JP3688517B2 - アルカリ蓄電池 - Google Patents

アルカリ蓄電池 Download PDF

Info

Publication number
JP3688517B2
JP3688517B2 JP16815599A JP16815599A JP3688517B2 JP 3688517 B2 JP3688517 B2 JP 3688517B2 JP 16815599 A JP16815599 A JP 16815599A JP 16815599 A JP16815599 A JP 16815599A JP 3688517 B2 JP3688517 B2 JP 3688517B2
Authority
JP
Japan
Prior art keywords
battery case
storage battery
lid
alkaline storage
safety valve
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP16815599A
Other languages
English (en)
Other versions
JP2000357499A (ja
Inventor
伊藤  隆
知徳 岸本
雄三 樋野
政彦 押谷
登 佐藤
一彦 八木
誉士 石倉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Honda Motor Co Ltd
Yuasa Corp
Original Assignee
Honda Motor Co Ltd
Yuasa Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Honda Motor Co Ltd, Yuasa Corp filed Critical Honda Motor Co Ltd
Priority to JP16815599A priority Critical patent/JP3688517B2/ja
Publication of JP2000357499A publication Critical patent/JP2000357499A/ja
Application granted granted Critical
Publication of JP3688517B2 publication Critical patent/JP3688517B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【0001】
【発明の属する技術分野】
本発明は、電槽及び蓋からなる容器を改良してなる密閉形アルカリ蓄電池に関するものである。
【0002】
【従来の技術】
水素吸蔵合金を主材とする負極を用いた密閉形アルカリ蓄電池は、優れた充放電特性や取り扱いの簡便さから、近年、その用途が拡大してきており、特に電気自動車用電池としての需要が見込まれている。しかし、電気自動車用電池としてのアルカリ蓄電池は、高出力密度と高エネルギー密度とを兼ね備えるだけでなく、車両に搭載するためにコンパクト且つ軽量でなければならない。そこで、蓄電池材料を収納する容器を構成する電槽などには樹脂が用いられており、ポリプロピレン(PP)樹脂が、ヒートシール性や耐薬品性に優れていることから、電槽などに一般に用いられていた。
【0003】
【発明が解決しようとする課題】
しかしながら、PP樹脂は剛性及び耐熱性に劣るので、充放電中に生じた熱や圧力によって電槽などに変形や割れが発生するという問題があった。
【0004】
本発明は、電槽などに変形や割れが発生するのを防止でき、また、蓄電池材料中の水分の減少を防止して長寿命化を図ることができる、アルカリ蓄電池を提供することを目的とする。
【0005】
【課題を解決するための手段】
請求項1記載の発明は、電槽とこれを塞ぐ蓋とからなる密閉容器内に蓄電池材料が収納されており、電槽と蓋とは溶着接合されており、蓋は、蓋本体に、少なくとも安全弁が溶着接合されて構成されている、アルカリ蓄電池において、電槽及び蓋本体が、変性ポリフェニレンオキサイド樹脂とポリフェニレンサルファイド樹脂とを含有した複合材でできており、安全弁が、変性ポリフェニレンオキサイド樹脂のみで、又は変性ポリフェニレンオキサイド樹脂とポリフェニレンサルファイド樹脂とを含有した複合材で、できており、電槽及び蓋本体の複合材のポリフェニレンサルファイド樹脂の含有割合が70重量部以上95重量部以下であり、安全弁の複合材のポリフェニレンサルファイド樹脂の含有割合が30重量部以下であることを特徴としている。
【0006】
【発明の実施の形態】
図1は本発明のアルカリ蓄電池、具体的には50Ahの電気自動車用ニッケル水素蓄電池の単電池を示す外観斜視図である。この蓄電池は、電槽1とこれを塞ぐ蓋2とからなる密閉容器3内に、正極、負極、セパレータ、及び電解液からなる蓄電池材料を収納して、構成されている。電槽1と蓋2とは部分41にて溶着接合されている。蓋2は、蓋本体21に、安全弁22が溶着接合されるとともに正極端子23及び負極端子24が取付けられて、構成されている。蓋本体21と安全弁22とは部分42にて溶着されている。
【0007】
図1に示すアルカリ蓄電池において、電槽1、蓋本体21、及び安全弁22の構成材料をそれぞれ表1及び表2のように設定して、実施形態1〜及び比較形態1〜のアルカリ蓄電池を作製した。
【0008】
【表1】
Figure 0003688517
【0009】
【表2】
Figure 0003688517
【0010】
実施形態1〜及び比較形態1〜のアルカリ蓄電池について、次の試験を行った。なお、透水性試験及び耐熱性試験については、電槽と同じ材料からなる試験片を作製し、これを用いて行った。試験片は、電槽と同じ材料のペレットを射出成形して角板を作製した後、1mmの厚さにプレスしてシート状とし、直径60mmの円盤状に打抜いて、作製した。試験の結果は表及び表に示した。
【0011】
[透水性試験]
50mlの水を入れた100mlの容器の開口を試験片で塞いでシールし、この容器を50℃の恒温槽内に560時間放置した後、容器内の水分重量の減少量を求めた。
【0012】
[耐熱性試験]
試験片を100℃の雰囲気下に置き、その曲げ弾性率を測定した。
【0013】
[圧壊試験]
蓄電池材料を収容していない密閉容器3に内部から外向きの圧力を加えていき、部分41又は部分42が破損した時の圧力を測定した。
【0014】
【表3】
Figure 0003688517
【0015】
【表4】
Figure 0003688517
【0016】
実施形態1〜の試験結果と比較形態1〜5の試験結果とを比較してみると、実施形態の方が、水分重量減少量が小さいので透水性が低く、曲げ弾性率及び圧壊強度が大きいので耐熱性及び剛性に優れている。なお、透水性試験及び耐熱性試験の結果は、電槽1及び蓋本体21について示すものであり、安全弁22について示すものではないが、安全弁22は密閉容器3において僅かな表面積しか占めないので、密閉容器3の透水性及び耐熱性には殆ど影響しない。従って、実施形態1〜のアルカリ蓄電池は、充放電中に生じた熱や圧力によって密閉容器3に変形や割れが発生するのを防止でき、また、密閉容器3内の蓄電池材料中の水分の減少を抑制して長寿命化を図ることができる。なお、全てにPP樹脂を用いた比較形態6の蓄電池は、透水性が非常に小さいが、耐熱性が極端に悪い。
【0017】
【発明の効果】
請求項1記載の発明によれば、密閉容器の耐熱性及び剛性を向上でき、したがって、充放電中に生じた熱や圧力によって密閉容器に変形や割れが発生するのを防止できる。また、密閉容器の透水性を低くでき、したがって、密閉容器内の蓄電池材料中の水分の減少を抑制して長寿命化を図ることができる。
【図面の簡単な説明】
【図1】 本発明のアルカリ蓄電池の単電池を示す外観斜視図である。
【符号の説明】
1 電槽
2 蓋
21 蓋本体
22 安全弁
3 密閉容器
41,42 (溶着)部分

Claims (1)

  1. 電槽とこれを塞ぐ蓋とからなる密閉容器内に蓄電池材料が収納されており、電槽と蓋とは溶着接合されており、蓋は、蓋本体に、少なくとも安全弁が溶着接合されて構成されている、アルカリ蓄電池において、
    電槽及び蓋本体が、変性ポリフェニレンオキサイド樹脂とポリフェニレンサルファイド樹脂とを含有した複合材でできており、
    安全弁が、変性ポリフェニレンオキサイド樹脂のみで、又は変性ポリフェニレンオキサイド樹脂とポリフェニレンサルファイド樹脂とを含有した複合材で、できており、
    電槽及び蓋本体の複合材のポリフェニレンサルファイド樹脂の含有割合が70重量部以上95重量部以下であり、
    安全弁の複合材のポリフェニレンサルファイド樹脂の含有割合が30重量部以下であることを特徴とするアルカリ蓄電池。
JP16815599A 1999-06-15 1999-06-15 アルカリ蓄電池 Expired - Lifetime JP3688517B2 (ja)