CN219851683U - 一种可避免工件在接刀口产生毛刺的顺送模具 - Google Patents
一种可避免工件在接刀口产生毛刺的顺送模具 Download PDFInfo
- Publication number
- CN219851683U CN219851683U CN202321250497.3U CN202321250497U CN219851683U CN 219851683 U CN219851683 U CN 219851683U CN 202321250497 U CN202321250497 U CN 202321250497U CN 219851683 U CN219851683 U CN 219851683U
- Authority
- CN
- China
- Prior art keywords
- edge
- knife
- burr
- produce
- work piece
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型公开了一种可避免接刀口产生毛刺的顺送模具,涉及板材冲压加工领域,包括上模和下模,在下模的后端设有切断用接刀口,用于顺送模具上的最后的切断工序。在所述接刀口的每一侧都设有两个向外的豁口,使得接刀口的宽度大于工件宽度;所述豁口左右对称,豁口的半径为2‑4毫米。本顺送模具的有益效果在于:所设计的接刀口应用于顺送模具中,可以有效地抵消因接刀不齐导致毛刺的产生,减少了二次打磨毛刺的工序,提高了生产效率,降低了成本。
Description
技术领域
本实用新型涉及板材冲压加工领域,具体是一种可避免工件在接刀口产生毛刺的顺送模具。
背景技术
金属板材顺送冲压加工时,在最后一步切断时,往往因为送料误差和带料直线度的原因,导致接刀口与实际切断位置产生微小位移,造成一侧材料单薄冲切强度不够;另一侧材料多余,冲裁后在单侧或者双侧产生毛刺。此时就需要二次打磨去掉毛刺,增加成本,降低加工效率。
实用新型内容
本实用新型的目的是提供一种可避免工件在接刀口产生毛刺的顺送模具,以解决上述背景技术中提到的问题。
为了实现上述目的,采用的技术方案是:
一种可避免接刀口产生毛刺的顺送模具,包括上模和下模,在下模的接刀口处每一侧都设有两个向外的豁口,使得接刀口的宽度略大于工件宽度。
优选地,所述豁口的半径为2-4毫米。
本实用新型的有益效果在于:本实用新型设计的接刀口应用于顺送模具中,可以有效地抵消因接刀不齐导致毛刺的产生,减少了二次打磨毛刺的工序,提高了生产效率,降低了成本。
附图说明
图1为本实用新型的下模排样示意图;
图2为本实用新型在改进前的接刀口处局部放大图;
图3为本实用新型在改进后的接刀口处局部放大图;
图4为加工后产品的示意图,图中A处为容易出毛刺的部位。
图中,1.接刀口处的豁口,2.工件。
具体实施方式
下面将结合实施例和附图对本实用新型做进一步解释和说明。
实施例:请参阅图1-4,一种可避免接刀口产生毛刺的顺送模具,用于板材冲压操作,包括上模和下模,在下模的后部设有接刀口,用于顺送冲压加工最后的切断工序。在所述接刀口的每一侧都设有两个向外的豁口1,使得接刀口的宽度大于工件2的宽度;所述豁口1左右对称,豁口的半径为4毫米。
以上所述,仅为本实用新型较佳的具体实施方式,但本实用新型的保护范围并不局限于此,任何熟悉本技术领域的技术人员在本实用新型披露的技术范围内,根据本实用新型的技术方案及其实用新型构思加以等同替换或改变,都应涵盖在本实用新型的保护范围之内。
Claims (2)
1.一种可避免工件在接刀口产生毛刺的顺送模具,包括上模和下模,其特征在于:在下模的接刀口处每一侧都设有两个向外的豁口,使得接刀口的宽度大于工件宽度。
2.根据权利要求1所述的顺送模具,其特征在于:所述豁口的半径为2-4毫米。