CS260371B1 - SpOeob odetránenia izolačního laku z vodičov - Google Patents

SpOeob odetránenia izolačního laku z vodičov Download PDF

Info

Publication number
CS260371B1
CS260371B1 CS873461A CS346187A CS260371B1 CS 260371 B1 CS260371 B1 CS 260371B1 CS 873461 A CS873461 A CS 873461A CS 346187 A CS346187 A CS 346187A CS 260371 B1 CS260371 B1 CS 260371B1
Authority
CS
Czechoslovakia
Prior art keywords
conductors
removal
spoeob
insulating varnish
temperature
Prior art date
Application number
CS873461A
Other languages
English (en)
Slovak (sk)
Other versions
CS346187A1 (en
Inventor
Karol Czifrik
Julius Borka
Original Assignee
Karol Czifrik
Julius Borka
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Karol Czifrik, Julius Borka filed Critical Karol Czifrik
Priority to CS873461A priority Critical patent/CS260371B1/cs
Publication of CS346187A1 publication Critical patent/CS346187A1/cs
Publication of CS260371B1 publication Critical patent/CS260371B1/cs

Description

Vynález sa týká spósobu odstránenía izolačného laku z vodičov, například vývodov cievok, vinutí transformátorov.
Doteraz známe spósoby odstránenia izolačného laku:
Mechanické odstránenie ostrým nástrojom je prácne, vodiče sú mechanicky namáhané, často poškodené. Při opalovaní laku v plameni tenké vodiče zhoria, odlakovanie přípravkami na báze organických rozpúšťadiel je náročné na dokonalé striekanie rozmáčeného laku. Uvedené nevýhody odstraňuje vynález, ktorého podstata spočívá v tom, že sa příslušná časť vodiča uvedie do kontaktu s chloridom zirtočnatým v teplote 300 až 500 °C a po rozklade laku sa povrch vodiča opláchne vodou. Výhodou odtzolovania chloridom zinočnatým, je, že prebehne dokonale behem 3 až 20 sekúnd podlá priemeru vodiča a druhu laku v uvedenom teplotnom rozsahu, přitom nezhoršuje mechanické vlastnosti médi. Metóda je vhodná pre súčasné odizolovanie vodičov s róznym priemerom a druhom laku, aj s priemerom menším ako 0,15 mm. Odsmaltovaná časť po opláchnutí vodou je kovovo čistá, kvalitně sa dá pocínovat
Skúšky boli převedené tým spósobom, že sme chlorid zinočnatý roztavili v sklenenej kadičke na rýchlovariči a do taveniny sme ponořili vývody tlmiviek v dlžke 20 až 30 milimetrov. Potřebná doba ponoru je v tabulke. Po rozložení laku sme vývody oplachovali vo vodě 3 až 5 sekúnd.
TABULKA
Priemer vodiča v mm Cas ponoru v sekundách Teplota taveniny v °C 350 400 450 0,1 7 4 3 0,2 8 6 3 0,3 10 až 12 6 až 7 4 až 5 0,5 15 až 17 8 až 10 5 až 6 0,8 25 až 30 15 až 20 8 až 10

Claims (1)

  1. PREDMET VYNALEZU Spósob odstránenia izolačného laku z vo- s chloridom zinočnatým o teplote 300 až dičov najmá měděných, vyznačený tým, Že 500 °C a po rozklade laku sa povrch vodiča sa příslušná časť vodiča uvedie do kontaktu opláchne vodou.
CS873461A 1987-05-14 1987-05-14 SpOeob odetránenia izolačního laku z vodičov CS260371B1 (sk)