CN2348997Y - 带水冷装置的挤出模具 - Google Patents
带水冷装置的挤出模具 Download PDFInfo
- Publication number
- CN2348997Y CN2348997Y CN 98226900 CN98226900U CN2348997Y CN 2348997 Y CN2348997 Y CN 2348997Y CN 98226900 CN98226900 CN 98226900 CN 98226900 U CN98226900 U CN 98226900U CN 2348997 Y CN2348997 Y CN 2348997Y
- Authority
- CN
- China
- Prior art keywords
- holes
- hole
- water cooling
- cooling device
- section
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型带水冷装置的挤出模具,有分流段,压缩段、成型段,在成型段距模具型腔10—30mm处设水冷装置,即开有若干个孔(B),孔B方向与型腔方向相反,位于产品出口两侧,孔径5—12mm,孔的间距1.5—10mm,孔的深度为15—80mm,在孔(B)的垂直方向上开有若干个孔(A),与孔(B)相通。优点:水冷装置能确保冷水直接通入模具内,使物料速冷,加大型腔内阻力保证产品完全定型,提高挤出速度,操作灵活效果好。
Description
本实用新型提出的是一种有水冷控制装置的挤出模具--带水冷装置的挤出模具。
现有的挤出模具,包括有分流段、压缩段、成型段,产品的冷却、定型通常在水箱内完成,因此,对产品冷却无法进行控制,造成产品的形状和尺寸不能保证。以至产品很难定型,更不能确保正常生产,尤其对宽度较大平板和形状复杂的型材,更难成型。
本实用新型的目的在于克服上述存在的缺陷,在塑料挤出成型模具的成型段上设置一个可控水冷装置,即通过打孔形成一个冷却区域,把冷却水直接通入模具内,使得物料在模具内能够得到快速冷却,从而加大模具型腔内阻力,保证产品的形状和尺寸,使产品完全定型,提高产品的挤出速度。
本实用新型的技术解决方案:
包括有分流段1,紧靠分流段1之后的有压缩段2、成型段3,其特征是在模具成型段3距模具型腔10-30mm处设水冷装置,即开有若干个孔(B),该孔(B)的方向与型腔方向相反,孔(B)的位置在产品出口的两侧,孔(B)的孔径在5-12mm,每个孔(B)的间距1.5-10mm,孔(B)的深度为15-80mm,在孔(B)的垂直方向上开有若干个孔(A),它与孔(B)是相通的。
本实用新型的优点:1、水冷装置能确保冷水直接通入模具内,使物料速冷,2、加大模具型腔的内阻力,保证产品形状、尺寸完全定型,3、提高产品的挤出速度,4、设计简单合理、操作灵活、效果好。
附图是本实用新型的实施例结构示意图
图中的5是速冷区,6是缓冷区,
下面结合实施例(附图)进一步描述本实用新型的工作过程和技术方案:
当胶状塑料溶体由挤出机挤入模具接头4,进入分流段1、压缩段2和进入成型段3时,因平板两边阻力明显大于中间阻力,使得中间出料明显快于两边,造成平板很难定型,如果让其进入水箱冷却,既不能保证产品形状和尺寸,同样也不能使其定型。本实用新型是在成型段型腔出口距型腔两边18mm处,打两排水孔,每排18个孔(B),孔(B)中心距为9mm,孔径为6mm,深度为50mm,同时在垂直于孔(B)方向型腔出口30mm处,由中间向两边打9个孔(A),孔(A)中心为两个孔(B)中心,两孔(A)中心距为18mm,深度与孔(B)接通即可,孔径为8mm。当冷却水由孔(A)进入模具,然后由两个孔B流出时,冷却水便吸收了产品热量,加快了中间冷却,增加了阻力,使得中间出料和两边出料同步,产品得以定型,同时,可调节孔(A)在孔(B)中的不同位置,即改变缓冷区和速冷区的区域大小,其定型效果可以根据需要进行调节。本实用新型设计简单合理,操作灵活,便于控制。
Claims (1)
1、带水冷装置的挤出模具,包括有分流段(1),紧靠分流段(1)之后有压缩段(2)、成型段(3),其特征是在模具成型段(3)距模具型腔10-30mm处设水冷装置,即开有若干个孔(B),该孔(B)的方向与型腔方向相反,孔(B)的位置在产品出口的两侧,孔(B)的孔径在5-12mm,每个孔(B)的间距1.5-10mm,孔(B)的深度为15-80mm,在孔(B)的垂直方向上开有若干个孔(A),它与孔(B)是相通的。