JP2012189986A5 - - Google Patents

Download PDF

Info

Publication number
JP2012189986A5
JP2012189986A5 JP2011274741A JP2011274741A JP2012189986A5 JP 2012189986 A5 JP2012189986 A5 JP 2012189986A5 JP 2011274741 A JP2011274741 A JP 2011274741A JP 2011274741 A JP2011274741 A JP 2011274741A JP 2012189986 A5 JP2012189986 A5 JP 2012189986A5
Authority
JP
Japan
Prior art keywords
refractive index
buffer layer
support member
display
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2011274741A
Other languages
Japanese (ja)
Other versions
JP2012189986A (en
JP6234658B2 (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2011274741A priority Critical patent/JP6234658B2/en
Priority claimed from JP2011274741A external-priority patent/JP6234658B2/en
Publication of JP2012189986A publication Critical patent/JP2012189986A/en
Publication of JP2012189986A5 publication Critical patent/JP2012189986A5/ja
Application granted granted Critical
Publication of JP6234658B2 publication Critical patent/JP6234658B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (15)

表示部に対して観察者側に配置される表示用前面板において、
少なくとも透明基板を含む支持部材と、
前記支持部材の観察者側または表示部側に設けられた緩衝層と、
前記緩衝層上に設けられた反射防止膜と、を備え、
前記支持部材の前記透明基板は、硬質な材料から構成されており、
前記反射防止膜は、最外面に位置する低屈折率層を有し、
前記低屈折率層の光屈折率は前記支持部材の前記透明基板の光屈折率よりも小さくなっており、
前記緩衝層の光屈折率は前記低屈折率層の光屈折率よりも大きくなっており、かつ、前記緩衝層の厚みは前記低屈折率層の厚みよりも大きくなっており、
前記緩衝層は、表示用前面板の外部から前記低屈折率層に応力が印加されている間、低屈折率層に印加される応力を緩和するとともに、応力が取り除かれた後、前記緩衝層の形状がほぼ回復するよう構成されている
ことを特徴とする表示用前面板。
In the display front plate disposed on the viewer side with respect to the display unit,
A support member including at least a transparent substrate;
A buffer layer provided on the observer side or the display unit side of the support member;
An antireflection film provided on the buffer layer,
The transparent substrate of the support member is made of a hard material,
The antireflection film has a low refractive index layer located on the outermost surface,
The light refractive index of the low refractive index layer is smaller than the light refractive index of the transparent substrate of the support member,
The light refractive index of the buffer layer is larger than the light refractive index of the low refractive index layer, and the thickness of the buffer layer is larger than the thickness of the low refractive index layer ,
The buffer layer relaxes stress applied to the low refractive index layer while stress is applied to the low refractive index layer from the outside of the display front plate, and after the stress is removed, the buffer layer A display front plate, wherein the shape of the display is substantially recovered .
前記低屈折率層の厚みは90〜120nmの範囲内となっており、
前記緩衝層の厚みは0.5μm以上となっており、
前記緩衝層に対して5mNの荷重でビッカース圧子を押し込んだ際のビッカース硬さは50〜100の範囲内であり、かつ、その際の前記緩衝層の総変形量に対する前記緩衝層の弾性変形量の割合は0.55以上であることを特徴とする請求項1に記載の表示用前面板。
The thickness of the low refractive index layer is in the range of 90 to 120 nm,
The buffer layer has a thickness of 0.5 μm or more,
The Vickers hardness when the Vickers indenter is pushed into the buffer layer with a load of 5 mN is in the range of 50 to 100, and the elastic deformation amount of the buffer layer with respect to the total deformation amount of the buffer layer at that time The display front plate according to claim 1, wherein the ratio is 0.55 or more.
前記緩衝層に対して5mNの荷重でビッカース圧子を押し込んだ際のビッカース硬さは60〜90の範囲内であり、かつ、その際の前記緩衝層の総変形量に対する前記緩衝層の弾性変形量の割合は0.60以上であることを特徴とする請求項2に記載の表示用前面板。   The Vickers hardness when the Vickers indenter is pushed into the buffer layer with a load of 5 mN is in the range of 60 to 90, and the elastic deformation amount of the buffer layer with respect to the total deformation amount of the buffer layer at that time The display front plate according to claim 2, wherein the ratio of is not less than 0.60. 前記緩衝層は、前記支持部材の前記透明基板の観察者側に直接的に設けられていることを特徴とする請求項1乃至3のいずれかに記載の表示用前面板。   The display front plate according to claim 1, wherein the buffer layer is provided directly on an observer side of the transparent substrate of the support member. 前記反射防止膜は、前記低屈折率層の表示部側に設けられた高屈折率層をさらに有し、
前記高屈折率層の光屈折率は、前記支持部材の前記透明基板の光屈折率よりも大きくなっていることを特徴とする請求項4に記載の表示用前面板。
The antireflection film further includes a high refractive index layer provided on the display unit side of the low refractive index layer,
The display front plate according to claim 4, wherein a light refractive index of the high refractive index layer is larger than a light refractive index of the transparent substrate of the support member.
前記緩衝層の光屈折率と前記支持部材の前記透明基板の光屈折率との差の絶対値が0.03以下になっていることを特徴とする請求項4または5に記載の表示用前面板。   6. The display before display according to claim 4, wherein an absolute value of a difference between a light refractive index of the buffer layer and a light refractive index of the transparent substrate of the support member is 0.03 or less. Face plate. 前記支持部材の表示部側に設けられた追加緩衝層と、
前記追加緩衝層の表示部側に設けられた追加反射防止膜と、をさらに備え、
前記追加反射防止膜は、表示部側の最外面に位置する追加低屈折率層を有し、
前記追加低屈折率層の光屈折率は前記支持部材の前記透明基板の光屈折率よりも小さく、かつ、前記追加低屈折率層の厚みは90〜120nmの範囲内となっており、
前記追加緩衝層の厚みは0.5μm以上となっており、
前記追加緩衝層に対して5mNの荷重でビッカース圧子を押し込んだ際のビッカース硬さは50〜100の範囲内であり、かつ、その際の前記追加緩衝層の総変形量に対する前記追加緩衝層の弾性変形量の割合は0.55以上であることを特徴とする請求項4乃至6のいずれかに記載の表示用前面板。
An additional buffer layer provided on the display portion side of the support member;
An additional antireflection film provided on the display portion side of the additional buffer layer, and
The additional antireflection film has an additional low refractive index layer located on the outermost surface on the display unit side,
The optical refractive index of the additional low refractive index layer is smaller than the optical refractive index of the transparent substrate of the support member, and the thickness of the additional low refractive index layer is in the range of 90 to 120 nm,
The additional buffer layer has a thickness of 0.5 μm or more,
The Vickers hardness when the Vickers indenter is pushed into the additional buffer layer with a load of 5 mN is within a range of 50 to 100, and the additional buffer layer has a total deformation amount with respect to the total deformation amount of the additional buffer layer. The display front plate according to claim 4, wherein a ratio of the elastic deformation amount is 0.55 or more.
前記前記支持部材の表示部側に設けられた追加反射防止膜をさらに備え、
前記追加反射防止膜は、表示部側の最外面に位置する追加低屈折率層を有し、
前記追加低屈折率層の光屈折率は、前記支持部材の前記透明基板の光屈折率よりも小さく、かつ前記反射防止膜の前記低屈折率層の光屈折率よりも大きくなっており、
前記追加低屈折率層の厚みは90〜120nmの範囲内となっていることを特徴とする請求項4乃至6のいずれかに記載の表示用前面板。
An additional antireflection film provided on the display side of the support member;
The additional antireflection film has an additional low refractive index layer located on the outermost surface on the display unit side,
The optical refractive index of the additional low refractive index layer is smaller than the optical refractive index of the transparent substrate of the support member and larger than the optical refractive index of the low refractive index layer of the antireflection film,
The display front plate according to claim 4, wherein a thickness of the additional low refractive index layer is in a range of 90 to 120 nm.
前記追加反射防止膜は、前記追加低屈折率層の観察者側に設けられた追加高屈折率層をさらに有し、
前記追加高屈折率層の光屈折率は、前記支持部材の前記透明基板の光屈折率よりも大きくなっていることを特徴とする請求項7または8に記載の表示用前面板。
The additional antireflection film further includes an additional high refractive index layer provided on the observer side of the additional low refractive index layer,
The display front plate according to claim 7 or 8, wherein a light refractive index of the additional high refractive index layer is larger than a light refractive index of the transparent substrate of the support member.
前記緩衝層は、前記支持部材の前記透明基板の表示部側に直接的に設けられていることを特徴とする請求項1乃至3のいずれかに記載の表示用前面板。   The display front plate according to claim 1, wherein the buffer layer is provided directly on the display unit side of the transparent substrate of the support member. 前記反射防止膜は、前記低屈折率層の観察者側に設けられた高屈折率層をさらに有し、 前記高屈折率層の光屈折率は、前記支持部材の前記透明基板の光屈折率よりも大きくなっていることを特徴とする請求項10に記載の表示用前面板。   The antireflection film further includes a high refractive index layer provided on the observer side of the low refractive index layer, and the optical refractive index of the high refractive index layer is the optical refractive index of the transparent substrate of the support member. The display front plate according to claim 10, wherein the display front plate is larger. 前記緩衝層の光屈折率と前記支持部材の前記透明基板の光屈折率との差の絶対値が0.03以下になっていることを特徴とする請求項10または11に記載の表示用前面板。   The display device according to claim 10 or 11, wherein an absolute value of a difference between a light refractive index of the buffer layer and a light refractive index of the transparent substrate of the support member is 0.03 or less. Face plate. センサ部を含むタッチパネルセンサをさらに備えたことを特徴とする請求項1乃至12のいずれかに記載の表示用前面板。   The display front plate according to claim 1, further comprising a touch panel sensor including a sensor unit. 前記センサ部が前記支持部材の前記透明基板の観察者側の面上または表示部側の面上に形成されていることを特徴とする請求項13に記載の表示用前面板。   14. The display front plate according to claim 13, wherein the sensor unit is formed on an observer side surface or a display unit side surface of the transparent substrate of the support member. 映像を表示するための光を観察者側に放射する表示部と、
前記表示部に対して観察者側に配置された表示用前面板と、を備え、
前記表示用前面板は、
少なくとも透明基板を含む支持部材と、
前記支持部材の観察者側または表示部側に設けられた緩衝層と、
前記緩衝層上に設けられた反射防止膜と、を備え、
前記支持部材の前記透明基板は、硬質な材料から構成されており、
前記反射防止膜は、最外面に位置する低屈折率層を有し、
前記低屈折率層の光屈折率は前記支持部材の前記透明基板の光屈折率よりも小さくなっており、
前記緩衝層の光屈折率は前記低屈折率層の光屈折率よりも大きくなっており、かつ、前記緩衝層の厚みは前記低屈折率層の厚みよりも大きくなっており、
前記緩衝層は、表示用前面板の外部から前記低屈折率層に応力が印加されている間、低屈折率層に印加される応力を緩和するとともに、応力が取り除かれた後、前記緩衝層の形状がほぼ回復するよう構成されている
ことを特徴とする表示装置。
A display unit that emits light for displaying images to the viewer side;
A display front plate disposed on the viewer side with respect to the display unit,
The display front plate is
A support member including at least a transparent substrate ;
A buffer layer provided on the observer side or the display unit side of the support member ;
An antireflection film provided on the buffer layer,
The transparent substrate of the support member is made of a hard material,
The antireflection film has a low refractive index layer located on the outermost surface,
The light refractive index of the low refractive index layer is smaller than the light refractive index of the transparent substrate of the support member,
The light refractive index of the buffer layer is larger than the light refractive index of the low refractive index layer, and the thickness of the buffer layer is larger than the thickness of the low refractive index layer ,
The buffer layer relaxes stress applied to the low refractive index layer while stress is applied to the low refractive index layer from the outside of the display front plate, and after the stress is removed, the buffer layer A display device characterized in that the shape of the display is substantially recovered .
JP2011274741A 2010-12-16 2011-12-15 Display front plate and display device Active JP6234658B2 (en)