JPH0228527B2 - - Google Patents
Info
- Publication number
- JPH0228527B2 JPH0228527B2 JP19045082A JP19045082A JPH0228527B2 JP H0228527 B2 JPH0228527 B2 JP H0228527B2 JP 19045082 A JP19045082 A JP 19045082A JP 19045082 A JP19045082 A JP 19045082A JP H0228527 B2 JPH0228527 B2 JP H0228527B2
- Authority
- JP
- Japan
- Prior art keywords
- blast furnace
- furnace slag
- grinding
- added
- salts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02W—CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
- Y02W30/00—Technologies for solid waste management
- Y02W30/50—Reuse, recycling or recovery technologies
Landscapes
- Disintegrating Or Milling (AREA)
- Curing Cements, Concrete, And Artificial Stone (AREA)
- Manufacture Of Iron (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57190450A JPS5978961A (ja) | 1982-10-28 | 1982-10-28 | 高炉スラグ粉砕助剤 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57190450A JPS5978961A (ja) | 1982-10-28 | 1982-10-28 | 高炉スラグ粉砕助剤 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5978961A JPS5978961A (ja) | 1984-05-08 |
| JPH0228527B2 true JPH0228527B2 (enrdf_load_stackoverflow) | 1990-06-25 |
Family
ID=16258329
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP57190450A Granted JPS5978961A (ja) | 1982-10-28 | 1982-10-28 | 高炉スラグ粉砕助剤 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5978961A (enrdf_load_stackoverflow) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4770147B2 (ja) * | 2004-09-17 | 2011-09-14 | 栗田工業株式会社 | 石炭の乾式粉砕助剤及び乾式粉砕方法 |
| JP5055219B2 (ja) | 2007-08-10 | 2012-10-24 | 花王株式会社 | 水硬性粉体の製造方法 |
| JP5122390B2 (ja) * | 2007-08-10 | 2013-01-16 | 花王株式会社 | 水硬性粉体の製造方法 |
-
1982
- 1982-10-28 JP JP57190450A patent/JPS5978961A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5978961A (ja) | 1984-05-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN111646727B (zh) | 一种复合水泥外加剂 | |
| CN114988741A (zh) | 一种锂盐基复合矿物掺合料及其制备方法 | |
| CN102531419B (zh) | 钢渣的活化方法 | |
| US3983040A (en) | Fire-retardant composition and process of producing same | |
| CN101784500A (zh) | 水硬性粉体的制造方法 | |
| CN102145906B (zh) | 一种以粉煤灰为原料制备低铁结晶氯化铝的方法 | |
| CN102965077B (zh) | 一种粉体矿粉添加剂 | |
| JPH0228527B2 (enrdf_load_stackoverflow) | ||
| CN103352099B (zh) | 利用拜耳法赤泥生产转炉冷却剂的方法 | |
| CN114920489A (zh) | 一种水泥生料添加剂及其应用和水泥生产工艺 | |
| CN113831051A (zh) | 一种矿粉助磨剂及其制备方法和应用 | |
| Li et al. | Improving the volume stability of steel slag for construction and building materials | |
| CN113953076B (zh) | 一种提高aod炉镍合金精炼渣粉磨效率和活性的方法 | |
| CN114804693B (zh) | 一种固废复配型粉煤灰激发剂及其应用 | |
| CN104823748A (zh) | 一种利用拜耳法赤泥制备人造土壤组合物的方法及其得到的人造土壤组合物 | |
| JPS5545717A (en) | Pulverized sodium polyacrylate and its preparation | |
| JPH0228526B2 (enrdf_load_stackoverflow) | ||
| CN109111140B (zh) | 一种应用柠檬酸渣制备高活性矿渣微粉的方法 | |
| CN113372028A (zh) | 一种高活性矿渣微粉复合掺料及其制备方法 | |
| CN106673666A (zh) | 一种高硬度特种陶瓷的制备方法 | |
| CN109954588B (zh) | 一种倍半氧化物抑制剂及其制备方法与用途 | |
| KR102012273B1 (ko) | 슬래그 성능개선 조성물 | |
| CN105883879A (zh) | 纳米包覆复合碳酸钙的制备方法 | |
| KR101545475B1 (ko) | 시멘트 클링커 분쇄 활성화 화합물을 포함하는 시멘트 클링커 분쇄조제용 조성물 | |
| KR101558932B1 (ko) | 고비중 및 저팽창성 제강슬래그 골재의 제조방법 |