CN206287623U - 抗划伤彩涂卷 - Google Patents
抗划伤彩涂卷 Download PDFInfo
- Publication number
- CN206287623U CN206287623U CN201621011888.XU CN201621011888U CN206287623U CN 206287623 U CN206287623 U CN 206287623U CN 201621011888 U CN201621011888 U CN 201621011888U CN 206287623 U CN206287623 U CN 206287623U
- Authority
- CN
- China
- Prior art keywords
- coating
- scratch resistance
- prepainted coil
- chemical treatment
- substrate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种抗划伤彩涂卷,包括基板,其特征是:所述基板上表面依次涂覆有第一化学处理层、底漆、聚碳酸酯涂层、抗划伤涂层和自清洁涂层;所述基板的下表面依次涂覆有第二化学处理层和背漆;所述聚碳酸酯涂层为混合有晶须硅的改性涂层;所述抗划伤涂层由聚硅氧烷、环氧改性聚氨酯丙烯酸酯和齐聚体构成。本实用新型提供了一种抗划伤性能极好的彩涂卷,延长彩涂卷的使用寿命。
Description
技术领域
本实用新型涉及一种抗划伤彩涂卷。
背景技术
通常彩涂卷会在表面做防腐蚀的涂层和油漆涂层,这样简单处理的彩涂卷具有一定的防蚀性,但是由于其无法抵抗外接的割划,很容易出现表面被刮花的情况,十分不美观,而且导致使用寿命大大降低;再者彩涂卷用于各个行业,表面始终需要接触空气,难免会积灰,需要自清洁涂层对其进行不定期清理,保持其表面清洁,同时也在一定程度上保护了彩涂卷,延长其使用寿命。
实用新型内容
针对现有技术的不足,本实用新型提供了一种抗划伤彩涂卷。
为实现上述目的,本实用新型提供了如下技术方案:包括基板,其特征是:所述基板上表面依次涂覆有第一化学处理层、底漆、聚碳酸酯涂层、抗划伤涂层和自清洁涂层;所述基板的下表面依次涂覆有第二化学处理层和背漆;所述聚碳酸酯涂层为混合有晶须硅的改性涂层;所述抗划伤涂层由聚硅氧烷、环氧改性聚氨酯丙烯酸酯和齐聚体构成。
通过上述技术方案,聚碳酸酯无臭、无味、五毒、刚硬而有韧性,具有突出的抗冲击能力和尺寸稳定性等特点,综合性能优异,其通过混合晶须硅进行改性,使聚碳酸酯涂层具有更好的耐候性,以及改善抗划性能;聚硅氧烷含有润滑剂成分,降低表面张力,减小摩擦系数,环氧改性聚氨酯丙烯酸酯增加涂层的附着力以及增强涂层的硬度、抗划伤性和耐磨性,齐聚体用于改善聚氨酯丙烯酸酯的结晶规整度,提高微相分离效果,提升聚氨酯丙烯酸酯的综合性能,保证抗划伤涂层起到抗划伤的效果;自清洁涂层,借助自然力量使钢板具有自清洁功能,提高彩涂卷的使用寿命。
优选的,所述基板为镀铝板,所述第一化学处理层和第二化学处理层均为镀锌钝化层。
通过上述技术方案,镀铝板环保健康,对人体无害,镀锌钝化层,能够抵抗大气腐蚀。
优选的,所述底漆和背漆均为丙烯酸/环氧树脂底漆层或者金属防腐底漆层。
通过上述技术方案,丙烯酸/环氧树脂底漆或者金属防腐底漆层进一步起到防腐保护作用,提高钢板的防腐性能。
优选的,所述自清洁涂层为纳米材料。
通过上述技术方案,自清洁涂层使钢板保持清洁状态,利用自然界的光照,室内室外均可以进行自清洁,纳米材料不断分解积聚在表面的有机物,使灰尘无法附着在其表面从而达到清洁的目的。
附图说明
图1为本实用新型抗划伤彩涂卷的示意图。
附图标记:1、基板;2、第一化学处理层;3、底漆;4、聚碳酸酯涂层;5、抗划伤涂层;6、自清洁涂层;7、第二化学处理层;8、背漆。
具体实施方式
通过图1对本实用新型抗划伤彩涂卷作进一步的说明。
本实用新型的抗划伤彩涂卷包括基板1,其特征是:所述基板1上表面依次涂覆有第一化学处理层2、底漆3、聚碳酸酯涂层4、抗划伤涂层5和自清洁涂层6;所述基板1的下表面依次涂覆有第二化学处理层7和背漆8;所述聚碳酸酯涂层5为混合有晶须硅的改性涂层,本实用新型采用晶须硅的质量分数为5%以提高聚碳酸酯的硬度,使其具有更好的综合性能;所述抗划伤涂层的成分由聚硅氧烷、环氧改性聚氨酯丙烯酸酯和齐聚体构成,所述聚硅氧烷也可采用聚二甲基铵盐改性物代替,齐聚体为聚氨酯用齐聚体。
优选的,所述基板1为镀铝板,所述第一化学处理层和第二化学处理层均为镀锌钝化层。
优选的,所述底漆3和背漆9均为丙烯酸/环氧树脂底漆或者金属防腐底漆层,丙烯酸/环氧树脂以环氧树脂,改性环氧树脂为主要成膜物质,具有很好的附着力和化学耐腐蚀性,金属底漆为以中分子环氧树脂、特种树脂、铁红、防锈颜料、助剂和溶剂等组成的乙组分和胺固化剂的双组份自干涂料,铁红及锌粉的保护作用使涂膜具有十分突出的防锈性能;具有漆膜硬度高;耐高温;干燥性能好;高附着力,良好的机械性能等优点。
优选的,所述自清洁涂层7为纳米材料,其厚度小于4μm。
本实用新型的抗划伤彩涂卷可用于多种领域,自动清洁,自动愈合裂痕,抗腐蚀性能也大大提高,从而大幅度提高钢板的使用寿命。
以上所述仅是本实用新型的优选实施方式,本实用新型的保护范围并不仅局限于上述实施例,凡属于本实用新型思路下的技术方案均属于本实用新型的保护范围。应当指出,对于本技术领域的普通技术人员来说,在不脱离本实用新型原理前提下的若干改进和润饰,这些改进和润饰也应视为本实用新型的保护范围。
Claims (2)
1.一种抗划伤彩涂卷,包括基板,其特征是:所述基板上表面依次涂覆有第一化学处理层、底漆、聚碳酸酯涂层、抗划伤涂层和自清洁涂层;所述基板的下表面依次涂覆有第二化学处理层和背漆;所述抗划伤涂层由聚硅氧烷、环氧改性聚氨酯丙烯酸酯和齐聚体构成,所述底漆和背漆均为丙烯酸/环氧树脂底漆层或者金属防腐底漆层,所述自清洁涂层为纳米材料。
2.根据权利要求1所述的抗划伤彩涂卷,其特征是:所述基板为镀铝板,所述第一化学处理层和第二化学处理层均为镀锌钝化层。