JPH0428779B2 - - Google Patents
Info
- Publication number
- JPH0428779B2 JPH0428779B2 JP60055531A JP5553185A JPH0428779B2 JP H0428779 B2 JPH0428779 B2 JP H0428779B2 JP 60055531 A JP60055531 A JP 60055531A JP 5553185 A JP5553185 A JP 5553185A JP H0428779 B2 JPH0428779 B2 JP H0428779B2
- Authority
- JP
- Japan
- Prior art keywords
- toughness
- tempered
- seamless steel
- tempering
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5553185A JPS61213344A (ja) | 1985-03-18 | 1985-03-18 | 高靭性シ−ムレス鋼管 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5553185A JPS61213344A (ja) | 1985-03-18 | 1985-03-18 | 高靭性シ−ムレス鋼管 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61213344A JPS61213344A (ja) | 1986-09-22 |
JPH0428779B2 true JPH0428779B2 (enrdf_load_stackoverflow) | 1992-05-15 |
Family
ID=13001309
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP5553185A Granted JPS61213344A (ja) | 1985-03-18 | 1985-03-18 | 高靭性シ−ムレス鋼管 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61213344A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE102005046459B4 (de) * | 2005-09-21 | 2013-11-28 | MHP Mannesmann Präzisrohr GmbH | Verfahren zur Herstellung von kaltgefertigten Präzisionsstahlrohren |
CN102615476A (zh) * | 2012-01-19 | 2012-08-01 | 南京理工大学 | 深海用x70级大口径厚壁无缝管及其制造方法 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS54112369A (en) * | 1978-02-23 | 1979-09-03 | Nippon Steel Corp | Electric welded steel tube provided with high toughness electric welded zone |
JPS54127824A (en) * | 1978-03-28 | 1979-10-04 | Kawasaki Steel Co | Steel material for electric seam pipe having good hook crack resistance |
-
1985
- 1985-03-18 JP JP5553185A patent/JPS61213344A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS61213344A (ja) | 1986-09-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP2567150B2 (ja) | 低温用高強度低降伏比ラインパイプ材の製造法 | |
JP2834654B2 (ja) | 高靱性熱間工具鋼 | |
JPH02250941A (ja) | 低炭素クロムモリブデン鋼及びその製造方法 | |
JP3077567B2 (ja) | 低温鉄筋用鋼材の製造方法 | |
JP3579307B2 (ja) | 溶接性及び歪時効後の靭性に優れた60キロ級直接焼入れ焼戻し鋼 | |
JPH0428779B2 (enrdf_load_stackoverflow) | ||
JP2500948B2 (ja) | 溶接性の優れた厚手80kgf/mm2 級高張力鋼の製造法 | |
JPS5920423A (ja) | 低温靭性の優れた80kgf/mm2級継目無鋼管の製造方法 | |
JPH083636A (ja) | 低降伏比高靱性鋼の製造方法 | |
JPS613833A (ja) | 溶接性にすぐれた高強度鋼の製造方法 | |
JPH0826395B2 (ja) | 溶接性の優れた80Kgf/mm▲上2▼級高張力鋼の製造法 | |
JPH048486B2 (enrdf_load_stackoverflow) | ||
JP3033459B2 (ja) | 非調質高張力鋼の製造方法 | |
JP3007246B2 (ja) | 溶接性の優れた降伏比80%以下の590N/mm2級高張力鋼の製造法 | |
JP3297090B2 (ja) | 降伏比上昇の少ない高張力鋼材の加工方法 | |
JP2529042B2 (ja) | 冷間成形による建築用低降伏比鋼管の製造法 | |
JPS62149845A (ja) | 溶接部じん性のすぐれたCu析出型鋼材とその製造方法 | |
JPH06145787A (ja) | 溶接性に優れた高張力鋼の製造方法 | |
JPS63206449A (ja) | 冷間圧造用低炭素鋼 | |
JPH04232209A (ja) | 耐ssc性の優れた油井用鋼管の製造法 | |
JP3062275B2 (ja) | 高強度軸部品用鋼材 | |
JP3007247B2 (ja) | 溶接性の優れた降伏比80%以下のTS590N/mm2級高張力鋼の製造法 | |
JP3426047B2 (ja) | 溶接性の優れた低降伏比590N/mm2 級高張力鋼の製造方法 | |
JPS6254019A (ja) | 溶接性および低温靭性に優れた80キロ級極厚高張力鋼板の製造方法 | |
JPH06279919A (ja) | 圧力容器用Cr−Mo鋼板及びその製造法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |