JP2008240036A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2008240036A5 JP2008240036A5 JP2007079917A JP2007079917A JP2008240036A5 JP 2008240036 A5 JP2008240036 A5 JP 2008240036A5 JP 2007079917 A JP2007079917 A JP 2007079917A JP 2007079917 A JP2007079917 A JP 2007079917A JP 2008240036 A5 JP2008240036 A5 JP 2008240036A5
- Authority
- JP
- Japan
- Prior art keywords
- stain
- evaluation
- evaluation criteria
- temperature
- stain resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000011156 evaluation Methods 0.000 description 4
- 229910000831 Steel Inorganic materials 0.000 description 1
- 239000010959 steel Substances 0.000 description 1
Priority Applications (4)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2007079917A JP5311756B2 (ja) | 2007-03-26 | 2007-03-26 | 耐しみ汚れ性に優れた電気Znめっき鋼板 |
| CNA2008100094821A CN101307474A (zh) | 2007-03-26 | 2008-02-03 | 耐斑污性优良的电镀锌钢板 |
| TW097105795A TWI369419B (en) | 2007-03-26 | 2008-02-19 | Stain-resistant electrogalvanized steel sheet |
| KR1020080027168A KR100987912B1 (ko) | 2007-03-26 | 2008-03-25 | 내얼룩 오염성이 우수한 전기 Zn 도금 강판 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2007079917A JP5311756B2 (ja) | 2007-03-26 | 2007-03-26 | 耐しみ汚れ性に優れた電気Znめっき鋼板 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2008240036A JP2008240036A (ja) | 2008-10-09 |
| JP2008240036A5 true JP2008240036A5 (enExample) | 2010-06-24 |
| JP5311756B2 JP5311756B2 (ja) | 2013-10-09 |
Family
ID=39911721
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2007079917A Expired - Fee Related JP5311756B2 (ja) | 2007-03-26 | 2007-03-26 | 耐しみ汚れ性に優れた電気Znめっき鋼板 |
Country Status (4)
| Country | Link |
|---|---|
| JP (1) | JP5311756B2 (enExample) |
| KR (1) | KR100987912B1 (enExample) |
| CN (1) | CN101307474A (enExample) |
| TW (1) | TWI369419B (enExample) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2009197303A (ja) * | 2008-02-25 | 2009-09-03 | Kobe Steel Ltd | 耐しみ汚れ性に優れた電気Znめっき鋼板 |
| KR101112580B1 (ko) * | 2009-01-09 | 2012-02-22 | 오경호 | 인조 동판 제조방법 |
| CN103140605B (zh) * | 2010-09-29 | 2015-09-02 | 杰富意钢铁株式会社 | 镀锌系钢板 |
| CN104878417A (zh) * | 2015-06-26 | 2015-09-02 | 厦门理工学院 | 一种电镀液、三维多孔结构锌薄膜材料及其制备方法 |
| JP6427541B2 (ja) * | 2016-09-16 | 2018-11-21 | 本田技研工業株式会社 | 亜鉛−ニッケル複合めっき浴及びめっき方法 |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH08188898A (ja) * | 1995-01-11 | 1996-07-23 | Kobe Steel Ltd | 電気亜鉛めっき鋼板およびその製法 |
| JPH09195082A (ja) * | 1996-01-17 | 1997-07-29 | Nippon Steel Corp | めっき外観に優れた電気亜鉛めっき鋼板及びその製造方法 |
| JP3043336B1 (ja) * | 1999-06-11 | 2000-05-22 | 株式会社神戸製鋼所 | 耐白錆性に優れる電気Znめっき鋼板およびその製造方法 |
| WO2002078949A1 (en) | 2001-03-30 | 2002-10-10 | Nippon Steel Corporation | Metal product surface-treated with alkali-soluble lubricating film exhibiting excellent formability and excellent film removal property being stable for a long time and independent of temperature for drying film |
| JP3801470B2 (ja) * | 2001-08-29 | 2006-07-26 | 新日本製鐵株式会社 | 防錆剤含有水分散性金属表面処理剤、表面処理金属材とその製造方法 |
| JP4318610B2 (ja) | 2004-07-30 | 2009-08-26 | 株式会社神戸製鋼所 | 表面処理金属板 |
| JP4057626B2 (ja) * | 2006-08-11 | 2008-03-05 | 株式会社神戸製鋼所 | 耐しみ汚れ性に優れた電気Znめっき鋼板 |
-
2007
- 2007-03-26 JP JP2007079917A patent/JP5311756B2/ja not_active Expired - Fee Related
-
2008
- 2008-02-03 CN CNA2008100094821A patent/CN101307474A/zh active Pending
- 2008-02-19 TW TW097105795A patent/TWI369419B/zh not_active IP Right Cessation
- 2008-03-25 KR KR1020080027168A patent/KR100987912B1/ko not_active Expired - Fee Related