JP5274269B2 - スルホン酸基とアミド基を有する重合体の製造方法 - Google Patents
スルホン酸基とアミド基を有する重合体の製造方法 Download PDFInfo
- Publication number
- JP5274269B2 JP5274269B2 JP2009003161A JP2009003161A JP5274269B2 JP 5274269 B2 JP5274269 B2 JP 5274269B2 JP 2009003161 A JP2009003161 A JP 2009003161A JP 2009003161 A JP2009003161 A JP 2009003161A JP 5274269 B2 JP5274269 B2 JP 5274269B2
- Authority
- JP
- Japan
- Prior art keywords
- polymer
- sulfonic acid
- chemical formula
- group
- vinyl
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2009003161A JP5274269B2 (ja) | 2009-01-09 | 2009-01-09 | スルホン酸基とアミド基を有する重合体の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2009003161A JP5274269B2 (ja) | 2009-01-09 | 2009-01-09 | スルホン酸基とアミド基を有する重合体の製造方法 |
Publications (3)
Publication Number | Publication Date |
---|---|
JP2010159358A JP2010159358A (ja) | 2010-07-22 |
JP2010159358A5 JP2010159358A5 (enrdf_load_stackoverflow) | 2012-02-23 |
JP5274269B2 true JP5274269B2 (ja) | 2013-08-28 |
Family
ID=42576764
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2009003161A Expired - Fee Related JP5274269B2 (ja) | 2009-01-09 | 2009-01-09 | スルホン酸基とアミド基を有する重合体の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JP5274269B2 (enrdf_load_stackoverflow) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN114107655B (zh) * | 2021-11-10 | 2023-05-30 | 湖南博一环保科技有限公司 | 一种双向逆流循环水洗工艺 |
Family Cites Families (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01172409A (ja) * | 1987-12-28 | 1989-07-07 | Exxon Res & Eng Co | 多機能性6向上剤用の重合体アミド |
WO2001098376A1 (fr) * | 2000-06-22 | 2001-12-27 | Idemitsu Petrochemical Co., Ltd. | Polymere reticule a base d'acide carboxylique insature, son procede de production et matiere absorbant l'eau |
JP4996060B2 (ja) * | 2004-05-12 | 2012-08-08 | キヤノン株式会社 | スルホン酸エステル基と、アミド基を有するポリマーを含む荷電制御剤、それを用いた静電荷像現像用トナー、画像形成方法および画像形成装置 |
JP4741883B2 (ja) * | 2004-06-11 | 2011-08-10 | キヤノン株式会社 | エステル基、カルボキシル基並びにスルホン酸基を有するポリヒドロキシアルカノエート並びにその製造方法 |
JP4553374B2 (ja) * | 2004-06-11 | 2010-09-29 | キヤノン株式会社 | スルホン酸基を有するポリヒドロキシアルカノエート並びにその製造方法 |
JP5328097B2 (ja) * | 2005-11-11 | 2013-10-30 | キヤノン株式会社 | スルホン酸基又はスルホン酸エステル基と、アミド基とを有するポリマー、及び該ポリマーを有する静電荷像現像トナー |
-
2009
- 2009-01-09 JP JP2009003161A patent/JP5274269B2/ja not_active Expired - Fee Related
Also Published As
Publication number | Publication date |
---|---|
JP2010159358A (ja) | 2010-07-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR100989499B1 (ko) | 술폰산기 또는 술폰산 에스테르기와 아미드기를 갖는중합체 및 이 중합체를 갖는 정전하 잠상 현상용 토너 | |
JP6643111B2 (ja) | トナー | |
KR102061400B1 (ko) | 호모아다만탄 유도체, 그 제조 방법 및 포토레지스트용 감광성 재료 | |
CA2855779C (en) | Polyester/polycarbonate block copolymers via one-pot, neat ring opening polymerization | |
KR100883487B1 (ko) | 설폰산기 혹은 설포네이트기와 아마이드기를 지닌 폴리머및 그 제조방법 | |
JP2021096463A (ja) | トナー及び二成分系現像剤 | |
Zhang et al. | One‐pot synthesis of ABC miktoarm star terpolymers by coupling ATRP, ROP, and click chemistry techniques | |
JP5198473B2 (ja) | フルオレン系樹脂重合体およびこれの製造方法 | |
CN111123670B (zh) | 调色剂 | |
TW201945333A (zh) | 新穎之二官能(甲基)丙烯酸酯化合物及聚合物 | |
CA2704377C (en) | Processes for the synthesis of polyester resins | |
JP5274269B2 (ja) | スルホン酸基とアミド基を有する重合体の製造方法 | |
TW200413326A (en) | Hexaarylbiimidazole compounds and photopolymerization initiator compositions containing the same | |
JP6478678B2 (ja) | トナー、及びトナーの製造方法 | |
JP6186705B2 (ja) | ポリエステル樹脂およびその製造方法 | |
JP6320006B2 (ja) | ブロック共重合体の製造方法およびトナーの製造方法 | |
JP5300271B2 (ja) | スルホン酸エステル基とアミド基を有する重合体の製造方法 | |
JP7337535B2 (ja) | アミド結合を有し、かつアルコキシシリル基を有する化合物の製造方法 | |
JP2007156457A (ja) | 荷電制御剤、及び静電荷現像用トナー | |
KR100196456B1 (ko) | 부분 tert-부톡시화 폴리(p-히드록시스티렌)의 제조방법 | |
JP5328097B2 (ja) | スルホン酸基又はスルホン酸エステル基と、アミド基とを有するポリマー、及び該ポリマーを有する静電荷像現像トナー | |
JP2018072621A (ja) | トナー粒子の製造方法 | |
JP5252885B2 (ja) | 樹脂の製造方法 | |
JP2008063309A (ja) | 重合性化合物の製造方法 | |
KR100841190B1 (ko) | 설폰산기 혹은 설포네이트기와 아마이드기를 지닌 폴리머및 그 제조방법 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20120110 |
|
A621 | Written request for application examination |
Free format text: JAPANESE INTERMEDIATE CODE: A621 Effective date: 20120110 |
|
A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20130222 |
|
A131 | Notification of reasons for refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A131 Effective date: 20130226 |
|
A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20130325 |
|
TRDD | Decision of grant or rejection written | ||
A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 Effective date: 20130416 |
|
A61 | First payment of annual fees (during grant procedure) |
Free format text: JAPANESE INTERMEDIATE CODE: A61 Effective date: 20130514 |
|
R151 | Written notification of patent or utility model registration |
Ref document number: 5274269 Country of ref document: JP Free format text: JAPANESE INTERMEDIATE CODE: R151 |
|
LAPS | Cancellation because of no payment of annual fees |