CN203573824U - 一种铜箔薄膜电容器 - Google Patents

一种铜箔薄膜电容器 Download PDF

Info

Publication number
CN203573824U
CN203573824U CN201320753341.7U CN201320753341U CN203573824U CN 203573824 U CN203573824 U CN 203573824U CN 201320753341 U CN201320753341 U CN 201320753341U CN 203573824 U CN203573824 U CN 203573824U
Authority
CN
China
Prior art keywords
copper foil
copper
film capacitor
fuse
foil film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201320753341.7U
Other languages
English (en)
Inventor
王沛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wang Pei
Original Assignee
SHANGHAI TIANFU ELECTRONIC TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI TIANFU ELECTRONIC TECHNOLOGY Co Ltd filed Critical SHANGHAI TIANFU ELECTRONIC TECHNOLOGY Co Ltd
Priority to CN201320753341.7U priority Critical patent/CN203573824U/zh
Application granted granted Critical
Publication of CN203573824U publication Critical patent/CN203573824U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种铜箔薄膜电容器,包括芯子、铜线和外壳,所述铜线焊接在芯子两侧极面,所述芯子和外壳之间灌注环氧树脂层,所述芯子由铜箔和聚丙烯薄膜双层卷绕而成,所述聚丙烯薄膜为四层,所述聚丙烯薄膜保持同一轴线位置,两层铜箔向不同方向错开,形成错边。本实用新型与现有技术相比具有以下优点:由于采用多层聚丙烯薄膜介质卷绕,使其比同类产品体积小,耐压更稳定;产品品质优良,且大大降低了成本,提高了工作耐温;以铜箔作为电极,提高了导线性能及频率;在音频领域的表现也非常出色。

Description

一种铜箔薄膜电容器
技术领域
 本实用新型涉及一种铜箔薄膜电容器。
背景技术
现在市场生产的电容器,多数为金属化薄膜电容器、铝电解电容器及其他复合介质的电容器。多数电极还是锌、铝或锌铝等材质。介质为薄膜和浸渍了油的纸或浸渍电解液的纸等。但是上述的这些产品,在使用要求:高频、大电流、低震荡、低漏电流等技术要求时,就只有靠串联、并联及增加引出截面积等手段来实现。但这无疑会增加产品的体积、损耗了更多的材料,也未必能在音频领域或更高的要求上达到更好的使用效果。而单独使用纸虽然有其在胆机里优异的表现,但在成本上、稳定、耐温性能上目前仍有欠缺。
发明内容
本实用新型是为了解决上述不足,提供了一种铜箔薄膜电容器。
本实用新型的上述目的通过以下的技术方案来实现:一种铜箔薄膜电容器,其特征在于:包括芯子、铜线和外壳,所述铜线焊接在芯子两侧极面,所述芯子和外壳之间灌注环氧树脂层,所述芯子由铜箔和聚丙烯薄膜双层卷绕而成,所述聚丙烯薄膜为四层,所述聚丙烯薄膜保持同一轴线位置,两层铜箔向不同方向错开,形成错边。
所述芯子上设有特氟龙胶带缠绕层,特氟龙胶带缠绕层外设有胶带包裹层。
所述铜线焊接在芯子两侧极面的形状呈盘绕状。
所述铜箔由无氧铜制成。
本实用新型的电容器适应于直流和VHF级信号的隔直流、旁路和耦合 ,广泛用于滤波、降噪等电路。
本实用新型与现有技术相比具有以下优点:由于采用多层聚丙烯薄膜介质卷绕,使其比同类产品体积小,耐压更稳定;产品品质优良,且大大降低了成本,提高了工作耐温;以铜箔作为电极,提高了导线性能及频率;在音频领域的表现也非常出色。
附图说明
图1是本实用新型的结构示意图。
图2是本实用新型芯子的结构示意图。
图3是本实用新型芯子极面的结构示意图。
具体实施方式
下面结合附图对本实用新型作进一步详述。
如图1、图2所示,一种铜箔薄膜电容器,其特征在于:包括芯子1、铜线2和外壳3,所述铜线2焊接在芯子1两侧极面,所述芯子1和外壳3之间灌注环氧树脂层4,所述芯子1由铜箔11和聚丙烯薄膜12双层卷绕而成,所述聚丙烯薄膜12为四层,所述聚丙烯薄膜12保持同一轴线位置,两层铜箔11向不同方向错开,形成错边13。
所述芯子1上设有特氟龙胶带缠绕层,特氟龙胶带缠绕层外设有胶带包裹层;如图3所示,所述铜线2焊接在芯子1两侧极面的形状呈盘绕状;所述铜箔11由无氧铜制成。
最后应说明的是:上述实施例仅仅是为清楚地说明本实用新型所作的举例,而并非对实施方式的限定,对于所属领域的普通技术人员来说,在上述说明的基础上还可以做出其它不同形式的变化或变动,这里无需也无法对所有的实施方式予以穷举,而由此所引申出的显而易见的变化或变动,仍处于本实用新型的保护范围之中。

Claims (4)

1.一种铜箔薄膜电容器,其特征在于:包括芯子、铜线和外壳,所述铜线焊接在芯子两侧极面,所述芯子和外壳之间灌注环氧树脂层,所述芯子由铜箔和聚丙烯薄膜双层卷绕而成,所述聚丙烯薄膜为四层,所述聚丙烯薄膜保持同一轴线位置,两层铜箔向不同方向错开,形成错边。
2.根据权利要求1所述的一种铜箔薄膜电容器,其特征在于:所述芯子上设有特氟龙胶带缠绕层,特氟龙胶带缠绕层外设有胶带包裹层。
3.根据权利要求1所述的一种铜箔薄膜电容器,其特征在于:所述铜线焊接在芯子两侧极面的形状呈盘绕状。
4.根据权利要求1所述的一种铜箔薄膜电容器,其特征在于:所述铜箔由无氧铜制成。
CN201320753341.7U 2013-11-26 2013-11-26 一种铜箔薄膜电容器 Expired - Fee Related CN203573824U (zh)