04-28 | 1986-11-18 | Energy Conversion Devices, Inc. | Rechargeable battery and electrode used therein |
| US4621034A (en) * | 1984-07-31 | 1986-11-04 | Kabushiki Kaisha Toshiba | Sealed metal oxide-hydrogen storage cell |
| US4696873A (en) * | 1985-06-21 | 1987-09-29 | Kabushiki Kaisha Toshiba | Rechargeable electrochemical cell with a negative electrode comprising a hydrogen absorbing alloy including rare earth component |
| US4728586A (en) * | 1986-12-29 | 1988-03-01 | Energy Conversion Devices, Inc. | Enhanced charge retention electrochemical hydrogen storage alloys and an enhanced charge retention electrochemical cell |
| US5006328A (en) * | 1987-11-17 | 1991-04-09 | Kuochih Hong | Method for preparing materials for hydrogen storage and for hydride electrode applications |
| EP0342654B1 (en) * | 1988-05-17 | 1993-09-15 | Mitsubishi Materials Corporation | Hydrogen absorbing ni-based alloy and rechargeable alkaline battery |
| US4898794A (en) * | 1988-12-27 | 1990-02-06 | Mitsubishi Metal Corporation | Hydrogen absorbing Ni,Zr-based alloy and rechargeable alkaline battery |
-
1991
- 1991-04-17 JP JP08511291A patent/JP3238930B2/ja not_active Expired - Lifetime
- 1991-09-09 US US07/756,496 patent/US5108851A/en not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN102618883A (zh) | 一种粗铅直接电解精炼的方法 | |
| CN112921360B (zh) | 一种熔盐电解制备稀土金属的方法 | |
| PL357637A1 (en) | Alloy for thin positive grid for lead acid batteries and method for manufacture of grid | |
| GB923066A (en) | Improved magnesium primary electric cell anode and magnesium primary electric cell | |
| JPH06179936A (ja) | アルミニウム電池用負極材料 | |
| US4253871A (en) | Alloys for making electrode supports in lead accumulators | |
| DE3064153D1 (en) | Process for reducing lead peroxide formation during lead electrowinning and an electrolyte for electrowinning lead | |
| GB2152951A (en) | Process for reductive plutonium stripping from an organic reprocessing solution into an aqueous, nitric acid solution by use of electrolytic current | |
| US3565695A (en) | Method of forming an amalgamated zinc electrode | |
| GB1400339A (en) | Wrought lead-calcium and lead-calcium-tin alloys | |
| US3257201A (en) | Aluminum alloy | |
| JP2832229B2 (ja) | アルカリ電池用亜鉛合金粉末およびその製造方法 | |
| JP2832231B2 (ja) | アルカリ電池用亜鉛合金粉末およびその製造方法 | |
| JPS51131474A (en) | An activated cathode | |
| JP2005108816A5 (ja) | アルカリ蓄電池用水素吸蔵合金及びアルカリ蓄電池 | |
| JPH0757734A5 (enExample) | ||
| DE3518421A1 (de) | Zinkchloridzelle | |
| JPH05156482A5 (enExample) | ||
| JPS5534110A (en) | Activated carbon regenerating method | |
| JPH0285332A (ja) | 電気防食に使用される流電陽極用マグネシウム合金 | |
| SU456852A1 (ru) | Способ корректировки электролита | |
| JPH0777128B2 (ja) | 水素吸蔵合金 | |
| SU523943A1 (ru) | Смесь дл модифицировани сталей и сплавов | |
| KR0127040B1 (ko) | 납축전지의 전해액 조성물 | |
| Timmins | World Review of Magnesium Supply and Demand |