CN205688008U - A kind of coating clamp of 3D mobile phone faceplate - Google Patents
A kind of coating clamp of 3D mobile phone faceplate Download PDFInfo
- Publication number
- CN205688008U CN205688008U CN201620541493.4U CN201620541493U CN205688008U CN 205688008 U CN205688008 U CN 205688008U CN 201620541493 U CN201620541493 U CN 201620541493U CN 205688008 U CN205688008 U CN 205688008U
- Authority
- CN
- China
- Prior art keywords
- support body
- mobile phone
- face
- coating clamp
- pole
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
This utility model provides the coating clamp of a kind of 3D mobile phone faceplate, belongs to field of mechanical technique.It solve existing substrate frame not easy heat radiation, need the long period could the technical problem such as cooling.This coating clamp includes support body, support body includes end face and bottom surface, there is between end face and bottom surface some sides, the groove that can place 3D mobile phone faceplate is all offered on each side, support body be fixedly arranged in the middle of pole, the upper end of pole passes from the end face of support body, and the bottom of pole passes from the bottom surface of support body, offering air vent on support body, air vent runs through the end face of support body and the bottom surface of support body.This utility model rapid heat dissipation, can cool down in the short period of time.
Description
Technical field
This utility model belongs to field of mechanical technique, relates to the coating clamp of a kind of 3D mobile phone faceplate.
Background technology
Control sputter coating refers to, under vacuum conditions, by voltage and the common effect in magnetic field, with the indifferent gas being ionized
Body ion pair target bombards, and causes target to be ejected and be deposited on substrate formation with the form of ion, atom or molecule
Thin film, magnetron sputtering coater technology is widely used in the plated film of auto mirror, mobile phone faceplate, inner and outer decorative parts of automobile.Authorize
Notification number is that the Chinese patent literature of CN 204982037U discloses a kind of rotary coater, this coater include vacuum (-tight) housing,
Thermal resistance evaporation source, controlled sputtering source, plasma source, work rest and the internal vacuum holding keeping vacuum state of vacuum (-tight) housing can be made
Putting, controlled sputtering source and plasma source are each attached on the inwall of vacuum (-tight) housing, and work rest is arranged in vacuum (-tight) housing, and work rest has
Base, base is fixed on the bottom of vacuum (-tight) housing, and thermal resistance evaporation source is fixed on base, and base rotation is provided with gear one, gear
Rotate on one and be provided with rotating shaft one, rotating shaft one is fixed with gear two, base be circular and be provided with on the lateral surface of base with
The gear teeth that gear two is meshed.
In above-mentioned coater, workpiece is placed in the groove two of substrate frame, substrate frame by being placed on work rest,
The weak point of substrate frame is: be not provided with radiator structure in substrate frame, after taking out in coater, and the temperature of substrate frame
Spend higher, need to wait that the long period can cool down, cause substrate inconvenience of taking.
Summary of the invention
The problems referred to above that this utility model exists for existing technology, it is provided that the coating clamp of a kind of 3D mobile phone faceplate,
Technical problem to be solved in the utility model is: how to improve the rate of cooling of coating clamp.
The purpose of this utility model can be realized by following technical proposal:
A kind of coating clamp of 3D mobile phone faceplate, described coating clamp includes that support body, described support body include end face and bottom surface,
There is between described end face and bottom surface some sides, each side all offers the groove that can place 3D mobile phone faceplate, described
Support body be fixedly arranged in the middle of pole, the upper end of described pole passes from the end face of described support body, the bottom of described pole from
The bottom surface of described support body passes, it is characterised in that offer air vent on described support body, and described air vent runs through the end face of support body
Bottom surface with support body.
Operation principle of the present utility model is: 3D mobile phone faceplate is placed in groove, and the middle part of the support body of coating clamp is solid
Surely having pole, can be placed on by support body on the work rest one of rotation by this support when plated film, work rest one is positioned at plated film
In machine, after plated film completes, support body is taken off from work rest one, be placed on the work rest two of outside, the support body of coating clamp
On offer air vent, outside air flows through the air vent on support body, it is possible to accelerates the rate of cooling of coating clamp, makes plated film
Fixture can cool down in the short period of time, if blowing support body bottom surface, then can further speed up rate of cooling.
In the coating clamp of above-mentioned a kind of 3D mobile phone faceplate, described air vent is several, and each air vent is all along propping up
Bar circumferentially disposed.Air vent quantity is the most, and rate of cooling is the fastest, each air vent all circumferentially disposed along pole, it is possible to make frame
Each position of body uniformly cools down.
In the coating clamp of above-mentioned a kind of 3D mobile phone faceplate, described pole is metalwork.What metal material was made props up
Bar intensity is higher and more durable.
In the coating clamp of above-mentioned a kind of 3D mobile phone faceplate, described pole is cylinder, each side of described support body
On groove be that several and quantity are equal.Cylindrical pole is easy to process, saves material, and side upper groove is the most, it is possible to
The quantity of the 3D mobile phone faceplate accommodated is the most, and each groove is evenly distributed on each side, it is possible to ensure 3D mobile phone faceplate surface
Plated film is more uniform.
In the coating clamp of above-mentioned a kind of 3D mobile phone faceplate, the most solid with on the bottom surface of support body on the end face of described support body
Surely having some clips, the clip on described end face is equal with the clip quantity on bottom surface.When coating clamp is taken out in coater
After, if not taking 3D mobile phone faceplate for a long time, then need covered with plastic film on the side of support body with dust-proof, to pass through end face
On clip plastic sheeting can be clamped with the clip on bottom surface, convenient fixing.
Compared with prior art, advantage of the present utility model is as follows:
1, offering air vent on the support body of this coating clamp, outside air flows through air vent, it is possible to make coating clamp
Cool down in the short period of time.
2, it is respectively and fixedly provided with some clips on the end face of the support body of this coating clamp and the bottom surface of support body, it is possible to solid easily
Surely for dust-proof plastic sheeting.
Accompanying drawing explanation
Fig. 1 is the structural representation of this coating clamp.
Fig. 2 is the axonometric chart at another visual angle of this coating clamp.
In figure, 1 support body;2 end faces;3 bottom surfaces;4 sides;5 grooves;6 poles;7 air vents;8 clips.
Detailed description of the invention
The following is specific embodiment of the utility model and combine accompanying drawing, the technical solution of the utility model is made further
Description, but this utility model is not limited to these embodiments.
As shown in Figure 1-2, this coating clamp include support body 1, support body 1 include end face 2 and bottom surface 3, end face 2 and bottom surface 3 it
Between there is some sides 4, each side 4 all offers the groove 5 that can place 3D mobile phone faceplate, being fixedly arranged in the middle of of support body 1
Pole 6, the upper end of pole 6 passes from the end face 2 of support body 1, and the bottom of pole 6 passes from the bottom surface 3 of support body 1, on support body 1
Offering air vent 7, air vent 7 runs through the end face 2 of support body 1 and the bottom surface 3 of support body 1.Pole 6 is metalwork, metal material system
Pole 6 intensity become is higher and more durable, and pole 6 can be fixed on support body 1 by the way of welding.
As it is shown in figure 1, air vent 7 is several, each air vent 7 all circumferentially disposed along pole 6.Air vent 7 quantity is more
Many, rate of cooling is the fastest, each air vent 7 all circumferentially disposed along pole 6, it is possible to make each position of support body 1 uniformly cool down.
As shown in Figure 1, 2, it is respectively and fixedly provided with some clips 8, on end face 2 on the end face 2 of support body 1 and on the bottom surface 3 of support body 1
Clip 8 is equal with clip 8 quantity on bottom surface 3.After coating clamp is taken out in coater, if not taking 3D hands for a long time
Machine side plate, then need on the side 4 of support body 1 covered with plastic film with dust-proof, by the clip 8 on end face 2 with on bottom surface 3
Plastic sheeting can be clamped by clip 8, convenient fixing.
As shown in the figures 1 and 2, pole 6 is cylinder, and the groove 5 on each side 4 of support body 1 is that several and quantity are equal.
Cylindrical pole 6 is easy to process, saves material, side 4 upper groove more than 5, it is possible to the quantity of the 3D mobile phone faceplate of receiving is more
Many, in the present embodiment, the groove 5 on each side 4 is 10, and 10 grooves 5 are divided into 5 row, often 2 groove 5 phases on row
To setting.Each groove 5 is evenly distributed on each side 4, it is possible to ensure that the plated film on 3D mobile phone faceplate surface is more uniform.
Specific embodiment described herein is only to this utility model spirit explanation for example.This utility model institute
Belong to those skilled in the art described specific embodiment to make various amendment or supplement or use similar
Mode substitute, but without departing from spirit of the present utility model or surmount scope defined in appended claims.
Claims (5)
1. a coating clamp for 3D mobile phone faceplate, described coating clamp includes that support body (1), described support body (1) include end face (2)
With bottom surface (3), there is between described end face (2) and bottom surface (3) some sides (4), each side (4) all offer and can place
The groove (5) of 3D mobile phone faceplate, described support body (1) be fixedly arranged in the middle of pole (6), the upper end of described pole (6) is from described
The end face (2) of support body (1) passes, and the bottom of described pole (6) passes from the bottom surface (3) of described support body (1), and its feature exists
In, described support body (1) offers air vent (7), described air vent (7) runs through the end face (2) of support body (1) and support body (1)
Bottom surface (3).
The coating clamp of a kind of 3D mobile phone faceplate the most according to claim 1, it is characterised in that described air vent (7) is
Several, each air vent (7) all circumferentially disposed along pole (6).
The coating clamp of a kind of 3D mobile phone faceplate the most according to claim 1, it is characterised in that described pole (6) is gold
Belong to part.
4. according to the coating clamp of a kind of 3D mobile phone faceplate described in claim 1 or 2 or 3, it is characterised in that described pole
(6) being cylinder, the groove (5) on each side (4) of described support body (1) is that several and quantity are equal.
5. according to the coating clamp of a kind of 3D mobile phone faceplate described in claim 1 or 2 or 3, it is characterised in that described support body
(1) end face (2) above and is respectively and fixedly provided with some clips (8) on the bottom surface (3) of support body (1), the clip (8) on described end face (2)
Equal with clip (8) quantity on bottom surface (3).