JP2000355746A5 - - Google Patents
Info
- Publication number
- JP2000355746A5 JP2000355746A5 JP2000-145460A JP2000145460A JP2000355746A5 JP 2000355746 A5 JP2000355746 A5 JP 2000355746A5 JP 2000145460 A JP2000145460 A JP 2000145460A JP 2000355746 A5 JP2000355746 A5 JP 2000355746A5
- Authority
- JP
- Japan
- Prior art keywords
- brass
- content
- rod
- hot extrusion
- amendment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2000145460A JP3303878B2 (ja) | 1996-09-09 | 2000-05-17 | 黄銅の製造方法及び製造設備 |
Applications Claiming Priority (21)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23759196 | 1996-09-09 | ||
| JP29177596 | 1996-11-01 | ||
| JP402797 | 1997-01-13 | ||
| JP3184997 | 1997-02-17 | ||
| JP7411197 | 1997-03-26 | ||
| JP8-237591 | 1997-05-20 | ||
| JP9-167837 | 1997-05-20 | ||
| JP8-291775 | 1997-05-20 | ||
| JP9-167836 | 1997-05-20 | ||
| JP9-167834 | 1997-05-20 | ||
| JP16783797 | 1997-05-20 | ||
| JP16783697 | 1997-05-20 | ||
| JP16783597 | 1997-05-20 | ||
| JP9-31849 | 1997-05-20 | ||
| JP16783497 | 1997-05-20 | ||
| JP9-74111 | 1997-05-20 | ||
| JP9-167835 | 1997-05-20 | ||
| JP9-167833 | 1997-05-20 | ||
| JP16783397 | 1997-05-20 | ||
| JP9-4027 | 1997-05-20 | ||
| JP2000145460A JP3303878B2 (ja) | 1996-09-09 | 2000-05-17 | 黄銅の製造方法及び製造設備 |
Related Parent Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP51249198A Division JP3303301B2 (ja) | 1996-09-09 | 1997-09-08 | 銅合金及びその製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2000355746A JP2000355746A (ja) | 2000-12-26 |
| JP2000355746A5 true JP2000355746A5 (enExample) | 2001-11-09 |
| JP3303878B2 JP3303878B2 (ja) | 2002-07-22 |
Family
ID=27581742
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2000145460A Expired - Lifetime JP3303878B2 (ja) | 1996-09-09 | 2000-05-17 | 黄銅の製造方法及び製造設備 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3303878B2 (enExample) |
Families Citing this family (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB2419603B (en) | 2002-07-18 | 2006-11-22 | Honda Motor Co Ltd | Composite copper material |
| FI118328B (fi) * | 2005-02-18 | 2007-10-15 | Luvata Oy | Metalliseoksen käyttö |
| JP5116976B2 (ja) * | 2006-02-10 | 2013-01-09 | 三菱伸銅株式会社 | 半融合金鋳造用原料黄銅合金 |
| JP2007211325A (ja) * | 2006-02-13 | 2007-08-23 | Sanbo Copper Alloy Co Ltd | 半融合金鋳造用原料アルミニウム青銅合金 |
| JP2007211324A (ja) * | 2006-02-13 | 2007-08-23 | Sanbo Copper Alloy Co Ltd | 半融合金鋳造用原料りん青銅合金 |
| WO2012004841A1 (ja) | 2010-07-05 | 2012-01-12 | Ykk株式会社 | 銅亜鉛合金製品及び銅亜鉛合金製品の製造方法 |
| JP6315868B1 (ja) * | 2017-11-28 | 2018-04-25 | 日酸Tanaka株式会社 | ガス切断火口 |
| PL3872198T3 (pl) * | 2019-06-25 | 2023-05-08 | Mitsubishi Materials Corporation | Automatowy stop miedzi i sposób wytwarzania automatowego stopu miedzi |
| MX2022005128A (es) * | 2019-12-11 | 2022-05-30 | Mitsubishi Materials Corp | Aleacion de cobre de facil corte y metodo para fabricar aleacion de cobre de facil corte. |
-
2000
- 2000-05-17 JP JP2000145460A patent/JP3303878B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN105925921B (zh) | 一种超薄异形铝合金挤压型材生产工艺及产品 | |
| JP2004161992A5 (enExample) | ||
| NO832744L (no) | Fremgangsmaate for produksjon av tiksotrope materialer | |
| CN103203596A (zh) | 一种it业用铝合金型材的生产工艺 | |
| CN111790864B (zh) | 一种提高6系铝合金抗氧化及电击穿性能的锻造方法 | |
| CN106756212A (zh) | 连铸连挤生产析出强化型高强度铜铬合金的方法 | |
| CN107119219B (zh) | 大直径aq80m镁合金棒材热挤压工艺 | |
| CN109513762A (zh) | 一种用于生产宽幅镁板的方法及模具装置 | |
| CN108273973B (zh) | 一种采用水平连铸工艺生产碲青铜棒的方法 | |
| JP2003266519A5 (ja) | ポリエステルフィルムの製造方法 | |
| CN112143943B (zh) | 一种耐热铝合金导线的制备方法 | |
| JPH11172536A5 (enExample) | ||
| CN108677073A (zh) | 一种高强度变形镁合金及其制备方法 | |
| CN109014107A (zh) | 大规格高碳铬轴承钢缩孔缺陷的控制方法 | |
| CN114525461B (zh) | 一种制备细晶kfc带材的方法及细晶kfc带材 | |
| JPS6144149B2 (enExample) | ||
| CN105329887A (zh) | 一种利用晶型诱导在螺杆挤出机中制备石墨烯的方法 | |
| JPH11135848A (ja) | 熱電半導体焼結体の製造方法及び熱電半導体焼結体 | |
| JPH01501917A (ja) | 膨張食品の製造方法 | |
| CN114752745B (zh) | 一种高性能三元铝锆合金导电杆的制备方法 | |
| CN101554636A (zh) | 一种连续柱状晶或单晶组织金属材料无模拉拔成形工艺 | |
| CN104796843A (zh) | 结晶peek膜和振膜的形成方法以及结晶peek振膜 | |
| CN102861775A (zh) | 一种铝型材的成型工艺 | |
| CN103361525B (zh) | 铝合金及其线材 | |
| CN103060613A (zh) | 抗氧化无铅喷金料及其制备方法 |