FR2453915A1 - Procede pour le depot electrolytique de couches d'argent et d'alliages d'argent - Google Patents
Procede pour le depot electrolytique de couches d'argent et d'alliages d'argentInfo
- Publication number
- FR2453915A1 FR2453915A1 FR8008079A FR8008079A FR2453915A1 FR 2453915 A1 FR2453915 A1 FR 2453915A1 FR 8008079 A FR8008079 A FR 8008079A FR 8008079 A FR8008079 A FR 8008079A FR 2453915 A1 FR2453915 A1 FR 2453915A1
- Authority
- FR
- France
- Prior art keywords
- silver
- electrolytic deposition
- layers
- alloys
- salt
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
A.PROCEDE POUR LE DEPOT ELECTROLYTIQUE DE COUCHES D'ARGENT ET D'ALLIAGES D'ARGENT. B.PROCEDE CARACTERISE EN CE QUE L'ELECTROLYTE EST CONSTITUE PAR UNE MASSE DE SEL FONDUE EN FUSION, CONTENANT UN SEL D'ARGENT, UN SULFOCYANURE ALCALIN ET EVENTUELLEMENT UN SEL D'UN OU DE PLUSIEURS METEAUX D'ALLIAGE.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE19792914880 DE2914880A1 (de) | 1979-04-12 | 1979-04-12 | Verfahren zur elektrolytischen abscheidung von silber- und silberlegierungsschichten |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2453915A1 true FR2453915A1 (fr) | 1980-11-07 |
FR2453915B1 FR2453915B1 (fr) | 1984-01-27 |
Family
ID=6068180
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR8008079A Granted FR2453915A1 (fr) | 1979-04-12 | 1980-04-10 | Procede pour le depot electrolytique de couches d'argent et d'alliages d'argent |
Country Status (5)
Country | Link |
---|---|
US (1) | US4274926A (fr) |
JP (1) | JPS55148796A (fr) |
DE (1) | DE2914880A1 (fr) |
FR (1) | FR2453915A1 (fr) |
GB (1) | GB2047275B (fr) |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4752364A (en) * | 1986-05-19 | 1988-06-21 | Delphi Research, Inc. | Method for treating organic waste material and a catalyst/cocatalyst composition useful therefor |
US5318688A (en) * | 1993-03-05 | 1994-06-07 | Texaco Inc. | Method of preparing a membrane |
US6309529B1 (en) | 1998-06-16 | 2001-10-30 | Tanaka Kikinozoku Kogyo K.K. | Method for producing sputtering target material |
JP3436763B2 (ja) * | 1998-06-17 | 2003-08-18 | 田中貴金属工業株式会社 | スパッタリングターゲット材 |
US6875324B2 (en) | 1998-06-17 | 2005-04-05 | Tanaka Kikinzoku Kogyo K.K. | Sputtering target material |
DE10107675B4 (de) * | 2001-02-19 | 2004-11-25 | Implantcast Gmbh | Endoprothese und Verfahren zu ihrer Herstellung |
DE102013215476B3 (de) * | 2013-08-06 | 2015-01-08 | Umicore Galvanotechnik Gmbh | Elektrolyt zur elektrolytischen Abscheidung von Silber-Palladium-Legierungen und Verfahren zu deren Abscheidung |
DE102018126174B3 (de) | 2018-10-22 | 2019-08-29 | Umicore Galvanotechnik Gmbh | Thermisch stabile Silberlegierungsschichten, Verfahren zur Abscheidung und Verwendung |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2267146A1 (fr) * | 1974-04-10 | 1975-11-07 | Stutterheim F Von |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4149942A (en) * | 1974-04-10 | 1979-04-17 | Stutterheim F Von | Process for dissolving metals in fused salt baths |
-
1979
- 1979-04-12 DE DE19792914880 patent/DE2914880A1/de not_active Withdrawn
-
1980
- 1980-03-31 US US06/135,765 patent/US4274926A/en not_active Expired - Lifetime
- 1980-04-08 GB GB8011543A patent/GB2047275B/en not_active Expired
- 1980-04-10 FR FR8008079A patent/FR2453915A1/fr active Granted
- 1980-04-10 JP JP4629880A patent/JPS55148796A/ja active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2267146A1 (fr) * | 1974-04-10 | 1975-11-07 | Stutterheim F Von |
Also Published As
Publication number | Publication date |
---|---|
GB2047275A (en) | 1980-11-26 |
JPS55148796A (en) | 1980-11-19 |
FR2453915B1 (fr) | 1984-01-27 |
GB2047275B (en) | 1983-04-20 |
US4274926A (en) | 1981-06-23 |
DE2914880A1 (de) | 1980-10-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR2525242B1 (fr) | Procede pour le depot electrolytique d'un alliage fe-zn | |
FR2474061B1 (fr) | Anode en cermet pour extraction electrolytique de metaux a partir de sels fondus et cellule d'electrolyse l'incorporant | |
ES8304043A1 (es) | Metodo de obtencion de vidrieras metalizadas semireflectantes. | |
FR2453915A1 (fr) | Procede pour le depot electrolytique de couches d'argent et d'alliages d'argent | |
BE857204A (fr) | Procede pour introduire en continu des additifs dans un recipient contenant un metal en fusion | |
FR2529811B1 (fr) | Fermeture pour un recipient renfermant une masse metallique fondue liquide, notamment fermeture a tiroir pour poche de coulee | |
IT8019097A0 (it) | Lega di palladio e bagni per la sua deposizione senza elettrolisi. | |
IT8123447A0 (it) | Sintesi in sale fuso di polvere di zirconato di metalli alcalino-terrosi. | |
NL184070B (nl) | Waterig bad voor elektrolytische afzetting van zink-nikkellegeringen; alsmede voortbrengselen met een dergelijke afzetting. | |
BE870602A (fr) | Compositions et procede ameliores pour inhiber la formation des conditions et composes explosifs dans les concentres d'argenture pour le depot non electrolytique d'argent | |
FR2317382A1 (fr) | Procede de depot electrolytique d'un alliage de fer, nickel et/ou cobalt | |
ES417246A1 (es) | Un procedimiento para la formacion de un electrodeposito deacero. | |
BE855424A (fr) | Procede et composition pour le depot electrolytique de nickel, cobalt, et alliages de ceux-ci avec le fer | |
FR2402015A1 (fr) | Nouveau procede de revetement electrolytique en argent | |
DE3463528D1 (en) | Process for the deposition of low carat brilliant gold-silver alloy coatings | |
FR2547318B1 (fr) | Composition d'electrolyte et procede pour le depot electrolytique de cuivre | |
GB1243459A (en) | Diffusion coating of metals | |
BE896701A (fr) | Procede et dispositif pour le depot, electrolytique, en continu et a haute densite de courant, d'une couche d'un alliage a base de zinc. | |
FR2290509A1 (fr) | Ensemble d'anodes pour cellule electrolytique et electrolyseur comportant cet ensemble, convenant en particulier pour l'electrolyse des solutions de chlorure de metaux alcalins | |
FR2343062A2 (fr) | Bain d'electrolyse ne contenant pas de cyanure pour le depot electrolytique de l'argent | |
FR2476150B1 (fr) | Anode metallique recouverte d'un revetement pour la production electrolytique de metaux | |
FR2493881B1 (fr) | Compositions et procede pour le depot electrolytique a grande vitesse d'argent brillant, employant un compose de selenium a valence 3 | |
GB1235374A (en) | Improvements relating to the continuous casting of metals | |
Gnezdilov | The Influence of Cathode Current Density on Refined Copper Quality | |
FR2353652A1 (fr) | Procede de depot galvanoplastique a partir d'un electrolyte salin en fusion |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |