JPH0337968B2 - - Google Patents

Info

Publication number
JPH0337968B2
JPH0337968B2 JP10074182A JP10074182A JPH0337968B2 JP H0337968 B2 JPH0337968 B2 JP H0337968B2 JP 10074182 A JP10074182 A JP 10074182A JP 10074182 A JP10074182 A JP 10074182A JP H0337968 B2 JPH0337968 B2 JP H0337968B2
Authority
JP
Japan
Prior art keywords
protein
dehydration
membrane
exchange membrane
cation exchange
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP10074182A
Other languages
English (en)
Japanese (ja)
Other versions
JPS58219903A (ja
Inventor
Tetsuo Tanaka
Tadashi Inoe
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Asahi Chemical Industry Co Ltd
Original Assignee
Asahi Chemical Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Asahi Chemical Industry Co Ltd filed Critical Asahi Chemical Industry Co Ltd
Priority to JP10074182A priority Critical patent/JPS58219903A/ja
Publication of JPS58219903A publication Critical patent/JPS58219903A/ja
Publication of JPH0337968B2 publication Critical patent/JPH0337968B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Separation Using Semi-Permeable Membranes (AREA)
JP10074182A 1982-06-14 1982-06-14 可溶性タンパク質水溶液の脱水方法 Granted JPS58219903A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP10074182A JPS58219903A (ja) 1982-06-14 1982-06-14 可溶性タンパク質水溶液の脱水方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP10074182A JPS58219903A (ja) 1982-06-14 1982-06-14 可溶性タンパク質水溶液の脱水方法

Publications (2)

Publication Number Publication Date
JPS58219903A JPS58219903A (ja) 1983-12-21
JPH0337968B2 true JPH0337968B2 (enExample) 1991-06-07

Family

ID=14281980

Family Applications (1)

Application Number Title Priority Date Filing Date
JP10074182A Granted JPS58219903A (ja) 1982-06-14 1982-06-14 可溶性タンパク質水溶液の脱水方法

Country Status (1)

Country Link
JP (1) JPS58219903A (enExample)

Also Published As

Publication number Publication date
JPS58219903A (ja) 1983-12-21

Similar Documents

Publication Publication Date Title
US9162185B2 (en) Ion-exchange membrane
US4549947A (en) Method and apparatus for dehydration of water-containing substance by electro-osmosis
CN110461916A (zh) 使用非均相离子交换膜载体的双极性离子交换膜和其制造方法
US3784457A (en) Process for removing electrolytes from aqueous solution
CN114405286A (zh) 一种离子交联型两性离子交换膜、制备方法及其在选择性电渗析中的用途
EP1031598B1 (en) Ion-selective membranes, their production process, use of the ion-selective membranes, and apparatuses provided with the ion-selective membranes
US3231485A (en) Process for purifying amino acids
JPS6145653B2 (enExample)
JP2005521771A (ja) ポリマーグラフト化支持体ポリマー
JPH0337968B2 (enExample)
US4585536A (en) Ion exchange membranes consisting of pyrrole polymers
EP0382440A1 (en) Cation exchange membranes
US2702272A (en) Electrolytically conductive membrane
DE3143804C2 (enExample)
JPH0347126B2 (enExample)
KR101681637B1 (ko) 니트릴 고무를 함유한 스티렌계-tert-부틸스티렌계 양이온교환 복합막 및 이의 제조방법
JP2743252B2 (ja) フルオロポリマー水性エマルジョンの濃縮方法
JPH0460690B2 (enExample)
JPS59145005A (ja) セルロ−ス水分散体の脱水方法
KR100460454B1 (ko) 친수성 고분자를 이용한 수팽윤성 양이온교환막 및 그의제조방법
JP2557525B2 (ja) 管状イオン交換体の製造方法
JP6195188B2 (ja) ペプチドの製造方法および該方法により得られるペプチド含有医薬組成物
JPH022863A (ja) アニオン荷電ポリオレフイン樹脂多孔膜の製造方法
JPS59145006A (ja) 高分子水溶液、分散液またはゲルの脱水濃縮方法
JPS59120210A (ja) 脱水濃縮方法