CN205710891U - 冲压用耐磨纳米涂层结构 - Google Patents
冲压用耐磨纳米涂层结构 Download PDFInfo
- Publication number
- CN205710891U CN205710891U CN201620270386.2U CN201620270386U CN205710891U CN 205710891 U CN205710891 U CN 205710891U CN 201620270386 U CN201620270386 U CN 201620270386U CN 205710891 U CN205710891 U CN 205710891U
- Authority
- CN
- China
- Prior art keywords
- layer
- coating structure
- basic unit
- punching press
- transition zone
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种冲压用耐磨纳米涂层结构,包括基层,在所述的基层上设有过渡层,在所述的过渡层上设有耐磨层,所述的基层为NGr层,所述的过渡层为NGrS2Mo层,所述的耐磨层为NS2Mo层。采用了上述涂层结构之后,通过在冲头以及模具的冲压部喷涂涂层结构,能够在实际使用过程中,增加模具的耐磨性能,提高模具的使用寿命,提高产品的生产质量。
Description
技术领域
本实用新型涉及纳米涂层技术行业,尤其是涉及一种冲压用耐磨纳米涂层结构。
背景技术
纳米涂层是利用现有技术,根据所要求的性能,添加适当的纳米材料,并对涂层工艺作相应的调整,纳米涂层的制作方法主要包括气相沉积、各类喷涂(含常温喷涂、火焰喷涂和等离子喷涂等)、镀覆(含电镀和化学镀)等多种方法。在现有技术中,为了使用高精度化、自动化、多功能化、高生产率化、环保等要求,要求特殊工件具有耐高温、耐磨损、耐腐蚀等特点,而纳米涂层就具有上述优点,纳米涂层的使用将越来越广泛。
在冲压技术行业中,冲压机的上下冲击会对模具造成摩擦损伤,从而导致模具以及冲头的寿命降低,并且会出现不合格产品,造成生产质量下降。
发明内容
本实用新型所要解决的技术问题是提供一种能够提高模具的耐磨性能且提高模具的使用寿命提高生产质量的冲压用耐磨纳米涂层结构。
本实用新型解决其技术问题所采用的技术方案是:一种冲压用耐磨纳米涂层结构,包括基层,在所述的基层上设有过渡层,在所述的过渡层上设有耐磨层,所述的基层为NGr层,所述的过渡层为NGrS2Mo层,所述的耐磨层为NS2Mo层。
进一步具体的,所述的基层的厚度为0.2μm,所述的过渡层的厚度为0.5μm,所述的耐磨层的厚度为2μm,通过对涂层厚度的控制,能够很好的实现耐磨效果。
进一步具体的,所述的耐磨层上设有NGr层、NGrS2Mo层以及NS2Mo层的一种或者两种或者三种,根据需要进行涂层的排布。
本实用新型的有益效果是:采用了上述涂层结构之后,通过在冲头以及模具的冲压部喷涂涂层结构,能够在实际使用过程中,增加模具的耐磨性能,提高模具的使用寿命,提高产品的生产质量。
附图说明
图1是本实用新型的结构示意图。
图中:1、NGr层;2、NGrS2Mo层;3、NS2Mo层。
具体实施方式
下面结合附图对本实用新型作详细的描述。
如图1所示一种冲压用耐磨纳米涂层结构,包括基层,在所述的基层上设有过渡层,在所述的过渡层上设有耐磨层,所述的基层为NGr层1其厚度为0.2μm,所述的过渡层为NGrS2Mo层2其厚度为0.5μm,所述的耐磨层为NS2Mo层3其厚度为2μm;所述的耐磨层上设有NGr层1、NGrS2Mo层2以及NS2Mo层3的一种或者两种或者三种,可以根据需要在耐磨层上继续喷涂NGr层1、NGrS2Mo层2以及NS2Mo层3其中的一种或者几种。
加工的时候,首先将连接件置于真空室内,保证室内温度为400~450℃以及室内压强为2Pa,保证室内偏压为100V以及弧电流为80A,喷涂时间8分钟形成NGr层1;继续保证室内温度为400~450℃,室内压强保证在1.5Pa,室内偏压为100V,弧电流为120A,喷涂时间10分钟形成NGrS2Mo层2;继续保证室内温度为400~450℃,室内压强稳定在1.5Pa,室内偏压升至150V维稳,弧电流升至150A维稳,喷涂时间100分钟形成NS2Mo层3。
通过在冲头以及模具的冲压部喷涂涂层结构,能够在实际使用过程中,增加模具的耐磨性能,提高模具的使用寿命,提高产品的生产质量。
需要强调的是:以上仅是本实用新型的较佳实施例而已,并非对本实用新型作任何形式上的限制,凡是依据本实用新型的技术实质对以上实施例所作的任何简单修改、等同变化与修饰,均仍属于本实用新型技术方案的范围内。
Claims (3)
1.一种冲压用耐磨纳米涂层结构,包括基层,其特征在于,在所述的基层上设有过渡层,在所述的过渡层上设有耐磨层,所述的基层为NGr层(1),所述的过渡层为NGrS2Mo层(2),所述的耐磨层为NS2Mo层(3)。
2.根据权利要求1所述的冲压用耐磨纳米涂层结构,其特征在于,所述的基层的厚度为0.2μm,所述的过渡层的厚度为0.5μm,所述的耐磨层的厚度为2μm。
3.根据权利要求1所述的冲压用耐磨纳米涂层结构,其特征在于,所述的耐磨层上设有NGr层(1)、NGrS2Mo层(2)以及NS2Mo层(3)的一种或者两种或者三种。