ES392619A1 - Procedimiento de tratamientos de superficies metalicas paramejorar su resistencia al desgaste y al gripado. - Google Patents
Procedimiento de tratamientos de superficies metalicas paramejorar su resistencia al desgaste y al gripado.Info
- Publication number
- ES392619A1 ES392619A1 ES392619A ES392619A ES392619A1 ES 392619 A1 ES392619 A1 ES 392619A1 ES 392619 A ES392619 A ES 392619A ES 392619 A ES392619 A ES 392619A ES 392619 A1 ES392619 A1 ES 392619A1
- Authority
- ES
- Spain
- Prior art keywords
- mixture
- metal surface
- treatment
- temperature
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D9/00—Electrolytic coating other than with metals
- C25D9/04—Electrolytic coating other than with metals with inorganic materials
- C25D9/06—Electrolytic coating other than with metals with inorganic materials by anodic processes
Landscapes
- Chemical & Material Sciences (AREA)
- Metallurgy (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- Materials Engineering (AREA)
- Inorganic Chemistry (AREA)
- Organic Chemistry (AREA)
- Electroplating Methods And Accessories (AREA)
- Heat Treatment Of Articles (AREA)
- Lubricants (AREA)
- Chemical Treatment Of Metals (AREA)
- Electroplating And Plating Baths Therefor (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7023726A FR2092874B1 (es) | 1970-06-26 | 1970-06-26 | |
FR7103716A FR2124083B2 (es) | 1970-06-26 | 1971-02-04 |
Publications (1)
Publication Number | Publication Date |
---|---|
ES392619A1 true ES392619A1 (es) | 1973-08-16 |
Family
ID=26215818
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES392619A Expired ES392619A1 (es) | 1970-06-26 | 1971-06-25 | Procedimiento de tratamientos de superficies metalicas paramejorar su resistencia al desgaste y al gripado. |
Country Status (10)
Country | Link |
---|---|
US (1) | US3753875A (es) |
BE (1) | BE768350A (es) |
CA (1) | CA957640A (es) |
CH (1) | CH527913A (es) |
CS (1) | CS180574B2 (es) |
DE (1) | DE2131152C3 (es) |
ES (1) | ES392619A1 (es) |
FR (2) | FR2092874B1 (es) |
GB (1) | GB1338791A (es) |
NL (1) | NL7108562A (es) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4452675A (en) * | 1982-10-18 | 1984-06-05 | Allied Corporation | Process for the activation of nickel electrodes via the electrochemical deposition of selenium and/or tellurium |
-
1970
- 1970-06-26 FR FR7023726A patent/FR2092874B1/fr not_active Expired
-
1971
- 1971-02-04 FR FR7103716A patent/FR2124083B2/fr not_active Expired
- 1971-06-09 US US00151478A patent/US3753875A/en not_active Expired - Lifetime
- 1971-06-10 BE BE768350A patent/BE768350A/xx unknown
- 1971-06-22 NL NL7108562A patent/NL7108562A/xx not_active Application Discontinuation
- 1971-06-23 DE DE2131152A patent/DE2131152C3/de not_active Expired
- 1971-06-24 GB GB2969271A patent/GB1338791A/en not_active Expired
- 1971-06-25 CA CA116,732A patent/CA957640A/en not_active Expired
- 1971-06-25 CS CS7100004727A patent/CS180574B2/cs unknown
- 1971-06-25 CH CH936771A patent/CH527913A/fr not_active IP Right Cessation
- 1971-06-25 ES ES392619A patent/ES392619A1/es not_active Expired
Also Published As
Publication number | Publication date |
---|---|
DE2131152C3 (de) | 1980-08-21 |
FR2092874A1 (es) | 1972-01-28 |
DE2131152A1 (de) | 1971-12-30 |
FR2124083A2 (es) | 1972-09-22 |
US3753875A (en) | 1973-08-21 |
FR2124083B2 (es) | 1975-06-06 |
DE2131152B2 (de) | 1979-12-20 |
CH527913A (fr) | 1972-09-15 |
CS180574B2 (en) | 1978-01-31 |
BE768350A (fr) | 1971-11-03 |
CA957640A (en) | 1974-11-12 |
FR2092874B1 (es) | 1973-10-19 |
NL7108562A (es) | 1971-12-28 |
GB1338791A (en) | 1973-11-28 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CS185634B2 (en) | Manufacturing of wear resistance layer on portions of bearings or tools exposed to working strain | |
ES334192A1 (es) | Un metodo de mejorar el flujo de agua y soluciones acuosas a traves de un estrato arcilloso. | |
ES377176A1 (es) | Un procedimiento para tratar termicamente un material ferroso endurecible por transicion. | |
ES354966A1 (es) | Un metodo para dotar a los metales de resistencia electricayno a la corrosion. | |
CS222205B2 (en) | Method of making the metal e.g. aluminium in the electrolyser | |
ES392619A1 (es) | Procedimiento de tratamientos de superficies metalicas paramejorar su resistencia al desgaste y al gripado. | |
ES324020A1 (es) | Procedimiento para la formacion de revestimientos protectores sobre una superficie que contiene cinc. | |
FR2189539A1 (en) | Aluminium as a refractory material - roughened by etching by mechanical abrasion or by electrolysis | |
IT966580B (it) | Processo di cromatura elettrolitica in particolare per la formazione di superfici di usura | |
Koizumi et al. | Pitting corrosion of titanium in high temperature halide solutions | |
SU450685A1 (ru) | Электролит дл электрохимической обработки | |
SICK | EROSION RESISTANCE OF COPPER MATERIALS WITH RESPECT TO RUNNING WATER | |
GB2115444B (en) | Fused salt bath composition | |
FR2126273A1 (en) | Electrolytic treatment for colouring anodized aluminium - - using direct and alternating current | |
ES391620A1 (es) | Un metodo para producir electroliticamente cobre catodico. | |
JPS5669340A (en) | Surface treating material for heat exchanger | |
ES343121A1 (es) | Procedimiento de tratamiento superficial de piezas metali- cas. | |
ES372263A1 (es) | Procedimiento de tratamiento superficial de superficies fe-rrosas para mejorar sus cualidades de frotamiento y de re- sistencia al desgaste. | |
JPS5384240A (en) | Processing method of heat coolecting surface | |
SU543662A1 (ru) | Способ обработки бурового раствора | |
GB1103414A (en) | Methods for determining the susceptibility of a metal to metal attack by a corrosiveelectrolyte | |
GB489800A (en) | Improvements in processes for producing protective coatings on metals of the iron group and their alloys | |
GB1184418A (en) | Treatment of Titanium and Titanium Alloys in a Cyanide Bath | |
Patrina | Use of Aluminizing in Electric Furnace Construction | |
ES406982A2 (es) | Procedimiento para el tenido electrolitico de objetos de aluminio o de una aleacion de aluminio. |