FR2448576A1 - Procede pour reduire la teneur en contaminants de masse fondue d'aluminium et d'alliage aluminium - Google Patents
Procede pour reduire la teneur en contaminants de masse fondue d'aluminium et d'alliage aluminiumInfo
- Publication number
- FR2448576A1 FR2448576A1 FR8002359A FR8002359A FR2448576A1 FR 2448576 A1 FR2448576 A1 FR 2448576A1 FR 8002359 A FR8002359 A FR 8002359A FR 8002359 A FR8002359 A FR 8002359A FR 2448576 A1 FR2448576 A1 FR 2448576A1
- Authority
- FR
- France
- Prior art keywords
- aluminum
- reducing
- aluminum alloy
- content
- molten mass
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PROCEDE POUR REDUIRE DANS UNE MASSE FONDUE D'ALUMINIUM OU D'ALLIAGE ALUMINIUM, LA TENEUR EN METAL ALCALIN, EN HYDROGENE GAZEUX ET EN CONTAMINANTS SOLIDES NON METALLIQUES, EN PARTICULIER DES OXYDES. ON INTRODUIT DANS CETTE MASSE FONDUE, ISOLEE DE L'AIR ET MAINTENUE A UNE TEMPERATURE COMPRISE ENTRE670 ET 860C, UN GAZ INERTE SOUS UNE PRESSION INFERIEURE A 2ATMOSPHERES (DE PREFERENCE DE L'AZOTE) CONTENANT UNE POUDRE SUSCEPTIBLE DE LIBERER DU CHLORE. PURIFICATION DES MASSES FONDUES D'ALUMINIUM OU D'ALLIAGE ALUMINIUM.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
HUMA003106 | 1979-02-08 |
Publications (1)
Publication Number | Publication Date |
---|---|
FR2448576A1 true FR2448576A1 (fr) | 1980-09-05 |
Family
ID=10999060
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR8002359A Pending FR2448576A1 (fr) | 1979-02-08 | 1980-02-04 | Procede pour reduire la teneur en contaminants de masse fondue d'aluminium et d'alliage aluminium |
Country Status (16)
Country | Link |
---|---|
JP (1) | JPS55138033A (fr) |
AU (1) | AU5530780A (fr) |
BE (1) | BE881572A (fr) |
BR (1) | BR8000768A (fr) |
CA (1) | CA1144378A (fr) |
CS (1) | CS216519B2 (fr) |
DD (1) | DD149084A5 (fr) |
DE (1) | DE3004120A1 (fr) |
ES (1) | ES488417A0 (fr) |
FR (1) | FR2448576A1 (fr) |
GB (1) | GB2041982A (fr) |
IT (1) | IT1150053B (fr) |
LU (1) | LU82135A1 (fr) |
NL (1) | NL8000567A (fr) |
PL (1) | PL221889A1 (fr) |
RO (1) | RO79075A (fr) |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4832740A (en) * | 1987-03-30 | 1989-05-23 | Swiss Aluminium Ltd. | Process for removing alkali and alkaline earth elements from aluminum melts |
IT1229673B (it) * | 1989-04-20 | 1991-09-06 | Protecme S R L | Dispositivo per la purificazione di metallo fuso, in particolare di alluminio. |
US5769924A (en) * | 1996-08-14 | 1998-06-23 | Eckert; C. Edward | Method of treating aluminum with chlorine produced from chlorocarbon compounds |
AU9354001A (en) * | 2000-09-12 | 2002-03-26 | Alcan Int Ltd | Process and apparatus for adding particulate solid material to molten metal |
CN101984099B (zh) * | 2010-11-24 | 2012-05-09 | 上海电机学院 | 铝熔体在线除气装置 |
CN101984098B (zh) * | 2010-11-24 | 2012-07-04 | 上海电机学院 | 铝熔体在线除气方法 |
CN102560160B (zh) * | 2011-12-29 | 2013-04-24 | 东南大学 | 铝合金真空静置除气熔炼装置 |
CN114015954B (zh) * | 2021-09-08 | 2022-07-01 | 先导薄膜材料有限公司 | 一种降低铝合金中氧含量的方法 |
Citations (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR724553A (fr) * | 1930-12-24 | 1932-04-29 | Alais & Froges & Camarque Cie | Procédé de purification des metaux |
GB603213A (en) * | 1945-07-24 | 1948-06-10 | Foundry Services Ltd | Improvements in or relating to the degassing of metals or metal alloys |
FR1010723A (fr) * | 1948-10-11 | 1952-06-16 | Perfectionnements apportés aux procédés pour éliminer les inclusions solides dans les bains métalliques | |
FR1038557A (fr) * | 1950-02-08 | 1953-09-30 | Affinerie De Juvisy | Procédé et dispositif de traitement de charges fondues par des réactifs, en particulier par des gaz |
DE1533078A1 (de) * | 1966-10-21 | 1969-12-04 | Riedelbauch & Stoffregen Dr | Verfahren zur raucharmen Chlorentgasung von Metallschmelzen |
CH491201A (de) * | 1966-09-02 | 1970-05-31 | Feichtinger Heinrich Ing Dr | Verfahren und Vorrichtung zum Behandeln von Metallschmelzen in Behältern |
DE2206722A1 (de) * | 1972-02-12 | 1973-08-16 | Vaw Ver Aluminium Werke Ag | Verfahren und vorrichtung zum reinigen, insbesondere zum entgasen, von schmelzfluessigem aluminium oder seinen legierungen |
FR2268082A1 (fr) * | 1974-04-16 | 1975-11-14 | Uddeholms Ab | |
FR2305502A1 (fr) * | 1975-03-27 | 1976-10-22 | Air Ind | Procede et installation d'affinage d'un produit metallique, notamment non ferreux |
FR2312570A1 (fr) * | 1975-05-28 | 1976-12-24 | Servimetal | Pastilles composites facilitant l'addition d'elements d'alliages dans l'aluminium et les alliages legers |
FR2370798A1 (fr) * | 1976-11-15 | 1978-06-09 | Vacmetal Gmbh | Procede pour diminuer la teneur en sodium d'un alliage aluminium-magnesium |
-
1980
- 1980-01-28 CS CS80586A patent/CS216519B2/cs unknown
- 1980-01-30 GB GB8003125A patent/GB2041982A/en not_active Withdrawn
- 1980-01-30 NL NL8000567A patent/NL8000567A/nl not_active Application Discontinuation
- 1980-02-04 FR FR8002359A patent/FR2448576A1/fr active Pending
- 1980-02-05 DE DE19803004120 patent/DE3004120A1/de not_active Withdrawn
- 1980-02-05 LU LU82135A patent/LU82135A1/fr unknown
- 1980-02-06 BE BE0/199283A patent/BE881572A/fr unknown
- 1980-02-06 DD DD80218924A patent/DD149084A5/de unknown
- 1980-02-06 RO RO80100105A patent/RO79075A/fr unknown
- 1980-02-07 AU AU55307/80A patent/AU5530780A/en not_active Abandoned
- 1980-02-07 IT IT19745/80A patent/IT1150053B/it active
- 1980-02-07 BR BR8000768A patent/BR8000768A/pt unknown
- 1980-02-07 JP JP1426380A patent/JPS55138033A/ja active Pending
- 1980-02-08 ES ES488417A patent/ES488417A0/es active Granted
- 1980-02-08 CA CA000345308A patent/CA1144378A/fr not_active Expired
- 1980-02-08 PL PL22188980A patent/PL221889A1/xx unknown
Patent Citations (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR724553A (fr) * | 1930-12-24 | 1932-04-29 | Alais & Froges & Camarque Cie | Procédé de purification des metaux |
GB603213A (en) * | 1945-07-24 | 1948-06-10 | Foundry Services Ltd | Improvements in or relating to the degassing of metals or metal alloys |
FR1010723A (fr) * | 1948-10-11 | 1952-06-16 | Perfectionnements apportés aux procédés pour éliminer les inclusions solides dans les bains métalliques | |
FR1038557A (fr) * | 1950-02-08 | 1953-09-30 | Affinerie De Juvisy | Procédé et dispositif de traitement de charges fondues par des réactifs, en particulier par des gaz |
CH491201A (de) * | 1966-09-02 | 1970-05-31 | Feichtinger Heinrich Ing Dr | Verfahren und Vorrichtung zum Behandeln von Metallschmelzen in Behältern |
DE1533078A1 (de) * | 1966-10-21 | 1969-12-04 | Riedelbauch & Stoffregen Dr | Verfahren zur raucharmen Chlorentgasung von Metallschmelzen |
DE2206722A1 (de) * | 1972-02-12 | 1973-08-16 | Vaw Ver Aluminium Werke Ag | Verfahren und vorrichtung zum reinigen, insbesondere zum entgasen, von schmelzfluessigem aluminium oder seinen legierungen |
FR2268082A1 (fr) * | 1974-04-16 | 1975-11-14 | Uddeholms Ab | |
FR2305502A1 (fr) * | 1975-03-27 | 1976-10-22 | Air Ind | Procede et installation d'affinage d'un produit metallique, notamment non ferreux |
FR2312570A1 (fr) * | 1975-05-28 | 1976-12-24 | Servimetal | Pastilles composites facilitant l'addition d'elements d'alliages dans l'aluminium et les alliages legers |
FR2370798A1 (fr) * | 1976-11-15 | 1978-06-09 | Vacmetal Gmbh | Procede pour diminuer la teneur en sodium d'un alliage aluminium-magnesium |
Also Published As
Publication number | Publication date |
---|---|
DE3004120A1 (de) | 1980-08-21 |
BE881572A (fr) | 1980-05-30 |
JPS55138033A (en) | 1980-10-28 |
RO79075A (fr) | 1982-11-30 |
BR8000768A (pt) | 1980-10-21 |
ES8101649A1 (es) | 1980-12-16 |
IT8019745A0 (it) | 1980-02-07 |
DD149084A5 (de) | 1981-06-24 |
IT1150053B (it) | 1986-12-10 |
GB2041982A (en) | 1980-09-17 |
NL8000567A (nl) | 1980-08-12 |
CS216519B2 (en) | 1982-11-26 |
ES488417A0 (es) | 1980-12-16 |
LU82135A1 (fr) | 1980-05-07 |
AU5530780A (en) | 1980-08-14 |
PL221889A1 (fr) | 1980-11-03 |
CA1144378A (fr) | 1983-04-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3958981A (en) | Process for degassing aluminum and aluminum alloys | |
GB1230553A (fr) | ||
FR2448576A1 (fr) | Procede pour reduire la teneur en contaminants de masse fondue d'aluminium et d'alliage aluminium | |
IE832676L (en) | Introducing substances into molten metals | |
FR2364971A1 (fr) | Lance et procede pour l'affinage de l'acier | |
US5972065A (en) | Purification of tantalum by plasma arc melting | |
US3658509A (en) | Process for the metallothermic production of magnesium | |
JPS57146466A (en) | Casting method for titanium casting consisting of pure titanium or alloy consisting essentially of titanium | |
US3975187A (en) | Treatment of carbothermically produced aluminum | |
GB1270126A (en) | Process for the purification of aluminium chloride | |
US3698888A (en) | Metallothermic production of magnesium | |
US3879192A (en) | Electroslag-remelting method | |
US4003738A (en) | Method of purifying aluminum | |
ES468691A1 (es) | Procedimiento para el tratamiento termico de materiales so- lidos de grano fino. | |
JPH0925522A (ja) | 高純度金属材料の製造方法 | |
ES8504952A1 (es) | Procedimiento para evitar interacciones entre un bano de metal y la atmosfera | |
JPS57120629A (en) | Refining method | |
RU2102495C1 (ru) | Металлотермическая реакционная смесь | |
SU1008261A1 (ru) | Способ рафинировани алюминиевых сплавов | |
Beskow | Formation and chemical development of non-metallic inclusions in ladle treatment of steel | |
US2822258A (en) | Method of producing metals from their chlorides | |
SU536240A1 (ru) | Способ рафинировани алюмини и его сплавов | |
SU399548A1 (ru) | ЁПТВАвторыА. Я. Веснин и Н. А. Чуватин | |
JPS57203729A (en) | Regenerating and refining method of copper or copper alloy using powder and granular copper oxide as oxidation-reduction agent | |
SU340309A1 (ru) | Способ электроннолучевого переплава сталей и сплавов |