CN204986222U - 双金属堆焊复合管件 - Google Patents

双金属堆焊复合管件 Download PDF

Info

Publication number
CN204986222U
CN204986222U CN201520735843.6U CN201520735843U CN204986222U CN 204986222 U CN204986222 U CN 204986222U CN 201520735843 U CN201520735843 U CN 201520735843U CN 204986222 U CN204986222 U CN 204986222U
Authority
CN
China
Prior art keywords
welding
pipe fitting
composite bed
basic unit
overlay cladding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201520735843.6U
Other languages
English (en)
Inventor
何清
张付峰
袁希海
王赤宇
许江新
白杨
任保剑
康佳音
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhengzhou Wanda's Heavy Industry Ltd Co
Original Assignee
Zhengzhou Wanda's Heavy Industry Ltd Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhengzhou Wanda's Heavy Industry Ltd Co filed Critical Zhengzhou Wanda's Heavy Industry Ltd Co
Priority to CN201520735843.6U priority Critical patent/CN204986222U/zh
Application granted granted Critical
Publication of CN204986222U publication Critical patent/CN204986222U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

双金属堆焊复合管件,包括管件本体,管件本体包括外层和位于外层内侧的内层,外层为基层,基层的材料为碳钢或合金钢,内层包括复合层和位于复合层两端的两个堆焊层,复合层为镍基合金或不锈钢,复合层位于基层内侧面的中间位置,复合层通过机械复合的方式与外侧的基层连接,堆焊层通过堆焊的方式连接在基层内侧的两端端部,复合层和堆焊层通过焊接连接。既解决安装焊接时管层焊缝紧密问题,又进一步确保焊接质量,降低成本,耐腐蚀、耐磨性能好、使用寿命长。

Description

双金属堆焊复合管件
技术领域
本实用新型涉及管件领域,具体涉及一种便于安装的耐腐蚀双金属复合管。
背景技术
近年来,随着石油、天然气、化工、船舶开发的迅速发展,管道腐蚀环境对输送管道提出了更高、更为苛刻的耐腐蚀要求,而针对直管的成型,一般采用机械复合和堆焊等方式,机械复合采用爆燃结合、拉拔结合或水压等方式,其制造工艺简单、生产成本较低、但在现场安装过程中,机械复合过程衬管和基管在加热的情况下,使衬管和基管间隙变大,特别是后焊部分,很容易造成衬管变形,焊接难度大,焊后经无损检测合格率低,不能达到焊接规范要求;管端堆焊复合方式具有便于安装、复合层、基层冶金结合、现场焊接效果好等优点,但其成本过高。
复合钢板的制造方法很多,以工业规模制造的方法有铸造复合法,爆炸复合(金属爆炸加工)法、热轧复合法和冷轧复合法等。机械复合方法为现有技术,通过机械的方式将两层金属层复合为一个整体。
实用新型内容
本实用新型的目的在于提供一种双金属堆焊复合管件,管端容易焊接且成本低。
本实用新型的技术方案是:
双金属堆焊复合管件,包括管件本体,管件本体包括外层和位于外层内侧的内层,外层为基层,基层的材料为碳钢或合金钢,内层包括复合层和位于复合层两端的两个堆焊层,复合层为镍基合金或不锈钢,复合层位于基层内侧面的中间位置,复合层通过机械复合的方式与外侧的基层连接,堆焊层通过堆焊的方式连接在基层内侧的两端端部,复合层和堆焊层通过焊接连接。
单个堆焊层的轴向长度小于300毫米。
单个堆焊层的轴向长度小于100-200毫米。
单个堆焊层的轴向长度小于150-200毫米。
复合层的端部与基层相邻的端部的距离大于300毫米。
复合层的厚度为3mm。
堆焊层由两层以上的子堆焊层组成。
子堆焊层的厚度为1-2mm,堆焊层的总厚度为2-4mm。
外层和内层长度相等。
堆焊层与复合层在焊接时的搭接量大于30%。
本实用新型为两端堆焊中间机械结合,克服单一的机械复合和单一的双层堆焊问题,提供一种中间机械复合,管件两端小于300毫米处采用冶金复合堆焊方式,分为两层,基层为碳钢或合金钢,复合层为镍基合金或不锈钢,堆焊层为2-5mm,搭接量大于30%,既解决安装焊接时管层焊缝紧密问题,又进一步确保焊接质量,降低成本,耐腐蚀、耐磨性能好、使用寿命长。
附图说明
图1是本实用新型的结构示意图。
具体实施方式
如图1所示,本实用新型包括管件本体,本实施例中管件本体为两端通透的直管(也可以根据需要为带有弧度的弧形管)。
管件本体包括直管的基层1,基层1的材料为碳钢或合金钢;基层1的内侧复合有复合层2,复合层2位于基层1除端部以外的中间位置,复合层2为镍基合金或不锈钢,复合层2的厚度为3mm,复合层2通过机械复合在基层1内。在基层1两端距离端部300毫米的距离内均为双层堆焊区域,双层堆焊区域处设有堆焊层3。堆焊层3的厚度为2-5mm,堆焊层3与复合层2的搭接量大于30%。堆焊层3由两层以上的子堆焊层组成,子堆焊层的厚度为0.5-2mm,堆焊层的总厚度为2-4mm。复合层2的端部设有30度的坡口。
复合层2和堆焊层3的交界处为焊圈4。堆焊层3由两层堆焊形成。堆焊层3的轴向长度小于300毫米,优选数值为100-200毫米,更优选的数值为150-200毫米。
复合层2的端部与基层1相邻的端部的距离大于300毫米。
操作过程:先将中间部分用普通的机械复合方法焊接,然后在管端小于300毫米进行堆焊作业。
堆焊过程:在确保堆焊界面干净的前提下,将管件预热至150-180度,焊接电流210A热丝为60,电压弧度11-13V焊接速度为200mm/min;送丝速度为2500mm/min;线速度为200mm/min;退步速度为摆10mm退10mm;焊接一层清除干净再焊第二层,堆焊层高为2-5mm,搭接量大于百分之30。双层焊接使管端堆焊焊缝更紧密,为焊接安装提供了很大的便利。

Claims (10)

1.双金属堆焊复合管件,包括管件本体,其特征在于:管件本体包括外层和位于外层内侧的内层,外层为基层,基层的材料为碳钢或合金钢,内层包括复合层和位于复合层两端的两个堆焊层,复合层为镍基合金或不锈钢,复合层位于基层内侧面的中间位置,复合层通过机械复合的方式与外侧的基层连接,堆焊层通过堆焊的方式连接在基层内侧的两端端部,复合层和堆焊层通过焊接连接。
2.根据权利要求1所述的双金属堆焊复合管件,其特征在于:单个堆焊层的轴向长度小于300毫米。
3.根据权利要求2所述的双金属堆焊复合管件,其特征在于:单个堆焊层的轴向长度小于100-200毫米。
4.根据权利要求3所述的双金属堆焊复合管件,其特征在于:单个堆焊层的轴向长度小于150-200毫米。
5.根据权利要求1所述的双金属堆焊复合管件,其特征在于:复合层的端部与基层相邻的端部的距离大于300毫米。
6.根据权利要求1-3任一条所述的双金属堆焊复合管件,其特征在于:复合层的厚度为3mm。
7.根据权利要求1-3任一条所述的双金属堆焊复合管件,其特征在于:堆焊层由两层以上的子堆焊层组成。
8.根据权利要求7所述的双金属堆焊复合管件,其特征在于:子堆焊层的厚度为1-2mm,堆焊层的总厚度为2-4mm。
9.根据权利要求1-3任一条所述的双金属堆焊复合管件,其特征在于:外层和内层长度相等。
10.根据权利要求1-3任一条所述的双金属堆焊复合管件,其特征在于:堆焊层与复合层在焊接时的搭接量大于30%。
CN201520735843.6U 2015-09-22 2015-09-22 双金属堆焊复合管件 Active CN204986222U (zh)