CN208452036U - 防咬胶免刮胶活络模 - Google Patents
防咬胶免刮胶活络模 Download PDFInfo
- Publication number
- CN208452036U CN208452036U CN201821085919.5U CN201821085919U CN208452036U CN 208452036 U CN208452036 U CN 208452036U CN 201821085919 U CN201821085919 U CN 201821085919U CN 208452036 U CN208452036 U CN 208452036U
- Authority
- CN
- China
- Prior art keywords
- rubber
- runner
- excessive glue
- glue groove
- epipleural
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种防咬胶免刮胶活络模,在花纹块上与上侧板贴合的面上开设溢胶槽,并在上侧板上开设流道,流道连通硫化腔与溢胶槽,当硫化腔内的橡胶受热膨胀后,多余的橡胶通过流道进入溢胶槽内,待脱模后,溢胶槽内多余的橡胶固化成橡胶圈,流道内剩余的橡胶固化形成连接环,连接环的厚度较小,与实心胎的接触面积较小,拉扯橡胶圈就能将连接环从实心胎上拉扯下来,避免了使用道具刮伤实心胎,保证了轮胎的质量,轮胎的制造精度较高,活络模具的硫化效率较高。
Description
技术领域
本实用新型涉及车轮制造,尤其是车轮制造模具技术领域,本实用新型提供一种防咬胶免刮胶活络模。
背景技术
随着工业车辆和其它各种特殊用途车辆对轮胎性能要求的不断提高,传统的充气轮胎在某些场合已不能满足使用要求。橡胶实心轮胎的出现,在某些方面可以满足特殊条件对轮胎的特殊要求。用于硫化成型各类轮胎的模具包括活络模具,由花纹圈、模套和上下侧板组成。活络模具在硫化时,花纹圈、模套和上下侧板合模后组成硫化腔,向硫化腔内注入橡胶,橡胶胚胎在加热后膨胀,多余的橡胶会进入花纹块与侧板之间的间隙内,硫化成型后,加工出的轮胎会出现咬胶的现象,需使用刀具将咬胶刮除,由于咬胶呈絮状,在刮除时容易刮伤轮胎,破坏轮胎质量,轮胎的制造精度较低,活络模具的硫化效率较低。
实用新型内容
本实用新型要解决的技术问题是:为了克服现有技术中活络模具硫化成型后,加工出的轮胎会出现咬胶的现象,需使用刀具将咬胶刮除,在刮除时容易刮伤轮胎,破坏轮胎质量,轮胎的制造精度较低,活络模具的硫化效率较低的问题,提供一种防咬胶免刮胶活络模。
本实用新型解决其技术问题所采用的技术方案是:一种防咬胶免刮胶活络模,包括花纹块和上侧板,所述花纹块上与上侧板贴合的面上开设有溢胶槽,所述上侧板上开设有流道,所述流道连通硫化腔与溢胶槽。
本实用新型的防咬胶免刮胶活络模,在花纹块上与上侧板贴合的面上开设溢胶槽,并在上侧板上开设流道,流道连通硫化腔与溢胶槽,当硫化腔内的橡胶受热膨胀后,多余的橡胶通过流道进入溢胶槽内,待脱模后,溢胶槽内多余的橡胶固化成橡胶圈,流道内剩余的橡胶固化形成连接环,连接环的厚度较小,与实心胎的接触面积较小,拉扯橡胶圈就能将连接环从实心胎上拉扯下来,避免了使用道具刮伤实心胎,保证了轮胎的质量,轮胎的制造精度较高,活络模具的硫化效率较高。
为了便于脱模和简化流道的加工步骤,所述溢胶槽的横截面形状为直角梯形,直角梯形的底面与上侧板贴合,上侧板与花纹块贴合的边上设有圆角,圆角与直角梯形的锐角面之间形成的间隙为流道。
本实用新型的有益效果是:本实用新型的防咬胶免刮胶活络模,在花纹块上与上侧板贴合的面上开设溢胶槽,并在上侧板上开设流道,流道连通硫化腔与溢胶槽,当硫化腔内的橡胶受热膨胀后,多余的橡胶通过流道进入溢胶槽内,待脱模后,溢胶槽内多余的橡胶固化成橡胶圈,流道内剩余的橡胶固化形成连接环,连接环的厚度较小,与实心胎的接触面积较小,拉扯橡胶圈就能将连接环从实心胎上拉扯下来,避免了使用道具刮伤实心胎,保证了轮胎的质量,轮胎的制造精度较高,活络模具的硫化效率较高。
附图说明
下面结合附图和实施例对本实用新型进一步说明。
图1是本实用新型的二维示意图;
图2是本实用新型图1中A处的放大图。
图中:1.花纹块,2.上侧板,3.溢胶槽,4.流道。
具体实施方式
现在结合附图对本实用新型做进一步详细的说明。这些附图均为简化的示意图,仅以示意方式说明本实用新型的基本结构,因此其仅显示与本实用新型有关的构成。
如图1所示的一种防咬胶免刮胶活络模,包括花纹块1和上侧板2,所述花纹块1上与上侧板2贴合的面上开设有溢胶槽3,所述上侧板2上开设有流道4,所述流道4连通硫化腔与溢胶槽3。
为了便于脱模和简化流道4的加工步骤,所述溢胶槽3的横截面形状为直角梯形,直角梯形的底面与上侧板2贴合,上侧板2与花纹块1贴合的边上设有圆角,如图2所示,圆角与直角梯形的锐角面之间形成的间隙为流道4。
本实用新型的防咬胶免刮胶活络模,在花纹块1上与上侧板2贴合的面上开设溢胶槽3,并在上侧板2上开设流道4,流道4连通硫化腔与溢胶槽3,当硫化腔内的橡胶受热膨胀后,多余的橡胶通过流道4进入溢胶槽3内,待脱模后,溢胶槽3内多余的橡胶固化成橡胶圈,流道4内剩余的橡胶固化形成连接环,连接环的厚度较小,与实心胎的接触面积较小,拉扯橡胶圈就能将连接环从实心胎上拉扯下来,避免了使用道具刮伤实心胎,保证了轮胎的质量,轮胎的制造精度较高,活络模具的硫化效率较高。
以上述依据本实用新型的理想实施例为启示,通过上述的说明内容,相关工作人员完全可以在不偏离本项实用新型技术思想的范围内,进行多样的变更以及修改。本项实用新型的技术性范围并不局限于说明书上的内容,必须要根据权利要求范围来确定其技术性范围。
Claims (2)
1.一种防咬胶免刮胶活络模,其特征在于:包括花纹块(1)和上侧板(2),所述花纹块(1)上与上侧板(2)贴合的面上开设有溢胶槽(3),所述上侧板(2)上开设有流道(4),所述流道(4)连通硫化腔与溢胶槽(3)。
2.如权利要求1所述的防咬胶免刮胶活络模,其特征在于:所述溢胶槽(3)的横截面形状为直角梯形,直角梯形的底面与上侧板(2)贴合,上侧板(2)与花纹块(1)贴合的边上设有圆角,圆角与直角梯形的锐角面之间形成的间隙为流道(4)。