Prior art keywords
atmosphere
reaction
oxidizing atmosphere
particle growth
aqueous solution
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2017250276A
Other languages
English (en)
Japanese (ja)
Other versions
JP2018104275A (ja
JP7087380B2 (ja
Filing date
Publication date
Application filed filed Critical
Publication of JP2018104275A publication Critical patent/JP2018104275A/ja
Publication of JP2018104275A5 publication Critical patent/JP2018104275A5/ja
Application granted granted Critical
Publication of JP7087380B2 publication Critical patent/JP7087380B2/ja
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2017250276A 2016-12-27 2017-12-26 遷移金属含有複合水酸化物粒子およびその製造方法、並びに、非水電解質二次電池用正極活物質およびその製造方法 Active JP7087380B2 (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2016252218 2016-12-27
JP2016252218 2016-12-27

Publications (3)

Publication Number Publication Date
JP2018104275A JP2018104275A (ja) 2018-07-05
JP2018104275A5 true JP2018104275A5 (cg-RX-API-DMAC7.html) 2020-10-15
JP7087380B2 JP7087380B2 (ja) 2022-06-21

Family

ID=62786559

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2017250276A Active JP7087380B2 (ja) 2016-12-27 2017-12-26 遷移金属含有複合水酸化物粒子およびその製造方法、並びに、非水電解質二次電池用正極活物質およびその製造方法

Country Status (1)

Country Link
JP (1) JP7087380B2 (cg-RX-API-DMAC7.html)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP7183813B2 (ja) * 2019-01-24 2022-12-06 住友金属鉱山株式会社 ニッケルマンガンコバルト含有複合水酸化物およびその製造方法、リチウムイオン二次電池用正極活物質およびその製造方法、並びに、リチウムイオン二次電池
JP7183812B2 (ja) * 2019-01-24 2022-12-06 住友金属鉱山株式会社 ニッケルマンガンコバルト含有複合水酸化物およびその製造方法、リチウムイオン二次電池用正極活物質およびその製造方法、並びに、リチウムイオン二次電池
JP7183814B2 (ja) * 2019-01-24 2022-12-06 住友金属鉱山株式会社 ニッケルマンガンコバルト含有複合水酸化物およびその製造方法、リチウムイオン二次電池用正極活物質およびその製造方法、並びに、リチウムイオン二次電池
JP7183815B2 (ja) * 2019-01-24 2022-12-06 住友金属鉱山株式会社 ニッケルマンガンコバルト含有複合水酸化物およびその製造方法、リチウムイオン二次電池用正極活物質およびその製造方法、並びに、リチウムイオン二次電池
JP7447401B2 (ja) * 2019-07-05 2024-03-12 住友金属鉱山株式会社 ニッケルマンガンコバルト含有複合水酸化物およびその製造方法、リチウムイオン二次電池用正極活物質およびその製造方法、並びに、リチウムイオン二次電池
JP7144371B2 (ja) 2019-07-18 2022-09-29 トヨタ自動車株式会社 非水電解質二次電池
US12381218B2 (en) 2019-09-19 2025-08-05 Sumitomo Metal Mining Co., Ltd. Positive electrode active material for lithium ion secondary battery and lithium ion secondary battery

Family Cites Families (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP6128303B2 (ja) * 2012-04-03 2017-05-17 国立研究開発法人産業技術総合研究所 リチウムマンガン系複合酸化物およびその製造方法
US10374232B2 (en) * 2013-03-15 2019-08-06 Nano One Materials Corp. Complexometric precursor formulation methodology for industrial production of fine and ultrafine powders and nanopowders for lithium metal oxides for battery applications
EP3007254B1 (en) * 2013-05-10 2023-04-19 Sumitomo Metal Mining Co., Ltd. Transition metal composite hydroxide particles, method for producing same, positive electrode active material for non-aqueous electrolyte secondary battery, method for producing same, and non-aqueous electrolyte secondary battery
JP6331983B2 (ja) * 2014-11-12 2018-05-30 住友金属鉱山株式会社 遷移金属複合水酸化物粒子の製造方法および非水電解質二次電池用正極活物質の製造方法
JP6596978B2 (ja) * 2015-06-26 2019-10-30 住友金属鉱山株式会社 遷移金属複合水酸化物粒子とその製造方法、非水電解質二次電池用正極活物質とその製造方法、および非水電解質二次電池

Similar Documents

Publication Publication Date Title
JP2018104275A5 (cg-RX-API-DMAC7.html)
Xu et al. Graphite-based lithium ion battery with ultrafast charging and discharging and excellent low temperature performance
JP2018104273A5 (cg-RX-API-DMAC7.html)
US10883955B2 (en) Carbon material supported hollow metal oxide nanoparticles, methods and applications
JP2018104276A5 (cg-RX-API-DMAC7.html)
JP2018104274A5 (cg-RX-API-DMAC7.html)
CN105144439B (zh) 非水电解质二次电池用正极活性物质及其制造方法
JP2024026097A (ja) 遷移金属含有複合水酸化物とその製造方法、非水電解質二次電池用正極活物質とその製造方法、および非水電解質二次電池
JP6949297B2 (ja) 遷移金属含有複合水酸化物とその製造方法、および、非水電解質二次電池用正極活物質とその製造方法
CN107534144B (zh) 非水系电解质二次电池用正极活性物质及其制造方法以及使用了该正极活性物质的非水系电解质二次电池
JP6347227B2 (ja) マンガンニッケルチタン複合水酸化物粒子とその製造方法、および、非水系電解質二次電池用正極活物質の製造方法
Yang et al. Enhanced high rate and low-temperature performances of mesoporous LiFePO4/Ketjen Black nanocomposite cathode material
JP7260249B2 (ja) 遷移金属含有複合水酸化物粒子とその製造方法、非水電解質二次電池用正極活物質とその製造方法、および非水電解質二次電池
JP6346448B2 (ja) 非水系電解質二次電池用正極活物質、および、非水系電解質二次電池
JP7087381B2 (ja) 遷移金属含有複合水酸化物粒子およびその製造方法、並びに、非水電解質二次電池用正極活物質およびその製造方法
JP7087380B2 (ja) 遷移金属含有複合水酸化物粒子およびその製造方法、並びに、非水電解質二次電池用正極活物質およびその製造方法
KR20140047044A (ko) 비수계 이차 전지용 정극 활물질 및 그의 제조 방법, 및 그 정극 활물질을 이용한 비수계 전해질 이차 전지
JP4829557B2 (ja) リチウム鉄複合酸化物の製造方法
JP2011048992A (ja) 炭素材料、電極材料及びリチウムイオン二次電池負極材料
JP7006255B2 (ja) 遷移金属含有複合水酸化物粒子およびその製造方法、並びに、非水電解質二次電池用正極活物質およびその製造方法
JP7035540B2 (ja) 遷移金属含有複合水酸化物粒子とその製造方法、非水電解質二次電池用正極活物質とその製造方法、および非水電解質二次電池
KR20150058213A (ko) 높은 분산성의 그래핀 조성물, 그의 제조 방법, 및 높은 분산성의 그래핀 조성물을 함유하는 리튬 이온 이차 배터리의 전극
JP7087379B2 (ja) 遷移金属含有複合水酸化物粒子およびその製造方法、並びに、非水電解質二次電池用正極活物質およびその製造方法
CN113224278A (zh) 改性磷酸铁锰锂材料、其制备方法及应用
TWI782192B (zh) 鋰離子二次電池用正極活性物質、鋰離子二次電池用正極材料和鋰離子二次電池