CN2510734Y - 不同厚度拱桥式耐磨刚玉陶瓷内衬弯头 - Google Patents

不同厚度拱桥式耐磨刚玉陶瓷内衬弯头 Download PDF

Info

Publication number
CN2510734Y
CN2510734Y CN 01274194 CN01274194U CN2510734Y CN 2510734 Y CN2510734 Y CN 2510734Y CN 01274194 CN01274194 CN 01274194 CN 01274194 U CN01274194 U CN 01274194U CN 2510734 Y CN2510734 Y CN 2510734Y
Authority
CN
China
Prior art keywords
elbow
corundum ceramic
thickness
ceramic piece
corundum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 01274194
Other languages
English (en)
Inventor
吴亦安
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WU YI'AN
Original Assignee
WU YI'AN
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WU YI'AN filed Critical WU YI'AN
Priority to CN 01274194 priority Critical patent/CN2510734Y/zh
Application granted granted Critical
Publication of CN2510734Y publication Critical patent/CN2510734Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种火力发电厂锅炉燃烧器前输煤粉管路弯头。本实用新型不同厚度拱桥式耐磨刚玉陶瓷内衬弯头,包括在外壳基材(3)内壁上贴有多块刚玉陶瓷块,多块刚玉陶瓷块紧密排列组成弯头内衬体(2),内衬体的刚玉陶瓷块在弯头外径处(1)的厚度大于弯头内径处(6)的厚度,刚玉陶瓷块厚度的排列从弯头外径处向弯头内径处以圆弧连接,多块刚玉陶瓷块内壁围成的弯头内衬体内径(5)相同。本实用新型具有耐磨损、耐腐蚀和耐高温的特点,其使用寿命比现有的输煤粉管路延长数倍。

Description

不同厚度拱桥式耐磨刚玉陶瓷内衬弯头
技术领域:
本实用新型涉及一种火力发电厂锅炉燃烧器前输煤粉管路弯曲部件。
背景技术:
燃煤电厂使用的锅炉大多数为煤粉炉,都需配备将块煤碾磨成煤粉的制粉系统。煤粉通过输煤粉管路进入到煤粉炉中燃烧发电,特别是煤粉进入锅炉燃烧器筒体前,由于煤粉以一定的速度进入燃烧器内,输煤粉管路内壁不断受到煤粉的冲击被磨损和腐蚀,且承受一定的温度。尤其是在燃烧器筒体前输煤粉管路弯头部位,受煤粉高速离心力的作用,弯头磨损率高出直管部位数倍,输煤粉管路容易损坏。现有的输煤粉管路弯头有的采用增加管路内壁合金材料厚度、有的采用耐磨合金材料或采用内衬陶瓷片以延长输煤粉管路使用寿命,但成本较高,效果不尽理想。
发明内容:
本实用新型提供一种不同厚度拱桥式耐磨刚玉陶瓷内衬弯头,该内衬弯头具有防磨、防腐、耐高温的特点,与现有技术相比,可延长弯头的使用寿命数倍,进而延长输煤粉管路的使用寿命。
本实用新型是这样实现的:一种不同厚度拱桥式耐磨刚玉陶瓷内衬弯头,包括在外壳基材内壁上贴有多块刚玉陶瓷块,其特征是多块刚玉陶瓷块紧密排列组成弯头内衬体,内衬体的刚玉陶瓷块在弯头外径处的厚度大于弯头内径处的厚度,刚玉陶瓷块厚度的排列从弯头外径处向弯头内径处以圆弧连接,多块刚玉陶瓷块内壁围成的弯头内衬体内径相同。
本实用新型的工作原理是在燃烧器筒体前输煤粉管路弯头内壁铺上一层刚玉陶瓷,刚玉陶瓷在弯头外径处的厚度大于弯头内径处的厚度,但多块刚玉陶瓷块内壁围成的弯头内衬体内径相同,由于弯头内衬体外径处受煤粉离心力冲击磨损程度较弯头内衬体内径处受煤粉冲击磨损程度大,弯头外径处厚实的刚玉陶瓷层耐磨损能力强,因此可大大提高弯头的使用寿命,且节约刚玉陶瓷,减轻弯头重量,延长输煤粉管路的使用寿命。
附图说明:
图1为本实用新型不同厚度拱桥式耐磨刚玉陶瓷内衬弯头结构示意图,图2为图1的侧视示意图。
图中:1.弯头外径处刚玉陶瓷块,2.内衬体,3.外壳基材,4.高温无机胶,5.内衬体内径,6.弯头内径处刚玉陶瓷块。
实施例说明:
参见图1、图2,一种不同厚度拱桥式耐磨刚玉陶瓷内衬弯头,包括在外壳基材3内壁上贴有多块刚玉陶瓷块,多块刚玉陶瓷块紧密排列组成弯头内衬体2,内衬体2的刚玉陶瓷块在弯头外径处1的厚度大于弯头内径处6的厚度,刚玉陶瓷块厚度的排列从弯头外径处1向弯头内径处6以圆弧连接,多块刚玉陶瓷块内壁围成的弯头内衬体内径5相同。在刚玉陶瓷块和外壳基材3间、刚玉陶瓷块和刚玉陶瓷块间的缝隙涂有高温无机胶4,经过热处理后达到外壳3和刚玉陶瓷块、刚玉陶瓷块之间紧贴的结果。在本实施例中,外壳基材3一般为碳钢材料,刚玉陶瓷1、6可采用95号刚玉陶瓷材料。
本实用新型实施时可根据用户要求的输煤粉管路内径φ大小,即内衬体内径,和选用的刚玉陶瓷在弯头外径处的最大厚度和弯头内径处的最小厚度,推算出弯头外壳基材的直径和刚玉陶瓷厚度,按照输煤粉管路外壳基材的形状尺寸,制作刚玉陶瓷块。
本实用新型可应用于发电厂锅炉燃烧器筒体前的输煤粉管路弯头,也可应用于其他需耐磨损、耐腐蚀和耐高温的部件和管路。

Claims (1)

1.一种不同厚度拱桥式耐磨刚玉陶瓷内衬弯头,包括在外壳基材(3)内壁上贴有多块刚玉陶瓷块,其特征是多块刚玉陶瓷块紧密排列组成弯头内衬体(2),内衬体(2)的刚玉陶瓷块在弯头外径处(1)的厚度大于弯头内径处(6)的厚度,刚玉陶瓷块厚度的排列从弯头外径处(1)向弯头内径处(6)以圆弧连接,多块刚玉陶瓷块内壁围成的弯头内衬体内径(5)相同。
CN 01274194 2001-12-13 2001-12-13 不同厚度拱桥式耐磨刚玉陶瓷内衬弯头 Expired - Fee Related CN2510734Y (zh)