JP3182780B2 - セラミック緻密層の形成方法 - Google Patents

セラミック緻密層の形成方法

Info

Publication number
JP3182780B2
JP3182780B2 JP07854891A JP7854891A JP3182780B2 JP 3182780 B2 JP3182780 B2 JP 3182780B2 JP 07854891 A JP07854891 A JP 07854891A JP 7854891 A JP7854891 A JP 7854891A JP 3182780 B2 JP3182780 B2 JP 3182780B2
Authority
JP
Japan
Prior art keywords
ceramic
porous substrate
layer
dense
forming
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP07854891A
Other languages
English (en)
Japanese (ja)
Other versions
JPH04292490A5 (enExample
JPH04292490A (ja
Inventor
正信 相沢
千尋 小林
正宏 黒石
治男 西山
Original Assignee
東陶機器株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 東陶機器株式会社 filed Critical 東陶機器株式会社
Priority to JP07854891A priority Critical patent/JP3182780B2/ja
Publication of JPH04292490A publication Critical patent/JPH04292490A/ja
Publication of JPH04292490A5 publication Critical patent/JPH04292490A5/ja
Application granted granted Critical
Publication of JP3182780B2 publication Critical patent/JP3182780B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Landscapes

  • Fuel Cell (AREA)
  • Separation Using Semi-Permeable Membranes (AREA)
JP07854891A 1991-03-18 1991-03-18 セラミック緻密層の形成方法 Expired - Lifetime JP3182780B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP07854891A JP3182780B2 (ja) 1991-03-18 1991-03-18 セラミック緻密層の形成方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP07854891A JP3182780B2 (ja) 1991-03-18 1991-03-18 セラミック緻密層の形成方法

Publications (3)

Publication Number Publication Date
JPH04292490A JPH04292490A (ja) 1992-10-16
JPH04292490A5 JPH04292490A5 (enExample) 1999-04-27
JP3182780B2 true JP3182780B2 (ja) 2001-07-03

Family

ID=13664974

Family Applications (1)

Application Number Title Priority Date Filing Date
JP07854891A Expired - Lifetime JP3182780B2 (ja) 1991-03-18 1991-03-18 セラミック緻密層の形成方法

Country Status (1)

Country Link
JP (1) JP3182780B2 (enExample)

Also Published As

Publication number Publication date
JPH04292490A (ja) 1992-10-16

Similar Documents

Publication Publication Date Title
CN103987681B (zh) 复合氧气传送膜
US5085742A (en) Solid oxide electrochemical cell fabrication process
US4861345A (en) Method of bonding a conductive layer on an electrode of an electrochemical cell
CA2204632A1 (en) Protective interlayer for high temperature solid electrolyte electrochemical cells
WO2000039864A2 (en) Fuel electrode formation for a solid oxide fuel cell
US5277995A (en) Electrode and method of interconnection sintering on an electrode of an electrochemical cell
JPH07320754A (ja) 固体電解質膜と電極膜との接続構造及びその製造方法
JPH1079259A (ja) 円筒型固体電解質燃料電池のセルおよびその製造方法
JPH04248272A (ja) 縦縞円筒型固体電解質燃料電池のインターコネクタの製造方法
JPH07254418A (ja) 固体電解質燃料電池及びその製造方法
JPH04292490A (ja) セラミック緻密層の形成方法
US6395206B1 (en) Method of removing an organic binder from a green ceramic form
JP2003288919A (ja) 電気伝導性セラミックスおよびその製造方法、ならびにそれを用いた固体酸化物形燃料電池用インターコネクタ
JP3050328B2 (ja) 固体電解質燃料電池の製造方法
JPH07320757A (ja) 固体電解質燃料電池インターコネクター及びその製造方 法
JP2006222068A (ja) セラミックヒータ及びその製造方法
US20190022596A1 (en) Catalyst-containing oxygen transport membrane
JP3050331B2 (ja) 固体電解質燃料電池の製造方法
JPH0721830A (ja) 固体電解質膜の製法
JPH08133739A (ja) ジルコニア膜の製造方法
JPH04355058A (ja) 固体電解質燃料電池及びその製造方法
JPS63121647A (ja) イツトリア安定化ジルコニア皮膜コ−テイング方法
JPH0574465A (ja) 固体電解質型燃料電池の製造方法
JPH03179670A (ja) 燃料電池用固体電解質の製造方法
JPH04204046A (ja) ガラスセラミックスからなる多孔質焼結体の製造方法および酸素濃度検出器

Legal Events

Date Code Title Description
A01 Written decision to grant a patent or to grant a registration (utility model)

Free format text: JAPANESE INTERMEDIATE CODE: A01

Effective date: 20010327

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20090427

Year of fee payment: 8

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20100427

Year of fee payment: 9

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20100427

Year of fee payment: 9

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20110427

Year of fee payment: 10

EXPY Cancellation because of completion of term