JP2008524444A5 - - Google Patents

Download PDF

Info

Publication number
JP2008524444A5
JP2008524444A5 JP2007546870A JP2007546870A JP2008524444A5 JP 2008524444 A5 JP2008524444 A5 JP 2008524444A5 JP 2007546870 A JP2007546870 A JP 2007546870A JP 2007546870 A JP2007546870 A JP 2007546870A JP 2008524444 A5 JP2008524444 A5 JP 2008524444A5
Authority
JP
Japan
Prior art keywords
based alloy
component
weight percent
metal
balance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2007546870A
Other languages
English (en)
Japanese (ja)
Other versions
JP2008524444A (ja
JP4866860B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority claimed from PCT/US2005/045318 external-priority patent/WO2006065939A1/en
Publication of JP2008524444A publication Critical patent/JP2008524444A/ja
Publication of JP2008524444A5 publication Critical patent/JP2008524444A5/ja
Application granted granted Critical
Publication of JP4866860B2 publication Critical patent/JP4866860B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP2007546870A 2004-12-15 2005-12-15 内燃エンジン用部品への耐高温劣化性の付与 Expired - Fee Related JP4866860B2 (ja)

Applications Claiming Priority (3)

Application Number Priority Date Filing Date Title
US63639804P 2004-12-15 2004-12-15
US60/636,398 2004-12-15
PCT/US2005/045318 WO2006065939A1 (en) 2004-12-15 2005-12-15 Imparting high-temperature degradation resistance to components for internal combustion engine systems

Publications (3)

Publication Number Publication Date
JP2008524444A JP2008524444A (ja) 2008-07-10
JP2008524444A5 true JP2008524444A5 (enExample) 2009-02-19
JP4866860B2 JP4866860B2 (ja) 2012-02-01

Family

ID=36088298

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2007546870A Expired - Fee Related JP4866860B2 (ja) 2004-12-15 2005-12-15 内燃エンジン用部品への耐高温劣化性の付与

Country Status (7)

Country Link
US (3) US8383203B2 (enExample)
EP (1) EP1844182B1 (enExample)
JP (1) JP4866860B2 (enExample)
AT (1) ATE478977T1 (enExample)
CA (1) CA2595712C (enExample)
DE (1) DE602005023218D1 (enExample)
WO (1) WO2006065939A1 (enExample)

Families Citing this family (21)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4545068B2 (ja) * 2005-08-25 2010-09-15 三菱重工業株式会社 可変容量型排気ターボ過給機及び可変ノズル機構構成部材の製造方法
US7749570B2 (en) * 2006-12-20 2010-07-06 General Electric Company Method for depositing a platinum-group-containing layer on a substrate
US8235092B2 (en) * 2007-01-30 2012-08-07 Minop Co. Insulated investment casting mold and method of making
DE102008053222A1 (de) * 2008-10-25 2010-04-29 Bosch Mahle Turbo Systems Gmbh & Co. Kg Turbolader
US8962154B2 (en) * 2011-06-17 2015-02-24 Kennametal Inc. Wear resistant inner coating for pipes and pipe fittings
EP2773860B8 (en) * 2011-10-31 2021-12-22 Tenneco Inc. Coated piston and a method of making a coated piston
US8828312B2 (en) * 2011-12-08 2014-09-09 Kennametal Inc. Dilution control in hardfacing severe service components
KR101981195B1 (ko) * 2012-04-29 2019-05-22 보르그워너 인코퍼레이티드 마모성 코팅을 구비한 vtg 터보차저 베인 팩 조립체
US20140272446A1 (en) * 2013-03-15 2014-09-18 Kannametal Inc. Wear-resistant claddings
US9346101B2 (en) * 2013-03-15 2016-05-24 Kennametal Inc. Cladded articles and methods of making the same
US9862029B2 (en) 2013-03-15 2018-01-09 Kennametal Inc Methods of making metal matrix composite and alloy articles
DE102013207440A1 (de) * 2013-04-24 2014-10-30 Bosch Mahle Turbo Systems Gmbh & Co. Kg Verfahren zur Herstellung eines Hebels einer variablen Turbinengeometrie
US10221702B2 (en) 2015-02-23 2019-03-05 Kennametal Inc. Imparting high-temperature wear resistance to turbine blade Z-notches
US10072504B2 (en) * 2015-12-22 2018-09-11 General Electric Company Alloy, welded article and welding process
JP6650347B2 (ja) * 2016-06-01 2020-02-19 三菱重工業株式会社 ターボチャージャ及びその製造方法
DE202016103778U1 (de) * 2016-07-13 2016-07-27 Bosch Mahle Turbo Systems Gmbh & Co. Kg Verstellring einer variablen Turbinengeometrie
US11117208B2 (en) 2017-03-21 2021-09-14 Kennametal Inc. Imparting wear resistance to superalloy articles
US11155904B2 (en) 2019-07-11 2021-10-26 L.E. Jones Company Cobalt-rich wear resistant alloy and method of making and use thereof
US11618075B2 (en) * 2020-11-13 2023-04-04 Garrett Transportation I Inc. Methods for the combined sintering and surface treatment of variable geometry turbocharger vanes
US11661861B2 (en) * 2021-03-03 2023-05-30 Garrett Transportation I Inc. Bi-metal variable geometry turbocharger vanes and methods for manufacturing the same using laser cladding
CN113604709A (zh) * 2021-08-18 2021-11-05 沈阳大陆激光先进制造技术创新有限公司 一种激光复合制造炉卷辊抗高温压入功能层合金材料及工艺方法

Family Cites Families (26)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3257178A (en) * 1966-06-21 Coated metal article
US3331700A (en) * 1963-04-01 1967-07-18 Du Pont Method of coating metals
US3330700A (en) * 1963-06-17 1967-07-11 Electro Optical Systems Inc Solar-cell panels
US3410732A (en) * 1965-04-30 1968-11-12 Du Pont Cobalt-base alloys
US3361560A (en) * 1966-04-19 1968-01-02 Du Pont Nickel silicon and refractory metal alloy
US3743556A (en) * 1970-03-30 1973-07-03 Composite Sciences Coating metallic substrate with powdered filler and molten metal
US3720537A (en) * 1970-11-25 1973-03-13 United Aircraft Corp Process of coating an alloy substrate with an alloy
US3676085A (en) * 1971-02-18 1972-07-11 United Aircraft Corp Cobalt base coating for the superalloys
US3795430A (en) * 1972-10-19 1974-03-05 Du Pont Wear resistant frictionally contacting surfaces
US3839024A (en) * 1973-02-15 1974-10-01 Du Pont Wear and corrosion resistant alloy
US3989863A (en) * 1975-07-09 1976-11-02 The International Nickel Company, Inc. Slurry coating process
US4124737A (en) * 1976-12-30 1978-11-07 Union Carbide Corporation High temperature wear resistant coating composition
US4421717A (en) * 1982-06-10 1983-12-20 Ford Motor Company Method of making wear resistant ferrous based parts
US4490411A (en) * 1983-03-14 1984-12-25 Darryl Feder Apparatus for and method of metalizing internal surfaces of metal bodies such as tubes and pipes
AR007698A1 (es) * 1996-08-28 1999-11-10 Deere & Co Metodo para aportar dureza superficial a una superficie metalica y un lodo preparado por dicho metodo
DE69803332T2 (de) * 1997-05-21 2002-08-29 Kabushiki Kaisha Toyota Chuo Kenkyusho, Nagakute Hartmolybdänlegierung, verschliessfeste Legierung und Verfahren zu ihrer Herstellung
US6649682B1 (en) * 1998-12-22 2003-11-18 Conforma Clad, Inc Process for making wear-resistant coatings
US7262240B1 (en) * 1998-12-22 2007-08-28 Kennametal Inc. Process for making wear-resistant coatings
US6413582B1 (en) * 1999-06-30 2002-07-02 General Electric Company Method for forming metallic-based coating
CA2314565C (en) * 1999-07-27 2007-06-12 Deloro Stellite Company, Inc. Saw blade tips and alloys therefor
CA2348145C (en) * 2001-05-22 2005-04-12 Surface Engineered Products Corporation Protective system for high temperature metal alloys
JP2002146409A (ja) 2000-11-06 2002-05-22 Toyota Motor Corp 焼結体の製造方法
US6805906B2 (en) * 2001-03-08 2004-10-19 Liburdi Engineering Limited Method of application of a protective coating to a substrate
US6749894B2 (en) * 2002-06-28 2004-06-15 Surface Engineered Products Corporation Corrosion-resistant coatings for steel tubes
US6852176B2 (en) * 2002-07-17 2005-02-08 Deloro Stellite Holdings Corporation Wear-resistant, corrosion-resistant cobalt-based alloys
JP2004153087A (ja) 2002-10-31 2004-05-27 Dainippon Ink & Chem Inc 電解コンデンサ陽極素子用電極とその製造方法

Similar Documents

Publication Publication Date Title
JP2008524444A5 (enExample)
US9340856B2 (en) Ni—Fe—Cr alloy and engine valve welded with the same alloy
JP5744006B2 (ja) 超合金部品およびスラリー組成物
CN105121678B (zh) 耐热性Ni基合金及其制造方法
JP6140260B2 (ja) 溶射用の溶射粉末、ピストンリング及びその製造方法
US9023423B2 (en) Method of deposition of metallic coatings using atomized spray
JP4866860B2 (ja) 内燃エンジン用部品への耐高温劣化性の付与
US5281484A (en) High stress capability, intermetallic phase titanium aluminide coated components
JP5755819B2 (ja) 耐高温腐食特性を備えたNi−Cr−Co系合金とそれを用いて表面改質したポペットバルブ
CN1115421C (zh) 以铝化钛为基础的合金
KR20180007693A (ko) 기계 부품의 제조 방법
JP5727903B2 (ja) 表面硬化用Co基合金
JP5763847B2 (ja) エンジンバルブ
JP2013533920A (ja) 無鉛滑り軸受
CN103402756B (zh) 制造无铅镀铝滑动轴承的方法
US9561556B2 (en) Process for producing intermetallic wear-resistant layer for titanium materials
CN1360074A (zh) 钛铝合金
US7261784B2 (en) Method of making a coating on a metal substrate and/or an article, such a coating, such a metal substrate and/or an article, and a cam forming such an article
Huang et al. Mechanical properties and corrosion resistance of a novel Ni‐Cr‐Mo alloy
JP2000199045A (ja) 溶射物および溶射方法
JPH01241A (ja) 超耐熱合金
JPH06322506A (ja) 溶射用合金粉末
Zhang et al. Synthesis and Evaluation of TiC/Al3Ti Coating on Iron Via Thermal Explosion of Al-Ti-C System
Chen et al. The effects of heat treatment on the microstructural characteristics of laser-consolidated IN-625 and IN-738 superalloys
Noda The state of development and practical use of intermetallic compound TiAl