JPH0254796A - ステンレス鋼の耐食性を改善する方法 - Google Patents

ステンレス鋼の耐食性を改善する方法

Info

Publication number
JPH0254796A
JPH0254796A JP20423988A JP20423988A JPH0254796A JP H0254796 A JPH0254796 A JP H0254796A JP 20423988 A JP20423988 A JP 20423988A JP 20423988 A JP20423988 A JP 20423988A JP H0254796 A JPH0254796 A JP H0254796A
Authority
JP
Japan
Prior art keywords
potential
stainless steel
corrosion resistance
corrosion
sulfuric acid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
JP20423988A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0254796A5 (enExample
Inventor
Yoshinori Nakayama
中山 佳則
Kikuo Takizawa
瀧沢 貴久男
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sanyo Electric Co Ltd
Original Assignee
Sanyo Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sanyo Electric Co Ltd filed Critical Sanyo Electric Co Ltd
Priority to JP20423988A priority Critical patent/JPH0254796A/ja
Publication of JPH0254796A publication Critical patent/JPH0254796A/ja
Publication of JPH0254796A5 publication Critical patent/JPH0254796A5/ja
Ceased legal-status Critical Current

Links

Landscapes

  • Preventing Corrosion Or Incrustation Of Metals (AREA)
JP20423988A 1988-08-17 1988-08-17 ステンレス鋼の耐食性を改善する方法 Ceased JPH0254796A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP20423988A JPH0254796A (ja) 1988-08-17 1988-08-17 ステンレス鋼の耐食性を改善する方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP20423988A JPH0254796A (ja) 1988-08-17 1988-08-17 ステンレス鋼の耐食性を改善する方法

Publications (2)

Publication Number Publication Date
JPH0254796A true JPH0254796A (ja) 1990-02-23
JPH0254796A5 JPH0254796A5 (enExample) 1996-10-15

Family

ID=16487153

Family Applications (1)

Application Number Title Priority Date Filing Date
JP20423988A Ceased JPH0254796A (ja) 1988-08-17 1988-08-17 ステンレス鋼の耐食性を改善する方法

Country Status (1)

Country Link
JP (1) JPH0254796A (enExample)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH04146678A (ja) * 1990-10-09 1992-05-20 Nec Corp レーザ装置
KR100386319B1 (ko) * 1996-12-26 2003-09-19 주식회사 포스코 텅스텐 함유 2상스텐레스강의 틈 부식(Crevice corrosion) 저항성을 향상 시키기위한 표면 처리법
WO2019082591A1 (ja) * 2017-10-25 2019-05-02 Jfeスチール株式会社 燃料電池のセパレータ用のステンレス鋼板の製造方法
CN109972186A (zh) * 2019-03-04 2019-07-05 东莞市凯盟表面处理技术开发有限公司 一种不锈钢钝化处理方法

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5433780A (en) * 1977-03-09 1979-03-12 Pasteur Institut Device for microsampling* weiching and distributing*and microanalytical method
JPS5964783A (ja) * 1982-09-30 1984-04-12 Sumitomo Metal Ind Ltd 化成処理性にすぐれた熱延鋼板の製造方法
JPS602695A (ja) * 1983-06-17 1985-01-08 Hitachi Ltd 発電プラント
JPS61270396A (ja) * 1985-05-25 1986-11-29 Ishikawajima Harima Heavy Ind Co Ltd ステンレス鋼材の不働態化処理方法

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5433780A (en) * 1977-03-09 1979-03-12 Pasteur Institut Device for microsampling* weiching and distributing*and microanalytical method
JPS5964783A (ja) * 1982-09-30 1984-04-12 Sumitomo Metal Ind Ltd 化成処理性にすぐれた熱延鋼板の製造方法
JPS602695A (ja) * 1983-06-17 1985-01-08 Hitachi Ltd 発電プラント
JPS61270396A (ja) * 1985-05-25 1986-11-29 Ishikawajima Harima Heavy Ind Co Ltd ステンレス鋼材の不働態化処理方法

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH04146678A (ja) * 1990-10-09 1992-05-20 Nec Corp レーザ装置
KR100386319B1 (ko) * 1996-12-26 2003-09-19 주식회사 포스코 텅스텐 함유 2상스텐레스강의 틈 부식(Crevice corrosion) 저항성을 향상 시키기위한 표면 처리법
WO2019082591A1 (ja) * 2017-10-25 2019-05-02 Jfeスチール株式会社 燃料電池のセパレータ用のステンレス鋼板の製造方法
JP6521203B1 (ja) * 2017-10-25 2019-05-29 Jfeスチール株式会社 燃料電池のセパレータ用のステンレス鋼板の製造方法
US20200248332A1 (en) * 2017-10-25 2020-08-06 Jfe Steel Corporation Production method for stainless steel sheet for fuel cell separators
TWI711212B (zh) * 2017-10-25 2020-11-21 日商杰富意鋼鐵股份有限公司 燃料電池之分隔件用之不鏽鋼鋼板之製造方法
US11618967B2 (en) 2017-10-25 2023-04-04 Jfe Steel Corporation Production method for stainless steel sheet for fuel cell separators
CN109972186A (zh) * 2019-03-04 2019-07-05 东莞市凯盟表面处理技术开发有限公司 一种不锈钢钝化处理方法
CN109972186B (zh) * 2019-03-04 2020-07-28 东莞市凯盟表面处理技术开发有限公司 一种不锈钢钝化处理方法

Similar Documents

Publication Publication Date Title
US4859288A (en) Porous anodic aluminum oxide films
Stelgerwald Effect of Cr content on pitting behavior of Fe-Cr alloys
KR102209596B1 (ko) 스테인리스 스틸의 표면개질 방법
Doménech‐Carbó et al. Dating of archaeological gold by means of solid state electrochemistry
Hahn et al. Effect of electropolishing variables on the current density-voltage relationship
CN103543152A (zh) 一种转子钢焊缝残余奥氏体的检测方法
JPS60100700A (ja) ニツケル、コバルト又は鉄を基礎とする合金から成る材料の電解研磨方法
Pryor Corrosion of Steel in Dilute Solutions of Sodium Salts of Weak Acids
SU1481267A1 (ru) Способ травлени материалов
Sathish et al. Corrosion behavior of Cu-Zn-Ni shape memory alloys
Gajek et al. Long-lasting hydrogen evolution on and hydrogen entry into iron in an aqueous solution
US2347040A (en) Method of anodically polishing steel
Singh et al. Active, passive and transpassive dissolution of a nickel base super alloy in concentrated acid mixture solution
JP2010209401A (ja) 粗面化金属材料の製造方法
Pungor et al. Surface studies on precipitate-based cyanide electrodes
Usanova et al. Corrosion resistance study of grey cast iron implanted with C, N, Cr and Cu ions
JPH05247700A (ja) ステンレス焼鈍鋼帯の電解デスケーリング方法
Koehler et al. Pitting and Uniform Corrosion of Aluminum by p H 3.5 Citrate Buffer Solution
Magnani The effect of chloride ions on the cracking behavior of U/7.5 wt% Nb/2.5 wt% Zr and U/4.5 wt% Nb
Allen The photo-electric behaviour of iron in the active and passive state
SU1720818A1 (ru) Электролит дл электрохимической обработки сталей
El Din et al. Corrosion Behaviour of Manganese‐Containing Stainless Steels. II. Potentiodynamic measurements in H2SO4 solutions
Sastri et al. Analysis of surface hydrogen in high-strength steels
El Din et al. Corrosion Behaviour of Manganese‐Containing Stainless Steels. III. Their susceptibility towards pitting corrosion
Wojan Electropolishing of 18–8 Stainless Steel