JP2004169064A5 - - Google Patents

Download PDF

Info

Publication number
JP2004169064A5
JP2004169064A5 JP2002333268A JP2002333268A JP2004169064A5 JP 2004169064 A5 JP2004169064 A5 JP 2004169064A5 JP 2002333268 A JP2002333268 A JP 2002333268A JP 2002333268 A JP2002333268 A JP 2002333268A JP 2004169064 A5 JP2004169064 A5 JP 2004169064A5
Authority
JP
Japan
Prior art keywords
copper
powder
alloy
hip
temperature
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2002333268A
Other languages
English (en)
Japanese (ja)
Other versions
JP2004169064A (ja
JP4295491B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2002333268A priority Critical patent/JP4295491B2/ja
Priority claimed from JP2002333268A external-priority patent/JP4295491B2/ja
Publication of JP2004169064A publication Critical patent/JP2004169064A/ja
Publication of JP2004169064A5 publication Critical patent/JP2004169064A5/ja
Application granted granted Critical
Publication of JP4295491B2 publication Critical patent/JP4295491B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP2002333268A 2002-11-18 2002-11-18 銅−タングステン合金およびその製造方法 Expired - Fee Related JP4295491B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2002333268A JP4295491B2 (ja) 2002-11-18 2002-11-18 銅−タングステン合金およびその製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2002333268A JP4295491B2 (ja) 2002-11-18 2002-11-18 銅−タングステン合金およびその製造方法

Publications (3)

Publication Number Publication Date
JP2004169064A JP2004169064A (ja) 2004-06-17
JP2004169064A5 true JP2004169064A5 (enrdf_load_stackoverflow) 2006-01-12
JP4295491B2 JP4295491B2 (ja) 2009-07-15

Family

ID=32698035

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2002333268A Expired - Fee Related JP4295491B2 (ja) 2002-11-18 2002-11-18 銅−タングステン合金およびその製造方法

Country Status (1)

Country Link
JP (1) JP4295491B2 (enrdf_load_stackoverflow)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
EP1443546A3 (en) * 2003-01-28 2009-05-06 Hitachi Ltd. Working method of metal material and semiconductor apparatus fabricated by the method
JP4508736B2 (ja) * 2004-06-15 2010-07-21 靖 渡辺 銅系材料およびその製造方法
JP5122856B2 (ja) * 2007-04-19 2013-01-16 光洋機械工業株式会社 放電ツルーイング電極、放電ツルーイング装置および研削装置
JP5318401B2 (ja) * 2007-10-25 2013-10-16 冨士ダイス株式会社 快削性銅−タングステン合金
JP5051168B2 (ja) * 2009-03-31 2012-10-17 日立ツール株式会社 窒化物分散Ti−Al系ターゲット及びその製造方法
CN112530724B (zh) * 2020-10-19 2023-09-08 陕西斯瑞新材料股份有限公司 一种利用钨粉制造电子束焊接铜钨触片的方法
CN115625334A (zh) * 2022-09-27 2023-01-20 宁波江丰电子材料股份有限公司 一种钨铜热沉材料及其制备方法与应用

Similar Documents

Publication Publication Date Title
CN110845237B (zh) 高熵陶瓷粉体及其制备方法和高熵陶瓷块体
CN101667498A (zh) 一种钨铜电触头的制备方法
CN108251685A (zh) 一种钨弥散强化铜基复合材料及其制备方法
CN106893951A (zh) 铜基块体非晶合金复合材料及其制备方法
CN107790722A (zh) 一种双孔结构TiAl多孔材料的制备方法
JP5376274B2 (ja) 良導電性ダイヤモンド焼結体の製造方法
JP4410066B2 (ja) 電気接点材料の製造方法
JP2004169064A5 (enrdf_load_stackoverflow)
CN101538694B (zh) 一种钛基非晶合金及其制备方法
CN108754272B (zh) 一种大长径比细晶钨铜棒材的制备方法
CN104878266A (zh) 一种具有高温稳定性的钨-碳化锆-铼合金及其制备方法
JP4295491B2 (ja) 銅−タングステン合金およびその製造方法
CN111618297B (zh) 一种快速烧结成型银基触头制备方法
CN110499435B (zh) 一种银基电接触材料及其制备方法
CN110846596A (zh) 一种Wf/W合金-金刚石复合材料及其制备方法
CN105463240A (zh) 一种铜铬电触头材料的制备方法
US1026343A (en) Manufacture of refractory conductors.
CN114480898B (zh) 一种Ti-13Cu-1Al合金材料及制备方法
CN114804892B (zh) 一种用于铝溶液加热器的氮化硅保护管及其制备方法
JP4603841B2 (ja) 耐酸化性を有するタングステン合金とその製造方法
CN109930031B (zh) ZrTiAlNiV合金的制备方法
JP4068486B2 (ja) 抵抗溶接用電極材料およびその製造方法
US4088503A (en) Backing for weld underside formation
JP5950400B2 (ja) 炭素材料及びその製造方法
CN105506342B (zh) 一种铆钉型银石墨电触头材料的制备方法