JP2004163981A5 - - Google Patents

Download PDF

Info

Publication number
JP2004163981A5
JP2004163981A5 JP2004030367A JP2004030367A JP2004163981A5 JP 2004163981 A5 JP2004163981 A5 JP 2004163981A5 JP 2004030367 A JP2004030367 A JP 2004030367A JP 2004030367 A JP2004030367 A JP 2004030367A JP 2004163981 A5 JP2004163981 A5 JP 2004163981A5
Authority
JP
Japan
Prior art keywords
film
drying
stretching
temperature
stage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2004030367A
Other languages
English (en)
Japanese (ja)
Other versions
JP4049382B2 (ja
JP2004163981A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2004030367A priority Critical patent/JP4049382B2/ja
Priority claimed from JP2004030367A external-priority patent/JP4049382B2/ja
Publication of JP2004163981A publication Critical patent/JP2004163981A/ja
Publication of JP2004163981A5 publication Critical patent/JP2004163981A5/ja
Application granted granted Critical
Publication of JP4049382B2 publication Critical patent/JP4049382B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

JP2004030367A 2004-02-06 2004-02-06 位相差フィルムの製造方法 Expired - Lifetime JP4049382B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2004030367A JP4049382B2 (ja) 2004-02-06 2004-02-06 位相差フィルムの製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2004030367A JP4049382B2 (ja) 2004-02-06 2004-02-06 位相差フィルムの製造方法

Related Parent Applications (1)

Application Number Title Priority Date Filing Date
JP17835497A Division JPH1119954A (ja) 1997-07-03 1997-07-03 位相差フィルムの製造方法およびその装置

Publications (3)

Publication Number Publication Date
JP2004163981A JP2004163981A (ja) 2004-06-10
JP2004163981A5 true JP2004163981A5 (enExample) 2007-02-08
JP4049382B2 JP4049382B2 (ja) 2008-02-20

Family

ID=32822064

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2004030367A Expired - Lifetime JP4049382B2 (ja) 2004-02-06 2004-02-06 位相差フィルムの製造方法

Country Status (1)

Country Link
JP (1) JP4049382B2 (enExample)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007121351A (ja) * 2005-10-25 2007-05-17 Kaneka Corp 位相差フィルム、及びその製造方法、並びに光学補償偏光板
JP2008068533A (ja) * 2006-09-14 2008-03-27 Fujifilm Corp 熱可塑性樹脂フィルムの縦延伸方法及びその方法で製造された縦延伸フィルム
JP4716036B2 (ja) * 2007-03-12 2011-07-06 富士フイルム株式会社 光学補償フィルムの製造方法
KR101433691B1 (ko) * 2007-09-21 2014-08-25 스미또모 가가꾸 가부시키가이샤 열가소성 수지제 위상차 필름의 제조 방법
JP5034897B2 (ja) * 2007-11-27 2012-09-26 コニカミノルタアドバンストレイヤー株式会社 芳香族ポリカーボネートフィルムの製造方法、芳香族ポリカーボネートフィルム、及び有機エレクトロルミネッセンス素子用基板
WO2011118145A1 (ja) * 2010-03-24 2011-09-29 コニカミノルタオプト株式会社 光学フィルムの製造方法、光学フィルム、偏光板、及び液晶表示装置
CN113232279A (zh) * 2021-05-17 2021-08-10 山西丁火光电科技有限公司 一种位相差膜制造方法

Similar Documents

Publication Publication Date Title
JP2011525634A5 (enExample)
JP2004163981A5 (enExample)
JP2005314669A5 (enExample)
JP2005330411A5 (enExample)
JP5657261B2 (ja) 溶液製膜方法
JPH01198638A (ja) ポリイミドフィルムの製造法
KR101857577B1 (ko) 저헤이즈 아크릴 수지 필름 제조 방법
JP2005301225A5 (enExample)
TWI669335B (zh) 丙烯酸樹脂薄膜
JP4049382B2 (ja) 位相差フィルムの製造方法
TW202101044A (zh) 偏光膜、偏光板、及該偏光膜之製造方法
KR101838493B1 (ko) 저투습 편광판
JP6955008B2 (ja) アクリルフィルム
KR101894814B1 (ko) 내응력(耐應力) 내백화(耐白化) 필름
KR102112028B1 (ko) 아크릴 필름
KR101894813B1 (ko) 내가열(耐加熱) 내백화(耐白化) 필름
KR101928860B1 (ko) 아크릴 필름
TW202039599A (zh) 偏光膜、偏光板及該偏光膜之製造方法
KR20190027011A (ko) 저투습 편광판
KR20180079615A (ko) 내응력(耐應力) 내백화(耐白化) 필름
JP4253791B2 (ja) ポリイミドフィルムの製造方法
KR20180079616A (ko) 내응력(耐應力) 내백화(耐白化) 필름
JP5636216B2 (ja) フィルム製造方法及び溶液製膜装置
KR101936702B1 (ko) 코팅 아크릴 필름
TWI692501B (zh) 丙烯酸樹脂薄膜