JP2016529199A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2016529199A5 JP2016529199A5 JP2016538987A JP2016538987A JP2016529199A5 JP 2016529199 A5 JP2016529199 A5 JP 2016529199A5 JP 2016538987 A JP2016538987 A JP 2016538987A JP 2016538987 A JP2016538987 A JP 2016538987A JP 2016529199 A5 JP2016529199 A5 JP 2016529199A5
- Authority
- JP
- Japan
- Prior art keywords
- glass
- mol
- ion
- exchanged
- sio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US201361870301P | 2013-08-27 | 2013-08-27 | |
| US61/870,301 | 2013-08-27 | ||
| PCT/US2014/052262 WO2015031188A1 (en) | 2013-08-27 | 2014-08-22 | Damage resistant glass with high coefficient of thermal expansion |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2016529199A JP2016529199A (ja) | 2016-09-23 |
| JP2016529199A5 true JP2016529199A5 (enExample) | 2017-09-28 |
| JP6600309B2 JP6600309B2 (ja) | 2019-10-30 |
Family
ID=51493068
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2016538987A Expired - Fee Related JP6600309B2 (ja) | 2013-08-27 | 2014-08-22 | 高い熱膨張係数を有する耐損傷性ガラス |
Country Status (7)
| Country | Link |
|---|---|
| US (2) | US9969644B2 (enExample) |
| EP (1) | EP3038983B1 (enExample) |
| JP (1) | JP6600309B2 (enExample) |
| KR (1) | KR102290967B1 (enExample) |
| CN (2) | CN105683108A (enExample) |
| TW (2) | TWI660930B (enExample) |
| WO (1) | WO2015031188A1 (enExample) |
Families Citing this family (40)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US9359251B2 (en) | 2012-02-29 | 2016-06-07 | Corning Incorporated | Ion exchanged glasses via non-error function compressive stress profiles |
| US11079309B2 (en) | 2013-07-26 | 2021-08-03 | Corning Incorporated | Strengthened glass articles having improved survivability |
| EP3038983B1 (en) * | 2013-08-27 | 2021-10-20 | Corning Incorporated | Damage resistant glass with high coefficient of thermal expansion |
| WO2015077135A1 (en) * | 2013-11-19 | 2015-05-28 | Corning Incorporated | Ion exchangeable high damage resistance glasses |
| US9517968B2 (en) | 2014-02-24 | 2016-12-13 | Corning Incorporated | Strengthened glass with deep depth of compression |
| US9359243B2 (en) * | 2014-05-13 | 2016-06-07 | Corning Incorporated | Transparent glass-ceramic articles, glass-ceramic precursor glasses and methods for forming the same |
| TWI705889B (zh) | 2014-06-19 | 2020-10-01 | 美商康寧公司 | 無易碎應力分布曲線的玻璃 |
| EP3896042A1 (en) | 2014-10-08 | 2021-10-20 | Corning Incorporated | Glasses and glass ceramics including a metal oxide concentration gradient |
| US10150698B2 (en) | 2014-10-31 | 2018-12-11 | Corning Incorporated | Strengthened glass with ultra deep depth of compression |
| KR102648369B1 (ko) | 2014-11-04 | 2024-03-15 | 코닝 인코포레이티드 | 비-취약성 응력 프로파일 및 이의 제조방법 |
| EP3502074A1 (en) | 2015-06-26 | 2019-06-26 | Corning Incorporated | Glass with high surface strength |
| US11104602B2 (en) | 2015-06-26 | 2021-08-31 | Corning Incorporated | Glass with high surface strength |
| US9701569B2 (en) | 2015-07-21 | 2017-07-11 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
| US11613103B2 (en) | 2015-07-21 | 2023-03-28 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
| EP3386928A1 (en) | 2015-12-08 | 2018-10-17 | Corning Incorporated | S-shaped stress profiles and methods of making |
| TWI675810B (zh) | 2015-12-11 | 2019-11-01 | 美商康寧公司 | 具有金屬氧化物濃度梯度之可熔融成形的玻璃基物件 |
| EP3390313A1 (en) | 2015-12-17 | 2018-10-24 | Corning Incorporated | Ion exchangeable glass with fast diffusion |
| TWI774655B (zh) * | 2016-02-22 | 2022-08-21 | 美商康寧公司 | 無鹼硼鋁矽酸鹽玻璃 |
| KR20210122313A (ko) | 2016-04-08 | 2021-10-08 | 코닝 인코포레이티드 | 두 영역을 포함하는 응력 프로파일을 포함하는 유리-계 물품, 및 제조 방법 |
| DE202017007020U1 (de) | 2016-04-08 | 2019-03-22 | Corning Incorporated | Artikel auf Glasbasis mit einem Metalloxid-Konzentrationsgradienten |
| CN109476530A (zh) | 2016-07-28 | 2019-03-15 | 康宁股份有限公司 | 具有抗光致暗化性的玻璃 |
| KR102640112B1 (ko) | 2016-11-07 | 2024-02-27 | 코닝 인코포레이티드 | 저점도 유리 및 제조를 위한 방법 및 시스템 |
| US11111173B2 (en) | 2016-11-07 | 2021-09-07 | Corning Incorporated | Lithium containing glasses |
| CN110191864B (zh) * | 2017-01-09 | 2022-05-10 | 康宁股份有限公司 | 具有低热膨胀系数的可离子交换玻璃 |
| WO2018164904A1 (en) * | 2017-03-09 | 2018-09-13 | Corning Incorporated | Method of electrostatic charge reduction of glass by surface chemical treatment |
| US11028007B2 (en) | 2017-06-22 | 2021-06-08 | Corning Incorporated | Automotive glass compositions, articles and hybrid laminates |
| NL2020896B1 (en) | 2018-05-08 | 2019-11-14 | Corning Inc | Water-containing glass-based articles with high indentation cracking threshold |
| WO2020102147A2 (en) | 2018-11-16 | 2020-05-22 | Corning Incorporated | Laminated glass articles comprising a hydrogen-containing glass core layer and methods of forming the same |
| TWI891613B (zh) | 2018-11-16 | 2025-08-01 | 美商康寧公司 | 用於透過蒸氣處理而強化之玻璃成分及方法 |
| CN109836037A (zh) * | 2019-03-22 | 2019-06-04 | 科立视材料科技有限公司 | 一种具有低成本高压缩应力层的磷铝硅酸盐玻璃 |
| US12122711B2 (en) | 2019-05-16 | 2024-10-22 | Corning Incorporated | Steam strengthenable glass compositions with low phosphorous content |
| WO2020231959A1 (en) | 2019-05-16 | 2020-11-19 | Corning Incorporated | Glasses with modified young's modulus profile |
| EP3969424B1 (en) | 2019-05-16 | 2024-11-13 | Corning Incorporated | Glass compositions and methods with steam treatment haze resistance |
| JP7296539B2 (ja) * | 2019-11-18 | 2023-06-23 | Agc株式会社 | 支持ガラス基板及び積層体 |
| DE112020006790T5 (de) | 2020-02-25 | 2023-01-12 | Nippon Electric Glass Co., Ltd. | Gehärtete glasplatte und glasplatte zur härtung |
| EP3904306B1 (en) | 2020-04-30 | 2023-06-07 | Schott Ag | Multi-fiber light guide, device with a multi-fiber light guide and method for producing the same |
| GB202012825D0 (en) | 2020-05-12 | 2020-09-30 | Corning Inc | Fusion formable and steam strengthenable glass compositions with platinum compatibility |
| JPWO2022145281A1 (enExample) | 2020-12-28 | 2022-07-07 | ||
| WO2024086037A1 (en) * | 2022-10-21 | 2024-04-25 | Corning Incorporated | Zircon-compatible alkali glasses |
| JP2024094213A (ja) | 2022-12-27 | 2024-07-09 | 日本電気硝子株式会社 | ガラス管及び医薬品容器 |
Family Cites Families (21)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4055703A (en) * | 1975-08-15 | 1977-10-25 | Ppg Industries, Inc. | Ion exchange strengthened glass containing P2 O5 |
| US4042405A (en) * | 1976-03-18 | 1977-08-16 | American Optical Corporation | High strength ophthalmic lens |
| GB2335423A (en) * | 1998-03-20 | 1999-09-22 | Pilkington Plc | Chemically toughenable glass |
| JP5589252B2 (ja) * | 2006-10-10 | 2014-09-17 | 日本電気硝子株式会社 | 強化ガラス基板 |
| KR101221834B1 (ko) * | 2006-10-10 | 2013-01-15 | 니폰 덴키 가라스 가부시키가이샤 | 강화 유리 기판 |
| US8802581B2 (en) * | 2009-08-21 | 2014-08-12 | Corning Incorporated | Zircon compatible glasses for down draw |
| JP5645099B2 (ja) * | 2009-09-09 | 2014-12-24 | 日本電気硝子株式会社 | 強化ガラス |
| US8778820B2 (en) * | 2010-05-27 | 2014-07-15 | Corning Incorporated | Glasses having low softening temperatures and high toughness |
| US9540278B2 (en) * | 2010-05-27 | 2017-01-10 | Corning Incorporated | Ion exchangeable glasses |
| US8759238B2 (en) * | 2010-05-27 | 2014-06-24 | Corning Incorporated | Ion exchangeable glasses |
| JP2012036074A (ja) * | 2010-07-12 | 2012-02-23 | Nippon Electric Glass Co Ltd | ガラス板 |
| US20120052271A1 (en) * | 2010-08-26 | 2012-03-01 | Sinue Gomez | Two-step method for strengthening glass |
| WO2012074983A1 (en) * | 2010-11-30 | 2012-06-07 | Corning Incorporated | Glass with surface and central regions under compression |
| US9346703B2 (en) * | 2010-11-30 | 2016-05-24 | Corning Incorporated | Ion exchangable glass with deep compressive layer and high damage threshold |
| JP2012148909A (ja) * | 2011-01-18 | 2012-08-09 | Nippon Electric Glass Co Ltd | 強化ガラス及び強化ガラス板 |
| JP2013043795A (ja) * | 2011-08-23 | 2013-03-04 | Nippon Electric Glass Co Ltd | 強化ガラス及びその製造方法 |
| KR102306087B1 (ko) | 2011-11-16 | 2021-09-29 | 코닝 인코포레이티드 | 높은 균열 개시 임계값을 갖는 이온 교환가능한 유리 |
| US10941071B2 (en) * | 2013-08-02 | 2021-03-09 | Corning Incorporated | Hybrid soda-lime silicate and aluminosilicate glass articles |
| EP3038983B1 (en) * | 2013-08-27 | 2021-10-20 | Corning Incorporated | Damage resistant glass with high coefficient of thermal expansion |
| TWI689480B (zh) * | 2013-08-29 | 2020-04-01 | 美商康寧公司 | 含有硼及磷的可離子交換玻璃 |
| EP3390313A1 (en) * | 2015-12-17 | 2018-10-24 | Corning Incorporated | Ion exchangeable glass with fast diffusion |
-
2014
- 2014-08-22 EP EP14761494.5A patent/EP3038983B1/en not_active Not-in-force
- 2014-08-22 CN CN201480058858.1A patent/CN105683108A/zh active Pending
- 2014-08-22 US US14/465,888 patent/US9969644B2/en active Active
- 2014-08-22 CN CN202111287979.1A patent/CN113860730A/zh active Pending
- 2014-08-22 KR KR1020167007766A patent/KR102290967B1/ko not_active Expired - Fee Related
- 2014-08-22 JP JP2016538987A patent/JP6600309B2/ja not_active Expired - Fee Related
- 2014-08-22 WO PCT/US2014/052262 patent/WO2015031188A1/en not_active Ceased
- 2014-08-26 TW TW107132600A patent/TWI660930B/zh not_active IP Right Cessation
- 2014-08-26 TW TW103129400A patent/TWI639572B/zh not_active IP Right Cessation
-
2018
- 2018-04-27 US US15/964,688 patent/US10919797B2/en active Active