JP2013095954A5 - - Google Patents

Download PDF

Info

Publication number
JP2013095954A5
JP2013095954A5 JP2011238491A JP2011238491A JP2013095954A5 JP 2013095954 A5 JP2013095954 A5 JP 2013095954A5 JP 2011238491 A JP2011238491 A JP 2011238491A JP 2011238491 A JP2011238491 A JP 2011238491A JP 2013095954 A5 JP2013095954 A5 JP 2013095954A5
Authority
JP
Japan
Prior art keywords
copper alloy
ion secondary
alloy foil
mpa
tensile strength
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
JP2011238491A
Other languages
English (en)
Other versions
JP2013095954A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2011238491A priority Critical patent/JP2013095954A/ja
Priority claimed from JP2011238491A external-priority patent/JP2013095954A/ja
Priority to KR1020137006252A priority patent/KR101669087B1/ko
Priority to PCT/JP2012/069368 priority patent/WO2013018773A1/ja
Priority to EP12819841.3A priority patent/EP2660359A4/en
Priority to TW101127554A priority patent/TWI496954B/zh
Priority to KR1020157022124A priority patent/KR20150097821A/ko
Priority to CN201280004436.7A priority patent/CN103348041B/zh
Publication of JP2013095954A publication Critical patent/JP2013095954A/ja
Priority to US13/965,291 priority patent/US9890463B2/en
Publication of JP2013095954A5 publication Critical patent/JP2013095954A5/ja
Withdrawn legal-status Critical Current

Description

本発明は、正極と、負極集電体の表面に負極活物質層が形成された負極と、非水電解液とを備えるリチウムイオン二次電池、ならびに、特に前記リチウムイオン二次電池の負極電極集電体を構成するのに優れた銅合金箔に関するものである。
本発明の銅合金箔は、常温での引張強度が650MPa以上で、300℃×1時間後の引張強度が450MPa以上で、導電率が80%以上である。
本発明は、常温での引張強さ650MPa以上、300℃×1時間熱処理後の引張強さ450MPa以上、導電率が80%以上の銅合金箔を製造し、提供することができる。
また、本発明によれば膨張、収縮性が大きく、かつポリイミドバインダにより密着性が向上したSi又はSn合金系活物質の大きな膨張、収縮に対して集電体(銅箔)と活物質との密着性を保持しながら、集電体(銅箔)が破断しない銅箔を提供することができ、該銅箔を集電体としたリチウムイオン二次電池用電極、該電極を使用したリチウムイオン二次電池を提供することができる。
また、本発明は塩素イオンの存在下でチオ尿素系化合物を添加することで、銅箔にタングステン(W)を添加することに成功し、上記特性の銅合金箔を提供することができる優れた効果を有するものである。

Claims (4)

  1. 常温での引張強度が650MPa以上で、300℃×1時間後の引張強度が450MPa以上で、導電率が80%以上である銅合金箔。
  2. 常温での伸びが2.5%以上、300℃×1時間後の伸びが3.5%以上である請求項1に記載の銅合金箔。
  3. 請求項1または2に記載の銅合金箔の表面に、シリコン、ゲルマニウム、錫又はそれらの合金化合物またはそれらを主成分とする活物質が堆積されているリチウムイオン二次電池用電極。
  4. 請求項3に記載のリチウムイオン二次電池用電極を使用したリチウムイオン二次電池。
JP2011238491A 2011-07-29 2011-10-31 銅合金箔、該銅合金箔の製造方法及び該銅合金箔を集電体とするリチウムイオン二次電池用電極及びリチウムイオン二次電池 Withdrawn JP2013095954A (ja)