FR2391014A1 - Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires - Google Patents
Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulairesInfo
- Publication number
- FR2391014A1 FR2391014A1 FR7715830A FR7715830A FR2391014A1 FR 2391014 A1 FR2391014 A1 FR 2391014A1 FR 7715830 A FR7715830 A FR 7715830A FR 7715830 A FR7715830 A FR 7715830A FR 2391014 A1 FR2391014 A1 FR 2391014A1
- Authority
- FR
- France
- Prior art keywords
- ingot mold
- continuous casting
- liquid metal
- metal bars
- casting process
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Procédé de coulée continue de barres métalliques à section droite non circulaire et plus particulièrement carrée ou sensiblement carrée, telles que billettes, blooms, destinées à la fabrications de produits longs. Ce procédé comprend une mise en mouvement du métal liquide en lingotière au moyen d'un champ magnétique tournant autour de son axe. Il se caractérise en de qu'on alimente la lingotière par un jet de coulée dont le point d'impact sur la surface libre du metal liquide en lingotière est localisé au voisinage d'un coin de la lingotière, et de préférence sur une diagonale sensiblement à mi-distance entre la paroi de la lingotière et le centre de la surface. La mise en oeuvre de l'invention favorise le rassemblement des crasses au centre de la surface libre du métal liquide en lingotière où elles pourront être aisément pêchées comme cela se pratique de façon habituelle en coulée continue centrifuge de produits ronds.
Priority Applications (9)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7715830A FR2391014A1 (fr) | 1977-05-18 | 1977-05-18 | Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires |
GB17656/78A GB1582501A (en) | 1977-05-18 | 1978-05-04 | Electromagnetic centrifugal continuous casting of square or near-square metal bars |
IT23088/78A IT1095878B (it) | 1977-05-18 | 1978-05-05 | Procedimento di colata continua centrifuga elettro-magnetica di barre metalliche a sezione non circolare |
DE19782820334 DE2820334A1 (de) | 1977-05-18 | 1978-05-10 | Verfahren und vorrichtung zum kontinuierlichen giessen von einen rechteckigen querschnitt aufweisendem halbzeug |
AT0340578A AT375572B (de) | 1977-05-18 | 1978-05-11 | Verfahren zum kontinuierlichen giessen von einen rechteckigen querschnitt aufweisendem halbzeug |
BE1008877A BE866997A (fr) | 1977-05-18 | 1978-05-12 | Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires |
US05/905,868 US4205715A (en) | 1977-05-18 | 1978-05-15 | Method of continuous centrifugally casting of metal strands of non-circular cross-section |
JP53057710A JPS6011582B2 (ja) | 1977-05-18 | 1978-05-17 | 非円形金属棒の電磁的連続遠心鋳造方法 |
LU79675A LU79675A1 (fr) | 1977-05-18 | 1978-05-18 | Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7715830A FR2391014A1 (fr) | 1977-05-18 | 1977-05-18 | Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2391014A1 true FR2391014A1 (fr) | 1978-12-15 |
FR2391014B1 FR2391014B1 (fr) | 1980-03-07 |
Family
ID=9191209
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7715830A Granted FR2391014A1 (fr) | 1977-05-18 | 1977-05-18 | Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires |
Country Status (9)
Country | Link |
---|---|
US (1) | US4205715A (fr) |
JP (1) | JPS6011582B2 (fr) |
AT (1) | AT375572B (fr) |
BE (1) | BE866997A (fr) |
DE (1) | DE2820334A1 (fr) |
FR (1) | FR2391014A1 (fr) |
GB (1) | GB1582501A (fr) |
IT (1) | IT1095878B (fr) |
LU (1) | LU79675A1 (fr) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2521886A3 (fr) * | 1982-02-22 | 1983-08-26 | Siderurgie Fse Inst Rech | Procede et dispositif pour mettre en rotation en lingotiere un metal en fusion coule en continu |
EP0201069A1 (fr) * | 1985-05-10 | 1986-11-12 | Erik A. Olsson | Procédé de coulée continue de produits métalliques |
Family Cites Families (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR851871A (fr) * | 1938-03-22 | 1940-01-16 | Ind De L Aluminium Sa | Procédé pour la coulée de pièces allongées en métal, en particulier en métal léger |
US2548696A (en) * | 1947-10-20 | 1951-04-10 | Dow Chemical Co | Spark-gap liquid level indicator |
AT200270B (de) * | 1955-01-15 | 1958-10-25 | Boehler & Co Ag Geb | Verfahren und Vorrichtung zur Bewegung der Schmelze im Strang von Stranggießanlagen |
DE1803473A1 (de) * | 1968-10-17 | 1970-05-21 | Demag Ag | Verfahren und Einrichtung zum Metall-,insbesondere Stahl-Stranggiessen |
SU383521A1 (ru) * | 1970-06-08 | 1973-05-23 | Авторы изобретени витель | Промежуточная емкость |
FR2118867B1 (fr) * | 1970-12-24 | 1974-02-15 | Etudes De Centrifugation | |
US3702630A (en) * | 1971-01-05 | 1972-11-14 | Centrifugation Soc Civ De | Apparatus for casting solid cylindrical metallic objects |
US3952791A (en) * | 1974-01-08 | 1976-04-27 | Nippon Steel Corporation | Method of continuous casting using linear magnetic field for core agitation |
SU440203A1 (ru) * | 1973-04-25 | 1974-08-25 | С. И. Петренко, Г. Гизатулин, Н. И. Голомазов, В. Н. Ирха, Н. И. Семенченко , В. А. Губа | УСТРОЙСТВО ДЛЯ НЕПРЕРЫВНОГО ЛИТЬЯ МЕТАЛЛИЧЕСКИХ ЗАГОТОВОКВ Г-и -1- Г- ; S 5 Ьиа?;'г ^-т-гр' VD^-J..;;, ^; ,. :.'-/>&' |
FR2315344A1 (fr) * | 1975-06-27 | 1977-01-21 | Siderurgie Fse Inst Rech | Lingotiere de coulee continue electrorotative |
-
1977
- 1977-05-18 FR FR7715830A patent/FR2391014A1/fr active Granted
-
1978
- 1978-05-04 GB GB17656/78A patent/GB1582501A/en not_active Expired
- 1978-05-05 IT IT23088/78A patent/IT1095878B/it active
- 1978-05-10 DE DE19782820334 patent/DE2820334A1/de active Granted
- 1978-05-11 AT AT0340578A patent/AT375572B/de not_active IP Right Cessation
- 1978-05-12 BE BE1008877A patent/BE866997A/fr not_active IP Right Cessation
- 1978-05-15 US US05/905,868 patent/US4205715A/en not_active Expired - Lifetime
- 1978-05-17 JP JP53057710A patent/JPS6011582B2/ja not_active Expired
- 1978-05-18 LU LU79675A patent/LU79675A1/fr unknown
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2521886A3 (fr) * | 1982-02-22 | 1983-08-26 | Siderurgie Fse Inst Rech | Procede et dispositif pour mettre en rotation en lingotiere un metal en fusion coule en continu |
EP0201069A1 (fr) * | 1985-05-10 | 1986-11-12 | Erik A. Olsson | Procédé de coulée continue de produits métalliques |
Also Published As
Publication number | Publication date |
---|---|
LU79675A1 (fr) | 1979-02-02 |
AT375572B (de) | 1984-08-27 |
JPS53142923A (en) | 1978-12-13 |
DE2820334A1 (de) | 1978-11-30 |
US4205715A (en) | 1980-06-03 |
DE2820334C2 (fr) | 1987-09-10 |
BE866997A (fr) | 1978-11-13 |
FR2391014B1 (fr) | 1980-03-07 |
JPS6011582B2 (ja) | 1985-03-27 |
IT7823088A0 (it) | 1978-05-05 |
IT1095878B (it) | 1985-08-17 |
GB1582501A (en) | 1981-01-07 |
ATA340578A (de) | 1984-01-15 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR2374113A1 (fr) | Procede pour la coulee continue horizontale, en particulier d'acier, et dispositif pour la mise en oeuvre de ce procede | |
AU2002222478B2 (en) | Treating molten metals by moving electric arc | |
AU2002222478A1 (en) | Treating molten metals by moving electric arc | |
FR2391015A1 (fr) | Perfectionnement au procede de coulee continue centrifuge de produits metalliques et dispositif de mise en oeuvre | |
FR2391014A1 (fr) | Procede de coulee continue centrifuge electromagnetique de barres metalliques non circulaires | |
FR2414969A1 (fr) | Procede de coulee continue de metaux, notamment d'acier, dispositif pour la mise en oeuvre et ebauche metallique creuse obtenue par ce procede | |
KR100417393B1 (ko) | 실제제품형상에근접하도록연속주조하는방법및장치 | |
GB1433173A (en) | Pouring pipe for pouring steel into a continuous casting mould | |
GB2046151A (en) | Method of Reducing Segregation in The Continuous Casting of Steel | |
SU1119769A1 (ru) | Устройство дл непрерывного горизонтального лить стали | |
JPH01150450A (ja) | 流し込みストランドの非凝固部分の取扱い方法及び装置 | |
AU2008200261B2 (en) | Treating molten metals by moving electric arc | |
SU1371762A1 (ru) | Способ обработки металла легирующими элементами при непрерывном литье заготовок | |
GB2144659A (en) | Horizontal continuous casting of round billets | |
US4777999A (en) | Use of magnetic field in continuous casting | |
JPH0569092A (ja) | 連続鋳造方法 | |
RU2112626C1 (ru) | Способ непрерывного литья заготовок | |
RU122052U1 (ru) | Кристаллизатор горизонтальной машины непрерывного литья заготовок из цветных металлов и сплавов | |
SU1138232A1 (ru) | Способ горизонтального непрерывного лить заготовок и машина дл его осуществлени | |
SU954155A1 (ru) | Способ непрерывного горизонтального лить чугунных трубных заготовок | |
SU1690944A1 (ru) | Способ непрерывной разливки металла | |
SU1140885A2 (ru) | Кузнечный слиток | |
RU2043838C1 (ru) | Механизм качания кристаллизатора | |
Rantanen | The Outokumpu Way for Continuous Rod | |
Li et al. | Factors Affecting the Quality of High-Speed Steel Produced by ESR |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
CL | Concession to grant licences | ||
ST | Notification of lapse |