JP2009032674A5 - - Google Patents

Download PDF

Info

Publication number
JP2009032674A5
JP2009032674A5 JP2008144695A JP2008144695A JP2009032674A5 JP 2009032674 A5 JP2009032674 A5 JP 2009032674A5 JP 2008144695 A JP2008144695 A JP 2008144695A JP 2008144695 A JP2008144695 A JP 2008144695A JP 2009032674 A5 JP2009032674 A5 JP 2009032674A5
Authority
JP
Japan
Prior art keywords
bonding material
manufacturing
heating
airtight container
container according
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2008144695A
Other languages
Japanese (ja)
Other versions
JP5025566B2 (en
JP2009032674A (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2008144695A priority Critical patent/JP5025566B2/en
Priority claimed from JP2008144695A external-priority patent/JP5025566B2/en
Priority to US12/136,181 priority patent/US7972461B2/en
Priority to CN2008101317812A priority patent/CN101335167B/en
Publication of JP2009032674A publication Critical patent/JP2009032674A/en
Publication of JP2009032674A5 publication Critical patent/JP2009032674A5/ja
Application granted granted Critical
Publication of JP5025566B2 publication Critical patent/JP5025566B2/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (11)

気密容器の製造方法であって、
気密容器を構成する第1の部材及び第2の部材の互いに対向する面の一方の面に、第2の接合材を環状に配置し、且つ該第2の接合材よりも押付圧力に対する圧縮率が小さい第1の接合材を、該第1の接合材の高さが該第2の接合材よりも小さくなるように、該第2の接合材に併設させて配置する、接合材配置工程と、
前記第1の接合材及び前記第2の接合材が、前記互いに対向する面の他方の面に接触するように、該他方の面を前記第1の接合材及び前記第2の接合材に押付ける加圧工程と、
前記他方の面に接触した前記第1の接合材を部分ごとに順次加熱溶融させる加熱工程と、
前記第1の接合材の加熱溶融した部分を冷却する工程と、
を有する、気密容器の製造方法。
A method of manufacturing an airtight container,
A second bonding material is annularly arranged on one surface of the first member and the second member of the airtight container that face each other, and the compressibility against the pressing pressure is higher than that of the second bonding material. A first bonding material having a small size is disposed adjacent to the second bonding material such that the height of the first bonding material is smaller than that of the second bonding material; ,
The first bonding material and the second bonding material, said to be in contact with the other surface of the opposing surfaces to each other, pressing the surface of said other to said first joining material and the second bonding material Applying a pressing process;
A heating step of sequentially heating and melting the first bonding material in contact with the other surface for each portion;
Cooling the heated and melted portion of the first bonding material;
A method for manufacturing an airtight container.
前記加熱工程は、前記第1の接合材の複数の部分を同時に加熱溶融させることを含む、請求項1に記載の気密容器の製造方法。   The method for manufacturing an airtight container according to claim 1, wherein the heating step includes simultaneously heating and melting a plurality of portions of the first bonding material. 前記加熱工程は、前記第1の接合材の加熱位置を変えながら複数回の加熱を行うことによって、前記第1の接合材の全てを加熱溶融させることを含む、請求項1または2に記載の気密容器の製造方法。   3. The heating step according to claim 1, wherein the heating step includes heating and melting all of the first bonding material by performing heating a plurality of times while changing a heating position of the first bonding material. A manufacturing method of an airtight container. 前記加熱工程は、前記第1の接合材に沿って加熱位置を走査しながら該第1の接合材を順次加熱溶融させることを含む、請求項1に記載の気密容器の製造方法。   2. The method for manufacturing an airtight container according to claim 1, wherein the heating step includes sequentially heating and melting the first bonding material while scanning a heating position along the first bonding material. 前記加熱工程は第1の接合材を局所加熱することを含む、請求項1からのいずれか1項に記載の気密容器の製造方法。 It said heating step comprises locally heating the first joining material, a manufacturing method of the airtight container according to any one of claims 1 to 4. 前記局所加熱は、レーザの照射によって行われる、請求項5に記載の気密容器の製造方法。   The method for manufacturing an airtight container according to claim 5, wherein the local heating is performed by laser irradiation. 前記局所加熱は、ハロゲンランプを照射することによって行われる、請求項5に記載の気密容器の製造方法。   The said local heating is a manufacturing method of the airtight container of Claim 5 performed by irradiating a halogen lamp. 前記第1の部材及び前記第2の部材はガラスからなり、
前記第1の接合材は金属またはガラスフリットからなる、
請求項7に記載の気密容器の製造方法。
The first member and the second member are made of glass,
The first bonding material is made of metal or glass frit.
The manufacturing method of the airtight container of Claim 7.
前記接合材配置工程は、前記第1の接合材として、シート状に焼成されたガラスフリットを用いることを含む、請求項に記載の気密容器の製造方法。 The method for manufacturing an airtight container according to claim 1 , wherein the bonding material arranging step includes using a glass frit baked into a sheet shape as the first bonding material. 前記接合材配置工程は、前記第1の接合材として、シート状のアルミニウムを用いることを含む、請求項に記載の気密容器の製造方法。 The method for manufacturing an airtight container according to claim 1 , wherein the bonding material arranging step includes using sheet-like aluminum as the first bonding material. 気密容器内に電子放出素子と画像形成部材とを有する画像表示装置の製造方法であって、前記気密容器が、請求項1から10のいずれか1項に記載の気密容器の製造方法によって形成されることを特徴とする画像表示装置の製造方法。   11. A method for manufacturing an image display device having an electron-emitting device and an image forming member in an air-tight container, wherein the air-tight container is formed by the method for manufacturing an air-tight container according to claim 1. A method of manufacturing an image display device.
JP2008144695A 2007-06-27 2008-06-02 Airtight container and method for manufacturing image forming apparatus using the same Expired - Fee Related JP5025566B2 (en)