GB860453A - Improvements in or relating to p-n-junction rectifiers - Google Patents
Improvements in or relating to p-n-junction rectifiersInfo
- Publication number
- GB860453A GB860453A GB3160459A GB3160459A GB860453A GB 860453 A GB860453 A GB 860453A GB 3160459 A GB3160459 A GB 3160459A GB 3160459 A GB3160459 A GB 3160459A GB 860453 A GB860453 A GB 860453A
- Authority
- GB
- United Kingdom
- Prior art keywords
- junction
- sept
- protected
- mica
- lacquer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
860,453. Semi-conductor devices. SIEMENSSCHUCKERTWERKE A.G. Sept. 16, 1959 [Sept. 26, 1958], No. 31604/59. Class 37. The p-n junction of a rectifier is protected from moisture by an insulating lacquer-containing, finely divided fibrous or flaky insulating material. In the device shown, the junction formed by alloying a gold antimony electrode 4 to a p-type silicon body 2 is mounted on a molybdenum plate 1 by an aluminium layer 3 and is protected by a lacquer 5 containing flaky mica. Fibrous asbestos may be used instead of mica. A high vacuum or silicone grease may provide additional protection.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DES60003A DE1078238B (en) | 1958-09-26 | 1958-09-26 | Rectifier arrangement with pn junction and method for its production |
Publications (1)
Publication Number | Publication Date |
---|---|
GB860453A true GB860453A (en) | 1961-02-08 |
Family
ID=7493767
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB3160459A Expired GB860453A (en) | 1958-09-26 | 1959-09-16 | Improvements in or relating to p-n-junction rectifiers |
Country Status (4)
Country | Link |
---|---|
CH (1) | CH373472A (en) |
DE (1) | DE1078238B (en) |
FR (1) | FR1235004A (en) |
GB (1) | GB860453A (en) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE1246886B (en) * | 1960-07-30 | 1967-08-10 | Elektronik M B H | Process for stabilizing and improving the blocking properties of semiconductor components |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
BE562973A (en) * | 1956-12-06 | 1900-01-01 |
-
1958
- 1958-09-26 DE DES60003A patent/DE1078238B/en active Pending
-
1959
- 1959-09-07 FR FR804496A patent/FR1235004A/en not_active Expired
- 1959-09-16 GB GB3160459A patent/GB860453A/en not_active Expired
- 1959-09-18 CH CH7837159A patent/CH373472A/en unknown
Also Published As
Publication number | Publication date |
---|---|
CH373472A (en) | 1963-11-30 |
DE1078238B (en) | 1960-03-24 |
FR1235004A (en) | 1960-07-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB943860A (en) | Semi-conductor device | |
GB783647A (en) | Improvements in or relating to barrier-layer systems | |
GB935459A (en) | A process for use in the production of a semi-conductor device | |
GB970895A (en) | Semi-conductor arrangements enclosed in housings | |
GB860453A (en) | Improvements in or relating to p-n-junction rectifiers | |
GB896717A (en) | Semiconductor diode | |
GB1088637A (en) | Four layer semiconductor switching devices having a shorted emitter | |
GB1037187A (en) | A process for the production of a highly doped p-conducting zone in a semiconductor body | |
GB984141A (en) | Improvements in or relating to methods of alloying to semiconductor bodies | |
GB779195A (en) | Improvements relating to hermetically sealed barrier-layer rectifiers | |
GB926423A (en) | Improvements in or relating to semiconductor rectifiers | |
GB1079309A (en) | Semiconductor rectifiers | |
GB1202342A (en) | Selenium rectifiers | |
GB916379A (en) | Improvements in and relating to semiconductor junction units | |
GB983623A (en) | Improvements relating to semi-conductor devices | |
GB1071208A (en) | An improved semiconductor device suitable for use as a high voltage rectifier | |
GB1266431A (en) | ||
GB851751A (en) | Improvements in and relating to the construction of semi-conductor diodes | |
GB1028715A (en) | Improvements in semi-conductors | |
GB592191A (en) | Improvements in and relating to the electro-forming of rectifiers | |
GB966416A (en) | Improvements in or relating to semiconductors | |
GB910589A (en) | Improvements in semiconductor rectifiers | |
GB889753A (en) | A process for applying an electrode to a semi-conductor body | |
GB1172471A (en) | Semiconductor Rectifier and Semiconductor Rectifier unit based thereon | |
GB890449A (en) | Improvements in or relating to semi-conductor rectifiers |