CN210617641U - 一种耐光照耐老化uv转印膜 - Google Patents
一种耐光照耐老化uv转印膜 Download PDFInfo
- Publication number
- CN210617641U CN210617641U CN201920917999.4U CN201920917999U CN210617641U CN 210617641 U CN210617641 U CN 210617641U CN 201920917999 U CN201920917999 U CN 201920917999U CN 210617641 U CN210617641 U CN 210617641U
- Authority
- CN
- China
- Prior art keywords
- layer
- resistant
- printing
- illumination
- wood grain
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型公开了一种耐光照耐老化UV转印膜,包括PET膜层、离型层、印刷层和胶粘层,所述离型层和印刷层之间增设有UV保护层,所述印刷层由第一木纹层、第二木纹层、第一底色层、第二底色层和第三底色层顺序涂覆而成,所述第一木纹层到第二木纹层的油墨深浅度逐渐加深,所述第一底色层、第二底色层和第三底色层的油墨深浅度逐渐加深。本实用新型将印刷层多层叠加设计,而且从表层至里层着色深浅度逐渐加色布置,使木纹纹路具有层次感,形象逼真,能有效提升产品附加值,最重要的是多层印刷层能有效阻隔光照透过性,再加上UV保护层的保护,有效提升耐光照、耐老化、热稳定性好、收缩率小等优点,从而延长产品使用寿命。
Description
技术领域
本实用新型涉及热转印技术领域,更具体地说是一种耐光照耐老化UV转印膜。
背景技术
热转印是将图案预先印刷到耐温薄膜上,通过加热、加压将薄膜上的精美图案转印到产品上的印刷工艺,该工艺印刷方式包括热转印膜的印制和热转印加工两大部分。
热转印膜一般由四层构成,分别是基底层、离型层、印刷层、胶粘层。
基底层:即离型层、印刷层、胶粘层的载体——热转印基膜,热转印基膜包括pet膜、opp膜、pvc膜等,需要根据具体产品的需要进行选择对应的基膜,否则会影响转印膜产品质量。
离型层:是一层离型剂的涂层,在常温下保持固体状态,在一定的温度下可熔化,与基底层的粘结力变小,能很快从基膜脱离,无粘连剩余物。
印刷层:该层是热转印制品图案体现美感的根本所在,其关键在于热转印油墨的选择与搭配,热转印工艺完成后,就只剩印刷层附着在热转印产品表面,所以印刷层材料的选择尤为重要,稍不注意就会影响转印膜产品质量。
胶粘层:其实际成分就是一种热熔胶。根据不同的承印物,选择对应的热转印胶水。
基底层是通过离型层剥离掉的,印刷层通过胶粘层粘附到承印物上,比如pvc及ps发泡板的转印、地板的转印、踢脚线的转印、密度板和型材的转印、pvc扣板的转印、铝合金的转印、建材行业如木塑门、钢木门以及生态门的转印等上,印刷层直接显露在外,受外界环境光照、温度、适度等影响,印刷层不耐光照,容易老化,产品寿命较短。
实用新型内容
本实用新型的目的在于克服现有技术以上缺陷,提供一种耐光照、耐老化、热稳定性好、收缩率小、寿命长,而且能有效提升产品附加值的耐光照耐老化UV转印膜。
为了达到以上目的,本实用新型是通过以下技术方案实现的:一种耐光照耐老化UV转印膜,包括PET膜层,所述PET膜层下表面上顺序涂覆有离型层、印刷层和胶粘层,其特征在于,所述离型层和印刷层之间增设有UV保护层,所述印刷层由第一木纹层、第二木纹层、第一底色层、第二底色层和第三底色层顺序涂覆而成,所述UV保护层涂覆在第一木纹层的上表面上,所述第一木纹层到第二木纹层的油墨深浅度逐渐加深,所述第一底色层、第二底色层和第三底色层的油墨深浅度逐渐加深。
作为优选,胶粘层由热熔胶构成,所述热熔胶涂覆在第三底色层的下表面上。
作为优选,离型层由硅油构成,所述硅油涂覆在PET膜层的下表面上。
作为上述方案的替换方案,离型层由离型剂构成,所述离型剂涂覆在PET膜层的下表面上。
作为优选,PET膜层由PET哑光膜构成。
作为上述方案的替换方案,PET膜层由PET亮光膜构成。
有益效果:本实用新型将印刷层多层叠加设计,而且从表层至里层着色深浅度逐渐加色布置,使木纹纹路具有层次感,形象逼真,能有效提升产品附加值,最重要的是多层印刷层能有效阻隔光照透过性,再加上UV保护层的保护,有效提升耐光照、耐老化、热稳定性好、收缩率小等优点,从而延长产品使用寿命。
附图说明
图1为本实用新型的结构示意图。
图中:1-PET膜层,2-离型层,3-UV保护层,4-第一木纹层,5-第二木纹层,6-第一底色层,7-第二底色层,8-第三底色层,9-胶粘层。
具体实施方式
为了使本实用新型的技术手段、创作特征与达成目的易于明白理解,以下结合具体实施例进一步阐述本实用新型。
实施例1:如图1所示,一种耐光照耐老化UV转印膜,包括PET膜层1,PET膜层1由PET哑光膜构成。
PET膜层1下表面上顺序涂覆有离型层2、印刷层和胶粘层9,离型层2和印刷层之间增设有UV保护层3。胶粘层9由热熔胶构成,热熔胶涂覆在第三底色层的下表面上。离型层2由硅油构成,硅油涂覆在PET膜层的下表面上。
印刷层由第一木纹层4、第二木纹层5、第一底色层6、第二底色层7和第三底色层8顺序涂覆而成,UV保护层3涂覆在第一木纹层4的上表面上,第一木纹层4到第二木纹层5的油墨深浅度逐渐加深,第一底色层6、第二底色层7和第三底色层8的油墨深浅度逐渐加深。
实施例2:离型层2由离型剂构成,离型剂涂覆在PET膜层的下表面上。
其余同实施例1。
实施例3:PET膜层1由PET亮光膜构成。
其余同实施例2。
使用:本实用新型将印刷层多层叠加设计,而且从表层至里层着色深浅度逐渐加色布置,使木纹纹路具有层次感,形象逼真,能有效提升产品附加值,最重要的是多层印刷层能有效阻隔光照透过性,再加上UV保护层的保护,有效提升耐光照、耐老化、热稳定性好、收缩率小等优点,从而延长产品使用寿命。
Claims (6)
1.一种耐光照耐老化UV转印膜,包括PET膜层,所述PET膜层下表面上顺序涂覆有离型层、印刷层和胶粘层,其特征在于,所述离型层和印刷层之间增设有UV保护层,所述印刷层由第一木纹层、第二木纹层、第一底色层、第二底色层和第三底色层顺序涂覆而成,所述UV保护层涂覆在第一木纹层的上表面上,所述第一木纹层到第二木纹层的油墨深浅度逐渐加深,所述第一底色层、第二底色层和第三底色层的油墨深浅度逐渐加深。
2.根据权利要求1所述的耐光照耐老化UV转印膜,其特征在于,胶粘层由热熔胶构成,所述热熔胶涂覆在第三底色层的下表面上。
3.根据权利要求1或2所述的耐光照耐老化UV转印膜,其特征在于,离型层由硅油构成,所述硅油涂覆在PET膜层的下表面上。
4.根据权利要求1或2所述的耐光照耐老化UV转印膜,其特征在于,离型层由离型剂构成,所述离型剂涂覆在PET膜层的下表面上。
5.根据权利要求1或2所述的耐光照耐老化UV转印膜,其特征在于,PET膜层由PET哑光膜构成。
6.根据权利要求1或2所述的耐光照耐老化UV转印膜,其特征在于,PET膜层由PET亮光膜构成。