JPH0377848B2 - - Google Patents
Info
- Publication number
- JPH0377848B2 JPH0377848B2 JP61077551A JP7755186A JPH0377848B2 JP H0377848 B2 JPH0377848 B2 JP H0377848B2 JP 61077551 A JP61077551 A JP 61077551A JP 7755186 A JP7755186 A JP 7755186A JP H0377848 B2 JPH0377848 B2 JP H0377848B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- resistance
- strength
- content
- welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Arc Welding In General (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7755186A JPS6250443A (ja) | 1986-04-05 | 1986-04-05 | 湿り蒸気下で使用する原子力発電給水加熱器用の耐E.C.性に優れる溶接性の良好な低C―低Si―Cr―Mo鋼材の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP7755186A JPS6250443A (ja) | 1986-04-05 | 1986-04-05 | 湿り蒸気下で使用する原子力発電給水加熱器用の耐E.C.性に優れる溶接性の良好な低C―低Si―Cr―Mo鋼材の製造方法 |
Related Parent Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2697681A Division JPS57143467A (en) | 1981-02-27 | 1981-02-27 | Low c-low si-cr-mo steel used in wet vapor |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6250443A JPS6250443A (ja) | 1987-03-05 |
| JPH0377848B2 true JPH0377848B2 (enExample) | 1991-12-11 |
Family
ID=13637150
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP7755186A Granted JPS6250443A (ja) | 1986-04-05 | 1986-04-05 | 湿り蒸気下で使用する原子力発電給水加熱器用の耐E.C.性に優れる溶接性の良好な低C―低Si―Cr―Mo鋼材の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6250443A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR102204996B1 (ko) * | 2020-07-21 | 2021-01-18 | 김구 | 매연 여과 필터 건조장치 및 방법 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6035423B2 (ja) * | 1977-03-11 | 1985-08-14 | 日本鋼管株式会社 | Sr脆化抵抗性の優れた鋼材 |
| JPS5853712B2 (ja) * | 1979-06-06 | 1983-11-30 | 川崎製鉄株式会社 | 焼戻軟化抵抗性にすぐれたクロム・モリブデン鋼 |
-
1986
- 1986-04-05 JP JP7755186A patent/JPS6250443A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR102204996B1 (ko) * | 2020-07-21 | 2021-01-18 | 김구 | 매연 여과 필터 건조장치 및 방법 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6250443A (ja) | 1987-03-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP3565331B2 (ja) | 高強度低合金耐熱鋼 | |
| JPS629646B2 (enExample) | ||
| JP5630322B2 (ja) | 靭性に優れる高張力鋼板とその製造方法 | |
| JPWO2006112428A1 (ja) | 低合金鋼 | |
| CN108637525A (zh) | 一种可免焊后去应力处理的低合金高强度钢用埋弧焊丝 | |
| JPS6151009B2 (enExample) | ||
| EP1070763A1 (en) | HIGH Cr STEEL PIPE FOR LINE PIPE | |
| JPS6254062A (ja) | 湿り蒸気下で使用する低C−Cr−Mo鋼 | |
| JP2659813B2 (ja) | 高強度低合金耐熱鋼の製造方法 | |
| JP4276341B2 (ja) | 引張強さ570〜720N/mm2の溶接熱影響部と母材の硬さ差が小さい厚鋼板およびその製造方法 | |
| JPS6156310B2 (enExample) | ||
| JPH0377848B2 (enExample) | ||
| JP3336877B2 (ja) | 脆性破壊伝播停止特性と溶接性に優れた厚肉高張力鋼板の製造方法 | |
| JP3661510B2 (ja) | 耐歪み時効特性に優れた高強度厚鋼板及びその製造方法 | |
| JPS6156309B2 (enExample) | ||
| JPH0860291A (ja) | 耐遅れ破壊性に優れた機械構造用鋼 | |
| JP5458923B2 (ja) | 耐脆性破壊特性に優れた溶接継手 | |
| JPH0825055B2 (ja) | 高Crフェライト鋼用溶接材料 | |
| JPH0254415B2 (enExample) | ||
| JP2659814B2 (ja) | 高強度低合金耐熱鋼の製造方法 | |
| JPH0254414B2 (enExample) | ||
| JPS6027731B2 (ja) | 200〜450℃の中温域において高い強度を示す蒸気輸送用鋼管の製造方法 | |
| JPS5913022A (ja) | 耐溶接継手軟化特性に優れた高靭性厚肉非調質50キロ級鋼の製造法 | |
| JP2002371336A (ja) | 高張力鋼材および鋼板 | |
| JPH07113126B2 (ja) | 耐応力腐食割れ性の優れたステンレス鋼の製造方法 |