CN203875479U - 一种锻铝与锻铝摩擦焊接防夹伤旋转夹具 - Google Patents
一种锻铝与锻铝摩擦焊接防夹伤旋转夹具 Download PDFInfo
- Publication number
- CN203875479U CN203875479U CN201420229630.1U CN201420229630U CN203875479U CN 203875479 U CN203875479 U CN 203875479U CN 201420229630 U CN201420229630 U CN 201420229630U CN 203875479 U CN203875479 U CN 203875479U
- Authority
- CN
- China
- Prior art keywords
- clamp body
- friction welding
- wrought aluminium
- clamping
- face
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种锻铝与锻铝摩擦焊接防夹伤旋转夹具。包括:一个外形是圆形,内孔为台阶孔,壁厚均匀、尺寸一致,台阶端面到外圆上均匀分布四个开口槽,台阶端面到台阶孔的小孔上也均匀分布四个开口槽,具有弹性的夹具体(1)对导电接头(2)定位、夹持;夹具体(1)台阶孔中的大孔与导电接头(2)的大外圆尺寸一致,对导电接头(2)精确定位;夹具体(1)台阶孔中的小孔尺寸比导电接头(2)的小外圆尺寸大一些,避免出现过定位现象;辅以液压卡盘或弹簧夹头的夹持,导电接头(2)外表面被夹具体(1)夹持后不会被夹溃,不会产生夹伤的痕迹;提高了导电接头(2)摩擦焊接质量。
Description
技术领域
本实用新型属于装备制造技术领域,特别涉及锻铝与锻铝制造的高、低压输变电中导电杆的摩擦焊接制造技术。
背景技术
随着高、低压输变电网络负荷日益增加、控制系统不断发展,摩擦焊接式、锻铝制成的导电杆需求日渐增多,以满足高、低压输变电网络更高综合性能的要求。由摩擦焊接技术制造的锻铝与锻铝摩擦焊接成的导电杆是由精密轧制的锻铝铝管两端分别焊接一个外表面有镀银层、材料是锻铝、外形为台阶圆的导电接头,采用公知的液压卡盘或弹簧夹头夹持导电接头进行摩擦焊接时,由于锻铝的强度低,按照现有的摩擦焊接制造技术,在夹紧时会把导电接头外圆表面夹溃、产生夹伤、镀银层的外表面被夹出凹坑、镀银层脱落,这些改变了导电接头的结构尺寸、电阻率,使用时出现尖边放电现象,使得摩擦焊接制造高、低压输变电导电杆无法使用,导致批量报废。
发明内容
为了解决外表面有镀银层、材料是锻铝的导电接头在摩擦焊接时,在摩擦焊机旋转夹具中外圆被夹伤、出现凹坑、镀银层被夹持后出现脱落的问题,提高产品焊接质量。本实用新型提供一种锻铝与锻铝摩擦焊接防夹伤旋转夹具。
为达到此目的,本实用新型所采用的技术方案是:用一个外形是圆形,内孔为同轴两段台阶孔,内孔和外圆壁厚、台阶孔壁厚均匀、尺寸一致,从台阶端面到外圆上均匀分布四个开口槽,从台阶端面到台阶孔的小孔上也均匀分布四个开口槽,具有弹性的夹具体对导电接头定位、夹持;夹具体台阶孔中的大孔与被焊接的导电接头的大外圆尺寸一致,用于对导电接头精确定位;夹具体台阶孔中的小孔尺寸比导电接头的小外圆尺寸大一些,导电接头小外圆穿过夹具体的小孔,夹具体台阶孔中的小孔就不对导电接头小外圆定位,避免出现过定位现象,提高了定位精确性;夹具体的外圆、内孔、台阶端面均加工的光滑,而且每个开口槽在台阶端面均收尾在各自对应的小圆孔中,使得夹具体没有被开口槽完全切断,仍是一个整体,同时提高了夹具体的弹性,产生适中的弹性夹紧力,辅以液压卡盘或弹簧夹头的夹持,导电接头外表面不会被夹具体夹溃,不会产生夹伤的痕迹、镀银层无脱落现象;实现了导电接头在摩擦焊机上可靠焊接,保证锻铝与锻铝制造的高、低压输变电导电杆摩擦焊接的顺利完成,提高了焊接质量和降低了生产成本。
本发明的有益效果是:使得外表面有镀银层的导电接头在摩擦焊机的旋转夹具中没有被夹伤,无变形,镀银层仍然完好的附着在导电接头的外表面、镀银层无脱落现象,提高了焊接质量,满足了使用要求。真正使锻铝与锻铝制造的高、低压输变导电杆摩擦焊接制造成为一种节能、降耗、环保、高效的产业技术。
下面结合附图和实施例对本实用新型作进一步说明
附图说明:
图1:夹具体右视图。
图2:夹具体主视图。
图3:夹具体左视图。
图4:夹具体A-A剖视图。
图5:夹具体B-B剖视图。
图6:夹具体C-C剖视图。
图中:1.夹具体 2.导电接头
具体实施方式:
实施例1:锻铝与锻铝制造的高、低压输变电导电杆摩擦焊接。采用一个外形是圆形,内孔为同轴两段台阶孔,各处壁厚均匀、尺寸一致,从台阶端面到外圆上均匀分布四个开口槽,从台阶端面到台阶孔的小孔上也均匀分布四个开口槽,具有弹性的夹具体1对导电接头2定位、夹持;夹具体1台阶孔中的大孔与被焊接的导电接头2的大外圆尺寸一致,用于对导电接头2精确定位;夹具体1台阶孔中的小孔尺寸比导电接头2的小外圆尺寸大一些,导电接头2小外圆穿过夹具体1的小孔;夹具体1的外圆、内孔、台阶端面均加工的光滑,而且每个开口槽在台阶端面均收尾在各自对应的小圆孔中,辅以液压卡盘或弹簧夹头的夹持,导电接头2外表面没有被夹具体夹1夹溃,没有产生夹伤的痕迹、镀银层无脱落;实现了导电接头2的可靠定位、夹持。在C500型摩擦焊机上实现锻铝与锻铝制造的高、低压输变电导电杆摩擦焊接的顺利完成。
Claims (3)
1.一种锻铝与锻铝摩擦焊接防夹伤旋转夹具,其特征是:一个外形是圆形,内孔为同轴两段台阶孔,内孔和外圆壁厚、台阶孔壁厚均匀、尺寸一致,从台阶端面到外圆上均匀分布四个开口槽,从台阶端面到台阶孔的小孔上也均匀分布四个开口槽,具有弹性的夹具体(1),对导电接头(2)定位、夹持;导电接头(2)外表面不会被夹溃,不会产生夹伤的痕迹,镀银层无脱落现象。
2.根据权利要求1所述的一种锻铝与锻铝摩擦焊接防夹伤旋转夹具,其特征是:夹具体(1)的每个开口槽在台阶端面均收尾在各自对应的小圆孔中。
3.根据权利要求1所述的一种锻铝与锻铝摩擦焊接防夹伤旋转夹具,其特征是:夹具体(1)的外圆、内孔、台阶端面均加工的光滑。