JP2893081B2 - オゾンガス貯蔵容器 - Google Patents

オゾンガス貯蔵容器

Info

Publication number
JP2893081B2
JP2893081B2 JP22433794A JP22433794A JP2893081B2 JP 2893081 B2 JP2893081 B2 JP 2893081B2 JP 22433794 A JP22433794 A JP 22433794A JP 22433794 A JP22433794 A JP 22433794A JP 2893081 B2 JP2893081 B2 JP 2893081B2
Authority
JP
Japan
Prior art keywords
ozone gas
storage container
passivation film
oxygen
container
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP22433794A
Other languages
English (en)
Other versions
JPH0885548A (ja
Inventor
国彦 小池
吾一 井上
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Iwatani Sangyo KK
Original Assignee
Iwatani Sangyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Iwatani Sangyo KK filed Critical Iwatani Sangyo KK
Priority to JP22433794A priority Critical patent/JP2893081B2/ja
Publication of JPH0885548A publication Critical patent/JPH0885548A/ja
Application granted granted Critical
Publication of JP2893081B2 publication Critical patent/JP2893081B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】
【0001】
【産業上の利用分野】本発明は、オゾンガスの貯蔵容器
に関する。
【0002】
【従来技術】オゾンガスはステンレス鋼容器やガラス容
器に充填されるが、酸素への自己分解性が強く、従来は
オゾンガスを長期間保存することはできないとされてい
た。本発明は、オゾンガスを長期間保存できる貯蔵容器
を提供することを目的とする。
【0003】
【課題を解決するための手段】上述の目的を達成するた
めに、電解研磨して鏡面仕上げしたステンレス鋼製貯蔵
容器の内面を不動態膜で覆ったことを特徴としている。
【0004】
【作用】本発明では、電解研磨して鏡面仕上げしたステ
ンレス鋼製貯蔵容器の内面を不動態膜で覆っているの
で、貯蔵容器の内周面の活性が抑制され、自己分解性が
抑制される。これにより、オゾンを貯蔵することができ
る。
【0005】
【実施例】内面に電解研磨を施し、加工変質層のない状
態に鏡面仕上げしたSUS316Lステンレス鋼製の気
密容器を真空引きしたのち、気密容器内に対酸素比がほ
ぼ100%の高濃度オゾンガスをゲージ圧0.63kg/c
m2程度の圧力で充填し、48時間程度放置して、気密容
器の内面に不動態膜を形成した。なお、この不動態膜の
形成処理は常温(室温)の状態で行う。
【0006】このようにして内面に不動態膜を形成した
気密容器と、内面に不動態膜を形成していない気密容器
とを使用して、対酸素比5%のオゾンガスを751.5T
orrで貯蔵した場合の時間経過によるオゾン比率の変化
を調べた。その結果は図1に示す通りであり、内面に不
動態膜を形成していない気密容器の場合、7時間半程度
ですべて酸素に分解されるのに対し、内面に不動態膜を
形成した容器では、10時間経過してもほとんど対酸素
比に変化がなく、自己分解は起こっていないことが分か
った。
【0007】次に内面に不動態膜を形成した気密容器
と、内面に不動態膜を形成していない気密容器とを使用
して、対酸素比50%のオゾンガスを0.63Kg/cm
2(ゲージ圧)で貯蔵した場合の時間経過によるオゾン比
率の変化を調べた。その結果は図2に示す通りであり、
内面に不動態膜を形成していない気密容器の場合、80
時間程度ですべて酸素に分解されるのに対し、内面に不
動態膜を形成した容器では、90時間を経過しても対酸
素比は5%程度の低下しか見られず、自己分解が抑制さ
れていることが分かった。
【0008】なお、容器内面に不動態膜を形成する際に
導入するオゾンガスの対酸素比が50%を切ると、常温
操作では不動態膜の生成が十分ではなく、自己分解の抑
制を行うことができなかった。したがって、不動態膜生
成時に導入するオゾンガスは対酸素比50%以上でよい
が、75%以上の高濃度オゾンガスが望ましい。
【0009】上記実施例では、対酸素比50%以上の高
濃度オゾンガスを用いて不動態膜を形成したものについ
て説明したが、不動態膜は母材を400℃〜500℃に
加熱した状態で酸素ガスと接触させる処理や、母材を硝
酸溶液等の酸化力のある溶液に浸漬させる処理で形成し
たものであってもよい。
【0010】
【発明の効果】本発明では、電解研磨して鏡面仕上げし
たステンレス鋼製貯蔵容器の内面を不動態膜で覆ったの
で、容器内面での活性が抑制され、貯蔵したオゾンガス
の自己分解を抑制して、長期間にわたってオゾンガスを
貯蔵することができる。
【図面の簡単な説明】
【図1】対酸素比5%のオゾンガスの時間経過によるオ
ゾン比率変化を示すグラフである。
【図2】対酸素比50%のオゾンガスの時間経過による
オゾン比率変化を示すグラフである。

Claims (2)

    (57)【特許請求の範囲】
  1. 【請求項1】 電解研磨して鏡面仕上げしたステンレス
    鋼製貯蔵容器の内面を不動態膜で覆ってなるオゾンガス
    貯蔵容器。
  2. 【請求項2】 対酸素比50%以上の高濃度オゾンガス
    を使用して不動態膜を形成した請求項1に記載のオゾン
    ガス貯蔵容器。
JP22433794A 1994-09-20 1994-09-20 オゾンガス貯蔵容器 Expired - Lifetime JP2893081B2 (ja)