CN205347595U - 一种用于镁电解槽的水冷石墨阳极 - Google Patents
一种用于镁电解槽的水冷石墨阳极 Download PDFInfo
- Publication number
- CN205347595U CN205347595U CN201520964764.2U CN201520964764U CN205347595U CN 205347595 U CN205347595 U CN 205347595U CN 201520964764 U CN201520964764 U CN 201520964764U CN 205347595 U CN205347595 U CN 205347595U
- Authority
- CN
- China
- Prior art keywords
- graphite anode
- anode block
- electric aluminum
- pieces
- block
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型公开了一种用于镁电解槽的水冷石墨阳极,包括两块石墨阳极块、两块带有冷却水槽的导电铝板;所述两块石墨阳极块侧部粘接在一起,所述两块导电铝板分别放置于所述石墨阳极块两侧;在所述两块导电铝板外侧安装有外侧夹板。每一块所述导电铝板均包括循环水入口、冷却水槽和循环水出口。在石墨阳极块外侧装夹带有冷却水槽的导电铝板,镁电解槽进行生产的过程中,将循环水通入带有冷却水槽的导电铝板,可降低石墨阳极块的温度,将镁电解槽外石墨阳极块温度控制在100℃以下,紧贴石墨阳极块的导电铝板不易被氧化,可减少接触电压降的增加,同时避免长期处在高温环境中的石墨阳极块折断,增加其寿命。
Description
技术领域
本实用新型属于金属镁冶炼技术领域,尤其涉及生产液镁用镁电解槽中石墨阳极的改进。
背景技术
镁电解槽在生产过程中,由石墨阳极块提供正极,现使用的石墨阳极块外侧由铜夹板进行固定后连接在支母线上,石墨阳极长期浸渍在槽内700℃左右的高温电解质中易折断寿命短,且露出镁电解槽的石墨阳极块由于温度高,外侧铜夹板表面易氧化,使铜夹板与石墨阳极块之间的电阻增大,从而增加其余石墨阳极之间的电压降,增加了镁电解槽的电耗,降低了镁电解的电流效率。
实用新型内容
本实用新型的目的是针对现有技术存在的问题,提供一种增加寿命、提高电流效率的水冷石墨阳极。
本实用新型采取如下技术方案:
一种用于镁电解槽的水冷石墨阳极,其特征在于,所述石墨阳极包括两块石墨阳极块(1)、两块带有冷却水槽的导电铝板(2);所述两块石墨阳极块(1)侧部粘接在一起,所述两块导电铝板(2)分别放置于所述石墨阳极块两侧;在所述两块导电铝板(2)外侧安装有外侧夹板。
根据上述的水冷石墨阳极,其特征在于,每一块所述导电铝板(2)均包括循环水入口(3)、冷却水槽(5)和循环水出口(4)。
根据上述的水冷石墨阳极,其特征在于,外侧夹板共4块,其中两块外侧夹板与一块所述导电铝板贴紧,另外两块外侧夹板与另一块所述所述导电铝板贴紧;所述外侧夹板通过双头螺栓螺母(7)与所述导电铝板连接。
本实用新型的有益效果:在石墨阳极块外侧装夹带有冷却水槽的导电铝板,镁电解槽进行生产的过程中,将循环水通入带有冷却水槽的导电铝板,可降低石墨阳极块的温度,将镁电解槽外石墨阳极块温度控制在100℃以下,紧贴石墨阳极块的导电铝板不易被氧化,可减少接触电压降的增加,同时避免长期处在高温环境中的石墨阳极块折断,增加其寿命。
附图说明
图1是本实用新型的结构示意图;
图2是图1的左视图。
具体实施方式
如图1和图2所示,本实用新型的用于镁电解槽的水冷石墨阳极包括两块石墨阳极块(1)、两块带有冷却水槽的导电铝板(2);两块石墨阳极块(1)侧部粘接在一起,组成镁电解槽用的阳极,两块导电铝板(2)分别放置于所述石墨阳极块两侧;在所述两块导电铝板(2)外侧安装有外侧夹板(6),外侧夹板(6)共4块,该4块外侧夹板使用双头螺栓螺母(7)装夹在两块导电铝板(2)的最外侧,对石墨阳极块和导电铝板起夹紧和保护作用,为了更好的起到加紧作用,双头螺栓分布于整个石墨阳极块。每一块所述导电铝板均包括循环水入口(3)、冷却水槽(5)和循环水出口(4),为循环水提供回路,对石墨阳极块起到冷却降温作用。
在石墨阳极块外侧装夹带有冷却水槽的导电铝板,镁电解槽进行生产的过程中,将循环水通入带有冷却水槽的导电铝板,可降低石墨阳极块的温度,将镁电解槽外石墨阳极块温度控制在100℃以下,紧贴石墨阳极块的导电铝板不易被氧化,可减少接触电压降的增加,同时避免长期处在高温环境中的石墨阳极块折断,增加其寿命。
Claims (3)
1.一种用于镁电解槽的水冷石墨阳极,其特征在于,所述石墨阳极包括两块石墨阳极块(1)、两块带有冷却水槽的导电铝板(2);所述两块石墨阳极块(1)侧部粘接在一起,所述两块导电铝板(2)分别放置于所述石墨阳极块两侧;在所述两块导电铝板(2)外侧安装有外侧夹板。
2.根据权利要求1所述的用于镁电解槽的水冷石墨阳极,其特征在于,每一块所述导电铝板均包括循环水入口(3)、冷却水槽(5)和循环水出口(4),通入循环水对石墨阳极块进行冷却降温。
3.根据权利要求1所述的用于镁电解槽的水冷石墨阳极,其特征在于,外侧夹板共4块,其中两块外侧夹板与一块所述导电铝板贴紧,另外两块外侧夹板与另一块所述所述导电铝板贴紧;所述外侧夹板通过双头螺栓螺母(7)与所述导电铝板连接。