ES8104387A3 - Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico - Google Patents

Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico

Info

Publication number
ES8104387A3
ES8104387A3 ES494042A ES494042A ES8104387A3 ES 8104387 A3 ES8104387 A3 ES 8104387A3 ES 494042 A ES494042 A ES 494042A ES 494042 A ES494042 A ES 494042A ES 8104387 A3 ES8104387 A3 ES 8104387A3
Authority
ES
Spain
Prior art keywords
corrosión
procedure
reduce
translation
machine
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
ES494042A
Other languages
English (en)
Other versions
ES494042A0 (es
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chemed Corp
Original Assignee
Chemed Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chemed Corp filed Critical Chemed Corp
Priority to ES494042A priority Critical patent/ES494042A0/es
Publication of ES8104387A3 publication Critical patent/ES8104387A3/es
Publication of ES494042A0 publication Critical patent/ES494042A0/es
Granted legal-status Critical Current

Abstract

PROCEDIMIENTO PARA REDUCIR LA CORROSION DE SUPERFICIES METALICAS EN UN CALENTADOR DE AIRE DE UN HORNO DE COMBUSTIBLES FOSILES. EL PROCEDIMIENTO CONSISTE EN INYECTAR UN ADITIVO EN LA CORRIENTE GASEOSA DE CHIMENEA, EN DONDE LA CORRIENTE TIENE UNA TEMPERATURA DE 1533 A 1199 K, APROXIMADAMENTE, A UNA VELOCIDAD DE 0,025-5 KG. DE ADITIVO POR TONELADA DE CARBON QUEMADO. CON ELLO SE PRETENDE REDUCIR LA CONCENTRACION DE TRIOXIDO DE AZUFRE LIBRE EN EL GAS DE LA CHIMENEA, LO QUE A SU VEZ REDUCE EL PUNTO DE ROCIO DE ACIDO SULFURICO Y, POR TANTO, LA CORROSION. A
ES494042A 1980-08-06 1980-08-06 Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico Granted ES494042A0 (es)

Priority Applications (1)

Application Number Priority Date Filing Date Title
ES494042A ES494042A0 (es) 1980-08-06 1980-08-06 Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
ES494042A ES494042A0 (es) 1980-08-06 1980-08-06 Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico

Publications (2)

Publication Number Publication Date
ES8104387A3 true ES8104387A3 (es) 1981-04-01
ES494042A0 ES494042A0 (es) 1981-04-01

Family

ID=8480929

Family Applications (1)

Application Number Title Priority Date Filing Date
ES494042A Granted ES494042A0 (es) 1980-08-06 1980-08-06 Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico

Country Status (1)

Country Link
ES (1) ES494042A0 (es)

Also Published As

Publication number Publication date
ES494042A0 (es) 1981-04-01

Similar Documents

Publication Publication Date Title
SE8206786D0 (sv) Reaktor for jerntillverkning
FR2389574A1 (es)
ES486524A1 (es) Procedimiento para convertir particulas contaminantes, emi- tidas en procesos quimicos o fisicos, en substancias inofen-sivas
GB1057577A (en) Melting furnace for the production of steel and method of operating the furnace
BG60231B2 (en) Process for removing sulphur compounds, in particular sulphur dioxide, from flue gasses
ATE123816T1 (de) Verfahren zur unterdrückung von staub und rauch bei der elektrostahlherstellung.
GB2011051A (en) Combustion process with reduced nitrogen oxides exhaust.
ES8104387A3 (es) Procedimiento para reducir la corrosion de superficies meta-licas en un calentador de aire de un horno de combustible fosil industrial o electrotermico
MX168393B (es) Procedimiento para la fusion de chatarra esponja de hierro y hierro crudo, crudo solido o similares.
SE8306722D0 (sv) Sett att reglera ett forbrenningsforlopp
JPS5798638A (en) Smelting method for metal sulfide mineral
JPS5435813A (en) Controlling method for carbon content of reduced pellets
JPS52105901A (en) Process for moisture conditioning of coke discharged from oven and app aratus for it
KR860006555A (ko) 저융점 금속의 첨가방법
JPS5377896A (en) Converter slag treating method
JPS5538975A (en) Recarburizer for iron manufacture and steel making
JPS5389877A (en) Controlling method for thermal decomposition furnace for solid waste
ATE89323T1 (de) Verschleisslanze.
JPS5266873A (en) Process for treating combustion gas
JPS5244767A (en) Method of treating exhaust gas containing acidic components
JPS5324302A (en) Manufacture of coke
JPS52147513A (en) Smelting method of low nitrogen steel at steel making arc furnace
ES454305A1 (es) Procedimiento para controlar los gases de escape en un con- vertidor con insuflacion de oxigeno.
JPS5624492A (en) Conversion of mined coal to anthracitic coal by adding compound of quartzite and fluorite
JPS5439391A (en) Method of regenerating high temperature gas refining catalyst